# US 2021/0197428 A1 · Process for manufacturing composite articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0197428 A1
- Document ID: US20210197428A1
- Status: Published application
- Kind: A1
- Application number: 17/057,455
- Filed: 2019-05-21
- Published: 2021-07-01
- Earliest claimed: 2018-05-24
- Assignees: Rhodia Operations
- Applicants: Rhodia Operations; Georges Pernoud SAS; Billion SAS
- Inventors: Gilles ORANGE; Fabien PASCAL; Patrice JACQUET; Alexandre GIROUD
- Web page: https://patentgrep.com/patent/US20210197428A1

## CPC

- B29C 45/0001: {characterised by the choice of material}
- B29C 45/78: of temperature
- B29C 45/0005: {using fibre reinforcements}
- B29C 45/14786: {Fibrous material or fibre containing material, e.g. fibre mats or fibre reinforced material}
- B29C 45/561: {Injection-compression moulding}
- B29C 70/345: {using matched moulds}
- B29C 70/467: {and impregnating the reinforcements during mould closing (B29C70/465 takes precedence)}
- B29C 70/48: and impregnating the reinforcements in the closed mould, e.g. resin transfer moulding [RTM] {, e.g. by vacuum}
- C08J 5/042: {with carbon fibres}
- C08J 5/043: {with glass fibres}
- B29C 2045/562: {Velocity profiles of the compression stroke}
- B29C 2945/76531: Temperature
- B29C 2945/76739: cavity walls
- B29K 2081/04: {Polysulfides, e.g. PPS, i.e. polyphenylene sulfide or derivatives thereof}
- B29K 2105/0058: {Liquid or visquous}
- B29K 2105/0088: {Blends of polymers}
- B29K 2307/04: Carbon
- B29K 2995/0039: Amorphous
- B29K 2995/004: Semi-crystalline
- C08J 2377/06: Polyamides derived from polyamines and polycarboxylic acids (C08J2377/10 takes precedence)
- C08J 2381/02: Polythioethers; Polythioether-ethers
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention relates to the use of thermoplastic polymer compositions for impregnating reinforcing materials in the form of fabric or industrial fabrics for the manufacture of composite materials. The field of the invention is that of composite materials as well as molding/consolidation processes and obtained parts. The invention more particularly relates to a method of manufacturing a composite article by injection molding comprising at least the steps of introducing at least one reinforcement fabric into a preheated mold, partial closure of the mold, a temperature rise step of the mold, optionally a step of maintaining the temperature of the mold before injection of a thermoplastic polymer composition, a step of injecting a thermoplastic polymer composition into the mold, a step of mold closure to the final part thickness allowing the flow of the resin through the reinforcing fabric, a cooling step and a recovery step of the obtained composite article.

