# US 2021/0238106 A1 · System and Method for Inhibiting Pyrrhotite-Caused Damage to Concrete Structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0238106 A1
- Document ID: US20210238106A1
- Status: Published application
- Kind: A1
- Application number: 17/161,473
- Filed: 2021-01-28
- Published: 2021-08-05
- Earliest claimed: 2020-02-03
- Inventors: Robert Ashley Walde
- Web page: https://patentgrep.com/patent/US20210238106A1

## CPC

- C04B 41/4535: {applied as a solution, emulsion, dispersion or suspension}
- C04B 41/71: at least one coating being an organic material
- C04B 41/009: {characterised by the material treated}
- C04B 41/4501: {with preformed sheet-like elements}
- C04B 41/4515: {application under vacuum or reduced pressure}
- C04B 41/4884: {Polyurethanes; Polyisocyanates}
- C04B 41/4955: {Polyorganosilanes, i.e. polymers with a Si-Si-Si- chain}
- C04B 41/4961: {Polyorganosiloxanes, i.e. polymers with a Si-O-Si-O-chain; "silicones"}
- C04B 41/5024: {Silicates (C04B41/5022 takes precedence; silico-fluorides C04B41/5018)}
- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 2111/26: Corrosion of reinforcement resistance
- C04B 2111/27: Water resistance, i.e. waterproof or water-repellent materials
- C04B 2111/723: {Repairing reinforced concrete}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A system and a method are provided for inhibiting pyrrhotite-caused damage to concrete structures. The system includes at least one concrete structure, a quantity of migratory corrosion-inhibiting solution, a quantity of concrete reinforcing solution, and a water sealing substance. The concrete structure can be any structure where the concrete aggregate contains pyrrhotite. The quantity of migratory corrosion-inhibiting solution is applied to the concrete structure to prevent further oxidation of pyrrhotite within the concrete structure. The quantity of concrete reinforcing solution is applied to the concrete structure to lower the porosity of the concrete structure and strengthen the overall integrity of the concrete structure. The water sealing substance is applied to the concrete structure to repel water from the concrete structure preventing any further chemical reactions with the pyrrhotite.

## Claims

### Claim 1

A method for inhibiting pyrrhotite-caused damage to concrete structures, the method comprises the steps of:
(A) providing at least one concrete structure, a quantity of migratory corrosion-inhibiting solution, a quantity of concrete-reinforcing solution, and a water-sealing substance;
(B) inspecting at least one fracture of the concrete structure in order to identify pyrrhotite-caused damage to the concrete structure;
(C) applying the quantity of corrosion-inhibiting solution onto the concrete structure, if the pyrrhotite-caused damage to the concrete structure is identified in step (B);
(D) applying the quantity of concrete-reinforcing solution onto the concrete structure, if the pyrrhotite-caused damage to the concrete structure is identified in step (B); and
(E) applying the water-sealing substance onto the concrete structure, if the pyrrhotite-caused damage to the concrete structure is identified in step (B).

### Claim 2 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1 comprises the step of:
determining that the concrete structure contains an aggregate from a source previously identified to contain pyrrhotite during step (B).

### Claim 3 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1 comprises the step of:
executing a petrographic analysis on the concrete structure during step (B).

### Claim 4 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1 comprises the steps of:
providing a vacuum pressure injection device; and
applying the quantity of migratory corrosion-inhibiting solution onto the concrete structure with the vacuum pressure injection device during step (C).

### Claim 5 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1 comprises the steps of:
reducing porosity of the concrete structure with the quantity of concrete-reinforcing solution during step (D); and
increasing structural integrity of the concrete structure with the quantity of concrete-reinforcing solution during step (D).

### Claim 6 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the quantity of migratory corrosion-inhibiting solution includes an active ingredient, and wherein the active ingredient is between 1 percentage by weight (wt. %) to 20 wt. % of the quantity of migratory corrosion-inhibiting solution.

### Claim 7 (depends on 6)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 6, wherein the active ingredient of the quantity of migratory corrosion-inhibiting solution is organic amine carboxylate.

### Claim 8 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the quantity of migratory corrosion-inhibiting solution is applied at a coverage ratio between 5 to 150 square feet per gallon (ft.2/gal.).

### Claim 9 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the quantity of concrete-reinforcing solution includes an active ingredient, and wherein the active ingredient is between 10 wt. % to 30 wt. % of the quantity of concrete-reinforcing solution.

### Claim 10 (depends on 9)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 9, wherein the active ingredient of the quantity of concrete-reinforcing solution is alkaline silicate.

### Claim 11 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the quantity of concrete-reinforcing solution is applied at a coverage ratio between 75 to 150 ft.2/gal.

### Claim 12 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the water-sealing substance is a quantity of water-sealing solution, and wherein the quantity of water-sealing solution includes an active ingredient, and wherein the active ingredient is between 10 wt. % to 100 wt. % of the quantity of water-sealing solution.

### Claim 13 (depends on 12)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 12, wherein the active ingredient of the quantity of water-sealing solution is organic silane.

### Claim 14 (depends on 12)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 12, wherein the active ingredient of the quantity of water-sealing solution is organic siloxane.

### Claim 15 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, wherein the water-sealing substance is a quantity of water-sealing solution, and wherein the quantity of water-sealing solution is applied at a coverage ratio between 75 to 150 ft.2/gal.

### Claim 16 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, the method comprises steps of:
providing the water-sealing substance as a plurality of fiber-reinforced polymer-laminate mats and a quantity of epoxy resin; and
adhering the plurality of fiber-reinforced polymer-laminate mats onto an exterior surface of the concrete structure with the quantity of epoxy resin during step (E).

### Claim 17 (depends on 1)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 1, the method comprises steps of:
providing a water sealing substance as a quantity of urethane-foam-forming materials; and
injecting the quantity of urethane-foam-forming materials onto the concrete structure during step (E).

### Claim 18 (depends on 17)

The method for inhibiting pyrrhotite-caused damage to concreate structures, the method as claimed in claim 17, wherein the quantity of urethane-foam-forming materials includes a quantity of isocyanate, an activator, and a quantity of water.