# US 2021/0202564 A1 · Method of forming image sensor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0202564 A1
- Document ID: US20210202564A1
- Status: Published application
- Kind: A1
- Application number: 17/183,871
- Filed: 2021-02-24
- Published: 2021-07-01
- Earliest claimed: 2017-11-10
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Chia-Yu WEI; Yen-Liang LIN; Kuo-Cheng LEE; Hsun-Ying HUANG; Hsin-Chi CHEN
- Web page: https://patentgrep.com/patent/US20210202564A1

## CPC

- H10F 39/184: {Infrared image sensors}
- H10F 30/221: the potential barrier being a PN homojunction
- H10F 39/028: {performed after manufacture of the image sensors, e.g. annealing, gettering of impurities, short-circuit elimination or recrystallisation}
- H10F 39/182: {Colour image sensors}
- H10F 39/199: {Back-illuminated image sensors}
- H10F 39/8033: {Photosensitive area}
- H10F 39/807: {Pixel isolation structures}
- H10F 77/14: Shape of semiconductor bodies; Shapes, relative sizes or dispositions of semiconductor regions within semiconductor bodies
- H10F 10/16: Photovoltaic cells having only PN heterojunction potential barriers
- H10F 39/014: {of CMOS image sensors}
- H10F 39/8053: {Colour filters}
- H10F 39/8063: {Microlenses}
- H10F 77/122: comprising only Group IV materials
- H10F 77/1226: comprising multiple Group IV elements, e.g. SiC
- H10F 77/123: comprising only Group II-VI materials, e.g. CdS, ZnS or HgCdTe
- H10F 77/124: comprising only Group III-V materials, e.g. GaAs
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

A method includes providing a semiconductor substrate having a front side surface and a back side surface opposite to the front side surface. A photosensitive region of the semiconductor substrate is etched to form a recess. A semiconductor material is deposited on the semiconductor substrate to form a radiation sensing member filling the recess. The semiconductor material has an optical band gap energy smaller than 1.77 eV. A device layer is formed over the front side surface of the semiconductor substrate and the radiation sensing member. A trench isolation is formed in an isolation region of the semiconductor substrate and extending from the back side surface of the semiconductor substrate.

## Claims

### Claim 1

A method comprising:
providing a semiconductor substrate having a front side surface and a back side surface opposite to the front side surface;
etching a photosensitive region of the semiconductor substrate to form a recess;
depositing a semiconductor material on the semiconductor substrate to form a radiation sensing member filling the recess, wherein the semiconductor material has an optical band gap energy smaller than 1.77 eV;
forming a device layer over the front side surface of the semiconductor substrate and the radiation sensing member; and
forming a trench isolation in an isolation region of the semiconductor substrate and extending from the back side surface of the semiconductor substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the semiconductor material is formed from germanium or silicon germanium.

### Claim 3 (depends on 1)

The method of claim 1, wherein the semiconductor material is formed from gallium arsenide, indium phosphide, gallium antimonide, cadmium telluride, indium arsenide or indium antimonide.

### Claim 4 (depends on 1)

The method of claim 1, wherein the semiconductor substrate is formed from silicon.

### Claim 5 (depends on 1)

The method of claim 1, wherein the semiconductor material is deposited on the semiconductor substrate by performing a physical vapor deposition (PVD) process, an atomic layer deposition (ALD) process or a plasma enhanced chemical vapor deposition (PECVD) process.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
thinning the semiconductor substrate until a thickness of the semiconductor substrate reaches a range from 1.5 μm to 8 μm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the radiation sensing member is formed having a thickness substantially greater than 100 nm.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
performing a chemical mechanical polishing (CMP) process on the semiconductor material to remove a portion of the semiconductor material over the semiconductor substrate.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
bonding a carrier substrate to the device layer.

### Claim 10

A method comprising:
providing a silicon substrate having a front side surface and a back side surface opposite to the front side surface;
etching a photosensitive region of the silicon substrate to form a recess;
depositing a germanium material on the silicon substrate to form a radiation sensing member filling the recess;
performing an annealing process on the radiation sensing member;
forming a device layer over the front side surface of the silicon substrate and the radiation sensing member; and
forming a trench isolation in an isolation region of the silicon substrate and extending from the back side surface of the silicon substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the annealing process is performed at a temperature in a range of about 500° C. to about 600° C.

### Claim 12 (depends on 10)

The method of claim 10, further comprising performing an ion implantation process to the radiation sensing member to form a pinned element in the radiation sensing member.

### Claim 13 (depends on 12)

The method of claim 12, wherein the annealing process is performed prior to performing the ion implantation process.

### Claim 14 (depends on 10)

The method of claim 10, wherein forming the trench isolation is such that the trench isolation is spaced apart from the germanium material.

### Claim 15

A method comprising:
forming a shallow isolation structure in an isolation region of a substrate;
after forming the shallow isolation structure, forming a recess in a photosensitive region of the substrate;
depositing a semiconductive material in the recess to form a radiation sensing member in the substrate, wherein the semiconductive material and the substrate have different materials;
forming a device layer over the shallow isolation structure and the radiation sensing member; and
forming a deep isolation structure under the shallow isolation structure.

### Claim 16 (depends on 15)

The method of claim 15, wherein forming the recess is such that the recess is deeper than the shallow isolation structure.

### Claim 17 (depends on 15)

The method of claim 15, wherein the semiconductive material is made from germanium, silicon germanium, gallium arsenide, indium phosphide, gallium antimonide, cadmium telluride, indium arsenide, or indium antimonide.

### Claim 18 (depends on 15)

The method of claim 15, wherein forming the device layer is such that the device layer is in contact with the semiconductive material and the substrate.

### Claim 19 (depends on 15)

The method of claim 15, wherein forming the deep isolation structure is such that the deep isolation structure is spaced apart from the semiconductive material.

### Claim 20 (depends on 15)

The method of claim 15, wherein depositing the semiconductive material is such that the semiconductive material is spaced apart from the shallow isolation structure.