# US 2021/0230058 A1 · Method for manufacturing an optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0230058 A1
- Document ID: US20210230058A1
- Status: Published application
- Kind: A1
- Application number: 17/159,670
- Filed: 2021-01-27
- Published: 2021-07-29
- Earliest claimed: 2020-01-29
- Assignees: Fujikura Ltd.
- Applicants: Fujikura Ltd.
- Inventors: Kenji Yamashiro; Miryo Kashiwazaki
- Web page: https://patentgrep.com/patent/US20210230058A1

## CPC

- C03C 25/12: General methods of coating; Devices therefor
- C03C 25/106: Single coatings
- C03C 25/26: Macromolecular compounds or prepolymers
- C03C 25/607: in the gaseous phase
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for manufacturing an optical fiber, the method includes: exposing a bare fiber formed of glass and having a temperature of 500° C. to 1,500° C. to a gas in which a moisture content is controlled to 2 to 20 g/m3; applying an uncured resin to an outer periphery of the bare fiber; and curing the resin to form a coating layer.

## Claims

### Claim 1

A method for manufacturing an optical fiber, the method comprising:
exposing a bare fiber having a temperature of 500° C. to 1,500° C. to a gas in which a moisture content is controlled to 2 to 20 g/m3, wherein the bare fiber is formed of glass;
applying an uncured resin to an outer periphery of the bare fiber; and
curing the resin to form a coating layer.

### Claim 2 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein Expression (1) or (2) is satisfied:
2≤W≤5 and 0.05≤T≤0.4 (1);
10≤W≤15 and 0.05≤T≤0.3 (2),
where W (g/m3) is the moisture content of the gas and T (sec) is a time for exposing the bare fiber to the gas.

### Claim 3 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein any one of Expression (3), (4), or (5) is satisfied:
3≤W≤5 and 0.3≤T≤0.4 (3);
4≤W≤15 and 0.1≤T≤0.3 (4);
10≤W≤15 and 0.05≤T≤0.3 (5),
where W (g/m3) is the moisture content of the gas and T (sec) is a time for exposing the bare fiber to the gas.

### Claim 4 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein Expression (6) or (7) is satisfied:
5≤W≤15 and 0.1≤T≤0.3 (6);
4≤W≤5 and 0.3≤T≤0.4 (7),
where W (g/m3) is the moisture content of the gas and T (sec) is a time for exposing the bare fiber to the gas.

### Claim 5 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein the bare fiber is cooled by a cooling device after the bare fiber is exposed to the gas.

### Claim 6 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein
the gas includes helium, and
the bare fiber is exposed to the gas in a cooling device for cooling the bare fiber.

### Claim 7 (depends on 1)

The method for manufacturing an optical fiber according to claim 1, wherein
the bare fiber is exposed to the gas such that a pulling force of the bare fiber pulled from the coating layer is 1.1 N/mm or less.