# US 2021/0202783 A1 · Crystalline silicon solar cell and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0202783 A1
- Document ID: US20210202783A1
- Status: Published application
- Kind: A1
- Application number: 17/203,788
- Filed: 2021-03-17
- Published: 2021-07-01
- Earliest claimed: 2018-09-17
- Assignees: Zhejiang Aiko Solar Energy Technology Co., Ltd.; Guangdong Aiko Solar Energy Technology Co., Ltd.
- Applicants: Zhejiang Aiko Solar Energy Technology Co., Ltd.; Guangdong Aiko Solar Energy Technology Co., Ltd.
- Inventors: Huimin WU; Xiaoming ZHANG; Jiebin FANG; Kang-Cheng LIN; Gang CHEN
- Web page: https://patentgrep.com/patent/US20210202783A1

## CPC

- H10F 71/1221: {comprising polycrystalline silicon}
- H10F 77/311: {for photovoltaic cells}
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 10/165: the heterojunctions being Group IV-IV heterojunctions, e.g. Si/Ge, SiGe/Si or Si/SiC photovoltaic cells
- H10F 77/211: {for photovoltaic cells}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/546: Polycrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The disclosure provides a method for preparing a crystalline silicon solar cell. The method includes: (1) forming a textured surface on a front face of a silicon wafer; (2) depositing a tunneling layer and a doped polysilicon layer on the textured surface of the silicon wafer; (3) depositing a first anti-reflection film layer on the front face of the silicon wafer; and (4) removing the tunneling layer by a laser, the doped polysilicon layer, and the first anti-reflection film layer from a non-electrode region on the front face of the silicon wafer.

## Claims

### Claim 1

A method, comprising:
(1) forming a textured surface on a front face of a silicon wafer;
(2) depositing a tunneling layer and a doped polysilicon layer on the textured surface of the silicon wafer;
(3) depositing a first anti-reflection film layer on the front face of the silicon wafer; and
(4) removing the tunneling layer by a laser, the doped polysilicon layer, and the first anti-reflection film layer from a non-electrode region on the front face of the silicon wafer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
(5) forming a textured surface on the front face of the silicon wafer again;
(6) performing phosphorus diffusion on a surface of the silicon wafer;
(7) removing a PN junction on a back face and a periphery of the silicon wafer and phosphosilicate glass on the front face;
(8) depositing a passivation film on the back face of the silicon wafer;
(9) depositing a second anti-reflection film layer on the front face of the silicon wafer;
(10) performing laser perforation on the back face of the silicon wafer;
(11) etching back electrode paste and aluminum paste on the back face of the silicon wafer; and etching positive electrode paste on the front face of the silicon wafer and drying; and
(12) sintering the silicon wafer obtained in 11) at a temperature of 700-950° C., to form a back electrode, an aluminum back electric field, and a positive electrode.

### Claim 3 (depends on 1)

The method of claim 1, wherein the tunneling layer is an SiO2 layer with a thickness of 0.5-8 nm; and a thickness of the doped polysilicon layer is 5-250 nm.

### Claim 4 (depends on 3)

The method of claim 3, wherein the thickness of the tunneling layer is 0.5-3 nm; and the thickness of the doped polysilicon layer is 50-150 nm.

### Claim 5 (depends on 3)

The method of claim 3, wherein after 2) is completed, a sheet resistance of the silicon wafer is 40-160 Ω/sq.

### Claim 6 (depends on 1)

The method of claim 1, wherein in 3), the first anti-reflection film layer is deposited using a plasma chemical vapor deposition method; the first anti-reflection film layer is a silicon nitride film layer with a thickness of 10-100 nm.

### Claim 7 (depends on 2)

The method of claim 2, wherein the positive electrode is in contact with the tunneling layer through the doped polysilicon layer, the first anti-reflection film layer, and the second anti-reflection film layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the silicon wafer is a P-type monocrystalline silicon wafer; and the doped polysilicon layer is a phosphorus-doped N+ type polysilicon layer.

### Claim 9 (depends on 2)

The method of claim 2, wherein in 5), a mixed solution of NaOH, Na2SiO3, and isopropanol is used to etch the surface of the silicon wafer to prepare a textured surface.

### Claim 10 (depends on 1)

The method of claim 1, wherein 4) is performed using a laser.

### Claim 11 (depends on 1)

A crystalline silicon solar cell, being prepared using the method of claim 1.

### Claim 12

A crystalline silicon solar cell, comprising: a silicon wafer; and an anti-reflection film layer and a positive electrode arranged on a front face of the silicon wafer;
wherein:
a tunneling layer, a doped polysilicon layer, and the anti-reflection film layer are arranged between the positive electrode and the silicon wafer; and
in a region having no positive electrode on the front face of the silicon wafer, the anti-reflection film layer is in direct contact with the silicon wafer.

### Claim 13 (depends on 12)

The cell of claim 12, further comprising: a passivation film, a back electrode, and a back electric field arranged on a back face of the silicon wafer.

### Claim 14 (depends on 12)

The cell of claim 12, wherein the tunneling layer is an SiO2 layer with a thickness of 0.5-8 nm; and a thickness of the doped polysilicon layer is 5-250 nm.

### Claim 15 (depends on 14)

The cell of claim 14, wherein the thickness of the tunneling layer is 0.5-3 nm; and the thickness of the doped polysilicon layer is 50-150 nm.

### Claim 16 (depends on 12)

The cell of claim 12, wherein the anti-reflection film layer is deposited using a plasma chemical vapor deposition method, and the anti-reflection film layer is a silicon nitride film layer.

### Claim 17 (depends on 12)

The cell of claim 12, wherein the silicon wafer is a P-type monocrystalline silicon wafer; and the doped polysilicon layer is a phosphorus-doped N+ type polysilicon layer.

### Claim 18 (depends on 13)

The cell of claim 13, wherein the passivation film comprises an aluminum oxide film and a silicon nitride film, and the aluminum oxide film is arranged between the silicon wafer and the silicon nitride film.

### Claim 19 (depends on 13)

The cell of claim 13, wherein the passivation film comprises an opening, and the back electric field is in contact with the silicon wafer through the opening.