# US 2021/0198760 A1 · A method for improving both strength and ductility of a press-hardening steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0198760 A1
- Document ID: US20210198760A1
- Status: Published application
- Kind: A1
- Application number: 17/058,464
- Filed: 2018-05-24
- Published: 2021-07-01
- Earliest claimed: 2018-05-24
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Qi LU; Jiachen PANG
- Web page: https://patentgrep.com/patent/US20210198760A1

## CPC

- C21D 1/673: for die quenching
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- B21D 22/022: {by heating the blank or stamping associated with heat treatment (C21D takes precedence)}
- C21D 1/26: Methods of annealing
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 9/0068: {for particular articles not mentioned below}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C21D 2211/001: Austenite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)

## Abstract

A method of forming a shaped steel object, includes cutting a blank from an alloy composition. The alloy composition includes 0.1-1 wt. % carbon, 0.1-3 wt. % manganese, 0.1-3 wt. % silicon, 1-10 wt. % aluminum, and a balance being iron. The method also includes heating the blank to a temperature above a temperature at which austenite begins to form to generate a heated blank, transferring the heated blank to a die, forming the heated blank into a predetermined shape defined by the die to generate a shaped steel object, and decreasing the temperature of the shaped steel object to ambient temperature. The heating is performed under an atmosphere comprising at least one of an inert gas, a carbon (C)-based gas, and nitrogen (N2) gas.

## Claims

### Claim 1

A method of forming a shaped steel object, the method comprising:
cutting a blank from an alloy composition, the alloy composition comprising:
carbon (C) at a concentration of greater than or equal to about 0.1 wt. % to less than or equal to about 1 wt. % of the alloy composition,
manganese (Mn) at a concentration of greater than or equal to about 0.1 wt. % to less than or equal to about 3 wt. % of the alloy composition,
silicon (Si) at a concentration of greater than or equal to about 0.1 w. % to less than or equal to about 3 wt. % of the alloy composition,
aluminum (Al) at a concentration of greater than or equal to about 1 wt. % to less than or equal to about 10 wt. % of the alloy composition, and
a balance of the alloy composition being iron (Fe);
heating the blank to a temperature above a temperature at which austenite begins to form (Ac1) to generate a heated blank, wherein the heating is performed under an atmosphere comprising at least one of an inert gas, a carbon-based gas, and nitrogen gas (N2);
transferring the heated blank to a die;
forming the heated blank into a predetermined shape defined by the die to generate a stamped object; and
decreasing the temperature of the stamped object to ambient temperature to form a shaped steel object.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the alloy composition further comprises:
chromium (Cr) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 5 wt. % of the alloy composition.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the alloy composition further comprises at least one of:
nickel (Ni) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 1 wt. % of the alloy composition,
molybdenum (Mo) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 1 wt. % of the alloy composition,
niobium (Nb) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 0.1 wt. % of the alloy composition,
vanadium (V) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 0.5 wt. % of the alloy composition,
copper (Cu) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 1 wt. % of the alloy composition,
titanium (Ti) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 0.5 wt. % of the alloy composition, and
boron (B) at a concentration of greater than or equal to about 0 wt. % to less than or equal to about 0.005 wt. % of the alloy composition.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the Si is at a concentration of about 0.2 wt. % and the Al is at a concentration of greater than or equal to about 1 wt. % to less than or equal to about 5 wt. %.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the C is at a concentration of greater than or equal to about 0.2 wt. % to less than or equal to about 0.6 wt. %.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the alloy composition is in the form of a coil.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the heating the blank comprises heating the blank to a temperature of greater than or equal to about 900° C. to less than or equal to about 950° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the heating is performed for a time period of greater than or equal to about 2 min. to less than or equal to about 20 min.

### Claim 9 (depends on 1)

The method according to claim 1, where the inert gas is selected from the group consisting of helium (He), neon (Ne), argon (Ar), krypton (Kr), xenon (Xe), and a combination thereof.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the C-based gas is selected from the group consisting of CH4, C2H6, and a combination thereof

### Claim 11 (depends on 1)

The method according to claim 1, wherein the heating is performed under an atmosphere comprising a gas selected from the group consisting of He, Ne, Ar, Kr, Xe, N2, CH4, C2H6, and combinations thereof.

### Claim 12 (depends on 1)

The method according to claim 1, wherein after the decreasing the temperature of the stamped object to ambient temperature, the method further comprises:
heating the shaped steel object to a temperature below a martensite start (Ms) temperature.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the heating the shaped steel object to a temperature below the Ms temperature comprises heating the shaped object to a temperature of greater than or equal to about 100° C. to less than or equal to about 400° C. for a time period of greater than or equal to about 0.1 min. to less than or equal to about 60 min.

### Claim 14 (depends on 13)

The method according to claim 13, further comprising:
cooling the shaped object to ambient temperature.

### Claim 15

A method of forming a shaped steel object, the method comprising:
cutting a blank from an alloy composition, the alloy composition comprising:
carbon (C) at a concentration of greater than or equal to about 0.2 wt. % to less than or equal to about 0.6 wt. % of the alloy composition,
manganese (Mn) at a concentration of greater than or equal to about 0.1 wt. % to less than or equal to about 3 wt. % of the alloy composition,
silicon (Si) at a concentration of greater than or equal to about 0.1 w. % to less than or equal to about 3 wt. % of the alloy composition,
aluminum (Al) at a concentration of greater than or equal to about 1 wt. % to less than or equal to about 5 wt. % of the alloy composition, and
a balance of the alloy composition being iron (Fe);
austenitizing the blank under an atmosphere comprising an inert gas to generate an austenitized blank;
forming the austenitized blank into a predetermined shape to generate a shaped object;
decreasing a temperature of the shaped object to ambient temperature at a constant rate to generate a shaped steel object; and
heating the shaped steel object to a temperature of greater than or equal to about 100° C. to less than or equal to about 400° C. for a time period of greater than or equal to about 2 min. to less than or equal to about 30 min.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the Al is at a concentration of greater than or equal to about 3 wt. % to less than or equal to about 4 wt. % of the alloy composition.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the method is free of shot blasting.

### Claim 18 (depends on 15)

The method according to claim 15, wherein the decreasing the temperature of the shaped steel object to ambient temperature at a constant rate comprises cooling the shaped steel object at a rate of greater than or equal to about 15° C./s until ambient temperature is reached.

### Claim 19

A shaped steel object comprising:
an alloy composition having a shape, the alloy composition comprising:
carbon (C) at a concentration of greater than or equal to about 0.2 wt. % to less than or equal to about 0.6 wt. % of the alloy composition,
manganese (Mn) at a concentration of greater than or equal to about 0.1 wt. % to less than or equal to about 3 wt. % of the alloy composition,
silicon (Si) at a concentration of greater than or equal to about 0.1 w. % to less than or equal to about 3 wt. % of the alloy composition,
aluminum (Al) at a concentration of greater than or equal to about 1 wt. % to less than or equal to about 5 wt. % of the alloy composition, and
a balance of the alloy composition being iron (Fe),
wherein the alloy composition was austenitized under at least one of an inert gas, a carbon (C)-based gas, and nitrogen (N2) gas prior to being formed into the shape, formed into the shape, and subjected to a post-heat treatment, and
wherein the shaped steel object has a higher strength and a higher ductility relative to a second shaped object that was not austenitized under at least one of an inert gas, a carbon (C)-based gas, and nitrogen (N2) gas and subjected to a post-heat treatment.

### Claim 20 (depends on 19)

The shaped steel object according to claim 19, wherein the shaped steel object is a part of an automobile.