# US 2021/0229179 A1 · Method for manufacture of transition metal oxide fine particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0229179 A1
- Document ID: US20210229179A1
- Status: Published application
- Kind: A1
- Application number: 17/050,270
- Filed: 2019-05-10
- Published: 2021-07-29
- Earliest claimed: 2018-05-11
- Assignees: LG Electronics Inc.
- Applicants: LG Electronics Inc.
- Inventors: Sanghyun HONG; Jihyun KIM; Seojin LEE; Sangeun SHIM; Jiyoung JUNG; Sosan HWANG; Yooseok KWON
- Web page: https://patentgrep.com/patent/US20210229179A1

## CPC

- C01G 41/00: Compounds of tungsten
- B22F 1/142: Thermal or thermo-mechanical treatment
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- C01B 13/363: {Mixtures of oxides or hydroxides by precipitation}
- C01G 39/02: Oxides; Hydroxides
- C01G 41/02: Oxides; Hydroxides
- B22F 2202/03: Treatment under cryogenic or supercritical conditions
- B22F 2302/25: Oxide
- B22F 2304/058: Particle size above 300 nm up to 1 micrometer
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/80: Compositional purity
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present invention provides a method for the manufacture of transition metal oxide fine particles, the method comprising the steps of: heating a strong-alkaline aqueous solution while stirring same; adding to and dissolving in the heated strong-alkaline aqueous solution a transition metal oxide; adding a strong-acid aqueous solution to the strong alkaline aqueous solution in which the transition metal oxide is dissolved, while stirring same, thereby re-dissolving a solid generated at the interface between the strong-alkaline aqueous solution and the strong-acid aqueous solution; adjusting the pH of the mixed aqueous solution resulting from mixing the strong-alkaline aqueous solution and the strong acid aqueous solution, through adjustment of the adding rate and amount of the strong-acid aqueous solution, to precipitate transition metal oxide fine particles; and separating the transition metal oxide fine particles from the mixed aqueous solution and sequentially washing, drying, and thermally treating the separated transition metal oxide fine particles.

## Claims

### Claim 1

A method for manufacture of transition metal oxide fine particles, the method comprising:
heating a strong alkaline aqueous solution while stirring;
adding a transition metal oxide in the heated strong alkaline aqueous solution to dissolve the transition metal oxide in the strong alkaline aqueous solution;
adding a strong acid aqueous solution to the strong alkaline aqueous solution in which the transition metal oxide is dissolved while stirring to re-dissolve a solid material formed at an interface between the strong alkaline aqueous solution and the strong acid aqueous solution;
adjusting a pH of a mixed aqueous solution of the strong alkaline aqueous solution and the strong acid aqueous solution by controlling speed and amount of adding the strong acid aqueous solution to precipitate transition metal oxide fine particles; and
separating the transition metal oxide fine particles from the mixed aqueous solution and sequentially washing, drying, and heat treating the separated transition metal oxide fine particles.

### Claim 2 (depends on 1)

The method of claim 1, wherein water and sodium hydroxide (NaOH) are mixed in a mass ratio of 6:1 to 10:1, then heated while stirring to produce the strong alkaline aqueous solution.

### Claim 3 (depends on 2)

The method of claim 2, wherein the purity of the sodium hydroxide is greater than or equal to 99%.

### Claim 4 (depends on 1)

The method of claim 1, wherein the heating of the strong alkaline aqueous solution while stirring is performed to heat the strong alkaline aqueous solution at 60 to 105° C. while stirring at 600 rpm to 700 rpm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the transition metal oxide includes at least one selected from a group composed of molybdenum trioxide and tungsten trioxide.

### Claim 6 (depends on 1)

The method of claim 1, wherein the dissolving of the transition metal oxide in the strong alkaline aqueous solution is performed to sequentially dissolve molybdenum trioxide and tungsten trioxide in the strong alkaline aqueous solution.

### Claim 7 (depends on 6)

The method of claim 6, wherein a temperature for dissolving the tungsten trioxide in the strong alkaline aqueous solution is lower than a temperature for dissolving the molybdenum trioxide in the strong alkaline aqueous solution.

### Claim 8 (depends on 5)

The method of claim 5, wherein the purity of the molybdenum trioxide is greater than or equal to 99.5%, and the purity of the tungsten trioxide is greater than or equal to 99%.

### Claim 9 (depends on 1)

The method of claim 1, wherein the dissolving of the transition metal oxide in the strong alkaline aqueous solution is performed until the transition metal oxide is saturated.

### Claim 10 (depends on 1)

The method of claim 1, wherein the dissolving of the transition metal oxide in the strong alkaline aqueous solution is performed to heat the transition metal oxide while stirring until all of suspended solids are dissolved in the strong alkaline aqueous solution.

### Claim 11 (depends on 1)

The method of claim 1, wherein the dissolving of the transition metal oxide in the strong alkaline aqueous solution is performed to heat the strong alkaline aqueous solution while stirring until the strong alkaline aqueous solution becomes transparent.

### Claim 12 (depends on 1)

The method of claim 1, wherein the dissolving of the transition metal oxide in the strong alkaline aqueous solution is performed under the same stirring and heating temperature conditions as the heating of the strong alkaline aqueous solution while stirring.

### Claim 13 (depends on 1)

The method of claim 1, wherein the strong acid aqueous solution is composed of 60% to 75% nitric acid.

### Claim 14 (depends on 1)

The method of claim 1, wherein the re-dissolving of the solid material comprises:
adding the strong acid aqueous solution;
stopping the addition of the strong acid aqueous solution when the solid material is formed;
stirring until the solid material is re-dissolved in the mixed aqueous solution of the strong alkaline aqueous solution and the strong acid aqueous solution; and
adding the strong acid aqueous solution again when the solid material is re-dissolved in the mixed aqueous solution.

### Claim 15 (depends on 1)

The method of claim 1, wherein the precipitating of the transition metal oxide fine particles is performed to generate the transition metal oxide fine particles by adjusting the pH of the mixed aqueous solution to weakly basic.

### Claim 16 (depends on 1)

The method of claim 1, wherein the precipitating of the transition metal oxide fine particles is performed to generate the transition metal oxide fine particles by reducing the pH of the mixed aqueous solution to 7.9 to 8.1.

### Claim 17 (depends on 1)

The method of claim 1, wherein the separating of the transition metal oxide fine particles from the mixed aqueous solution is performed to filter the transition metal oxide fine particles using a membrane filter, and the washing of the separated transition metal oxide fine particles is performed by using distilled water of 100 g or less.

### Claim 18 (depends on 17)

The method of claim 17, wherein the washing of the separated transition metal oxide fine particles is performed such that the transition metal oxide fine particles washed with the distilled water are additionally washed with an aqueous solution of ethanol.

### Claim 19 (depends on 1)

The method of claim 1, wherein the drying of the transition metal oxide fine particles is performed to freeze dry the transition metal oxide fine particles.

### Claim 20 (depends on 1)

The method of claim 1, wherein the drying of the transition metal oxide fine particles comprises:
primary drying that involves drying the transition metal oxide fine particles at a room temperature for at least 24 hours; and
second drying that involves drying the primarily dried transition metal oxide fine particles in a vacuum while increasing a temperature above the room temperature.

### Claim 21 (depends on 1)

The method of claim 1, wherein the heat treating of the transition metal oxide fine particles is performed such that the transition metal oxide fine particles separated from the mixed aqueous solution are dried and heat treated at a temperature of 380° C. to 450° C. for at least 30 minutes.