# US 2021/0229217 A1 · Methods for site-specific enhancement of soft magnetic alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0229217 A1
- Document ID: US20210229217A1
- Status: Published application
- Kind: A1
- Application number: 17/157,550
- Filed: 2021-01-25
- Published: 2021-07-29
- Earliest claimed: 2020-01-27
- Assignees: National Technology & Engineering Solutions of Sandia, LLC
- Applicants: National Technology & Engineering Solutions of Sandia, LLC
- Inventors: Jeffrey Rodelas; Donald F. Susan; Andrew Kustas
- Web page: https://patentgrep.com/patent/US20210229217A1

## CPC

- B23K 26/323: involving parts made of dissimilar metallic material
- B23K 15/0046: {Welding}
- B23K 26/24: Seam welding
- B23K 26/354: by melting
- B32B 15/011: {all layers being formed of iron alloys or steels}
- C22F 3/02: by solidifying a melt controlled by supersonic waves or electric or magnetic fields
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- H01F 41/02: for manufacturing cores, coils, or magnets (H01F41/14 takes precedence; for dynamo-electric machines H02K15/00)
- B23K 2103/18: Dissimilar materials
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The present invention relates to methods of enhancing the surface properties of soft alloys by using a high energy beam. In particular embodiments, the methods can also allow for beam-based welding of such soft alloys to another metal component.

## Claims

### Claim 1

A method comprising:
providing a component comprising a soft magnetic alloy; and
treating a surface portion of the component with a high energy beam, thereby melting and solidifying the surface portion to provide a treated surface portion.

### Claim 2 (depends on 1)

The method of claim 1, wherein the soft magnetic alloy comprises iron and cobalt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the high energy beam comprises a laser beam or an electron beam.

### Claim 4 (depends on 1)

The method of claim 1, wherein the high energy beam comprises a power of from about 200 W to about 500 W.

### Claim 5 (depends on 1)

The method of claim 1, wherein the high energy beam comprises a frequency oscillation of from about 250 Hz to 1 kHz.

### Claim 6 (depends on 1)

The method of claim 1, wherein the high energy beam is translated along a wobble path.

### Claim 7 (depends on 3)

The method of claim 3, wherein the laser beam comprises a wavelength of from about 1000 nm to about 1200 nm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the high energy beam comprises a focused beam size of from about 20 μm to about 80 μm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the solidifying comprises cooling at a rate of from about 500° C./sec to about 5000° C./sec.

### Claim 10 (depends on 1)

The method of claim 1, wherein the treated surface portion comprises at least about 80% increase in tensile strain-to-failure, as compared to the surface portion prior to treatment.

### Claim 11 (depends on 1)

The method of claim 1, wherein the treated surface portion comprises at least about 30% increase in tensile strength, as compared to the surface portion prior to treatment.

### Claim 12 (depends on 1)

The method of claim 1, wherein the component comprises a solenoid, an actuator, a tape core, a magnetic core, a rotor, a stator, a magnetic bearing, a motor, or a generator.

### Claim 13

A method comprising:
providing a first component comprising a soft magnetic alloy in proximity to a second component comprising a metal; and
welding the first component and second component together by applying a high energy beam to a surface portion of the first component and/or second component.

### Claim 14 (depends on 13)

The method of claim 13, wherein the soft magnetic alloy comprises iron and cobalt.

### Claim 15 (depends on 13)

The method of claim 13, wherein the high energy beam comprises a laser beam or an electron beam.

### Claim 16 (depends on 13)

The method of claim 13, wherein the second component comprises a stainless steel or a soft magnetic alloy.

### Claim 17 (depends on 13)

The method of claim 13, wherein a gap is present between the first component and the second component, and wherein the welding step comprises applying the high energy beam or the electron beam within the gap.

### Claim 18 (depends on 13)

The method of claim 13, wherein the first and second components are in contact at a contact point, and wherein the welding step comprises applying the high energy beam or the electron beam at an offset from the contact point.

### Claim 19 (depends on 13)

The method of claim 13, wherein the high energy beam comprises a power of from about 200 W to about 500 W.

### Claim 20 (depends on 13)

The method of claim 13, wherein the high energy beam comprises a frequency oscillation of from about 250 Hz to 1 kHz.

### Claim 21 (depends on 13)

The method of claim 13, wherein the high energy electron beam is translated along a wobble path.

### Claim 22 (depends on 15)

The method of claim 15, wherein the laser beam comprises a wavelength of from about 1000 nm to about 1200 nm.

### Claim 23 (depends on 13)

The method of claim 13, wherein the high energy beam comprises a focused beam size of from about 20 μm to about 80 μm.

### Claim 24 (depends on 13)

The method of claim 13, wherein the solidifying comprises cooling at a rate of from about 500° C./sec to about 5000° C./sec.

### Claim 25 (depends on 13)

The method of claim 13, wherein the first component comprises a solenoid, an actuator, a tape core, a magnetic core, a rotor, a stator, a magnetic bearing, a motor, or a generator.