# US 2021/0198778 A1 · Method for producing magnesium alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0198778 A1
- Document ID: US20210198778A1
- Status: Published application
- Kind: A1
- Application number: 17/185,521
- Filed: 2021-02-25
- Published: 2021-07-01
- Earliest claimed: 2012-06-26
- Assignees: BIOTRONIK SE & Co. KG
- Applicants: Biotronik AG
- Inventors: Heinz Mueller; Peter Uggowitzer; Joerg Loeffler
- Web page: https://patentgrep.com/patent/US20210198778A1

## CPC

- C22F 1/06: of magnesium or alloys based thereon
- A61F 2/82: Devices providing patency to, or preventing collapsing of, tubular structures of the body, e.g. stents (stent-grafts for tubular structures of the body other than blood vessels A61F2/04; stent-grafts for blood vessels A61F2/07)
- A61L 27/047: {Other specific metals or alloys not covered by A61L27/042 - A61L27/045 or A61L27/06}
- A61L 27/58: Materials at least partially resorbable by the body
- A61L 31/022: {Metals or alloys}
- A61L 31/148: {Materials at least partially resorbable by the body}
- C22C 23/02: with aluminium as the next major constituent
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method for producing a magnesium alloy having improved mechanical and electrochemical properties. The method includes generating a high-purity magnesium by vacuum distillation. A billet of the alloy is generated by synthesis of the high-purity magnesium with 2.0 to 10.0% by weight Al, the remainder being magnesium containing impurities, which promote electrochemical potential differences and/or the formation of precipitations and/or intermetallic phases, in a total amount of no more than 0.0063% by weight of Fe, Si, Mn, Co, Ni, Cu, Zr, Y, Sc or rare earths having the ordinal numbers 21, 57 to 71 and 89 to 103, Be, Cd, In, Sn and/or Pb as well as P, wherein the matrix of the alloy includes intermetallic phases formed of Mg and Al. The alloy is homogenized by annealing at a temperature between 150° C. and 450° C. The homogenized alloy is formed in the temperature range between 200° C. and 400° C.

## Claims

### Claim 1

A method for producing a magnesium alloy having improved mechanical and electrochemical properties, comprising:
a) generating a high-purity magnesium by vacuum distillation;
b) generating a billet of the alloy by synthesis of the high-purity magnesium with 2.0 to 10.0% by weight Al, the remainder being magnesium containing impurities, which promote electrochemical potential differences and/or the formation of precipitations and/or intermetallic phases, in a total amount of no more than 0.0063% by weight of Fe, Si, Mn, Co, Ni, Cu, Zr, Y, Sc or rare earths having the ordinal numbers 21, 57 to 71 and 89 to 103, Be, Cd, In, Sn and/or Pb as well as P, wherein the matrix of the alloy includes intermetallic phases formed of Mg and Al;
c) homogenizing the alloy by annealing at a temperature between 150° C. and 450° C.;
d) forming of the homogenized alloy in the temperature range between 200° C. and 400° C.

### Claim 2 (depends on 1)

The method according to claim 1, comprising annealing with a holding period of between 4 to 40 hours.

### Claim 3 (depends on 1)

The method according to claim 1, comprising annealing with a holding period sufficient to produce a homogeneous fine grain of <10 μm.

### Claim 4 (depends on 1)

The method according to claim 1, comprising annealing with a holding period of at least 3 hours.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the matrix of the alloy includes solid solutions between aluminum and zinc.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the synthesis of the high-purity magnesium is with less or equal 1.0% by weight Zn.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the billet comprises a content of Zn that less or equal 2.0% by weight, and/or the content of Al is 2.0 to 8.0% by weight.

### Claim 8 (depends on 1)

The method according to claim 1, wherein individual impurities in the total sum of impurities amount to the following in % by weight: Fe, Si, Mn, Ni, Co, Cu each with <0.0005; Zr, Y each with <0.0003; and P<0.0002.

### Claim 9 (depends on 1)

The method according to claim 1, wherein Fe, Si, Mn, Co, Ni, and Cu together total no more than 0.003% by weight.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the forming process comprises extrusion, equal channel angular extrusion (EACE) and/or a multiple forging process.

### Claim 11 (depends on 1)

The method according to claim 1, wherein steps c) and d) are repeated at least once.

### Claim 12 (depends on 1)

The method according to claim 1, wherein step c) is performed at a temperature between 250° C. and 450° C. and/or step d) is performed at a temperature between 225° C. and 400° C.