## Claims

### Claim 1

A process for manufacturing a composite article by injection molding a polymer composition comprising at least one semi-crystalline thermoplastic polymer and/or at least one amorphous thermoplastic polymer, comprising the following steps:
(a) Introducing at least one reinforcement material into a preheated mold having a temperature T1 that is in the range of from 50° C. to a temperature T1max, wherein T1max is defined as follows:
T1max=Tgmax+40° C., (i)
if the polymer composition has no melting transition, or
if the polymer composition has at least one melting transition and the highest melting temperature Tmmax of the polymer composition is lower than Tgmax+40° C., wherein Tgmax denotes the highest glass transition temperature of the polymer composition,
or
T1max=Tmmax, (ii)
if the polymer composition has at least one melting transition and the highest melting temperature Tmmax of the polymer composition is equal or greater than Tgmax+40° C.;
(b) partially closing the mold, such that the mold exhibits an open gap with a volume of from 70% to 200% of the polymer volume to be injected;
(c)raising the temperature of the mold to a temperature T2 that is in the range of from T2min to T2max, wherein T2min and T2max are defined as follows:
T2min=Tgmax+50° C., T2max=Tgmax+300° C., (i)
if the polymer composition has no melting transition,
or
T2min=Tgmax+50° C., T2max=Tgmax+150° C., (ii)
if the polymer composition has at least one melting transition and the highest melting temperature Tmmax of the polymer composition is lower than Tgmax+40° C.,
or
T2min=Tmmax+10° C., T2max=Tmmax+100° C., (iii)
if the polymer composition has at least one melting transition and the highest melting temperature Tmmax of the polymer composition is equal or greater than Tgmax+40° C.;
(d) optionally maintaining the temperature of the mold for a period of time;
(e) injecting a polymer composition having a melt viscosity of from 5 to 200 Pas, determined according to ISO 11403-2 at the temperature of step (c) and a shear rate of 100 s−1, into the mold, filling the free cavity obtained by partial closure of the mold;
(f) closing the mold to the final thickness of the part, maintaining the temperature of step (c), employing a compression rate of from 0.001 to 0.5 mm/s and permitting the mold pressure to rise to a range of from 0.2 to 17.5 MPa, preferably of from 0.5 to 10 MPa;
(g) cooling the mold to a temperature T3 that is in the range of from T3min to T3max, wherein T3min and T3max are defined as follows:
T3min=Tgmin−100° C., T3max=Tgmin+50° C., (i)
if the polymer composition has no crystallization transition, and wherein Tgmin denotes the lowest glass transition temperature of the polymer composition; or
T3min=Tcmin−120° C., T3max=Tcmin+25° C., (ii)
if the polymer composition has at least one crystallization transition, and wherein Tcmin denotes the lowest crystallization temperature of the polymer composition;
and
(h) opening the mold, ejecting and recovering the produced composite article.

### Claim 2 (depends on 1)

The process of claim 1, wherein the preheated mold has a temperature in the range of from 75° C. to T1max.

### Claim 3 (depends on 1)

The process of claim 1, wherein the reinforcement material is heated before introduction into the mold.

### Claim 4 (depends on 1)

The process of claim 1, wherein temperature raising step (c) is carried out in a period of from 1 minute to 30 minutes.

### Claim 5 (depends on 1)

The process of claim 1, wherein injection step (e) is carried out in a period of from 10 seconds to 2 minutes.

### Claim 6 (depends on 1)

The process of claim 1, wherein the composite article comprises from 20% to 65% by volume of reinforcing material, based on the total volume of the composite article.

### Claim 7 (depends on 1)

The process of claim 1, wherein the variation of viscosity of the polymer composition amounts to less than ±20%.

### Claim 8 (depends on 1)

The process of claim 1, wherein the semi-crystalline polymer comprises a fully aliphatic polyamide or a partially aromatic polyamide or mixtures thereof.

### Claim 9 (depends on 1)

The process of claim 1, wherein the semi-crystalline polymer comprises a polyphenylene sulphide or a mixture of two or more polyphenylene sulfides.

### Claim 10 (depends on 1)

The process of claim 1, wherein the polymer composition comprises at least one polyamide and at least one polyphenylene sulphide.

### Claim 11 (depends on 1)

The process of claim 1, wherein the amorphous thermoplastic polymer is at least one from the group consisting of: polyacrylate, polystyrene, polycarbonate, polyurethane, polydimethylphenylene ether, polyarylether sulfone, polyetherimide, and polyamideimide.

### Claim 12 (depends on 1)

The process of claim 1, wherein the polymer composition comprises a mixture comprising at least one semi-crystalline and at least one amorphous polymer.

### Claim 13 (depends on 1)

The process of claim 1, wherein the polymer composition comprises a mixture comprising at least one polymer having a glass transition temperature of from 5° C. to 80° C., and at least one polymer having a glass transition temperature of from 81° C. to 250° C.

### Claim 14 (depends on 1)

The process of claim 1, wherein the polymer composition comprises a mixture comprising at least one polymer having a melt viscosity of from 1 to 50 Pa·s and at least one polymer having a melt viscosity of from 75 to 350 Pa·s.

### Claim 15 (depends on 1)

The process of claim 1, wherein the polymer composition exhibits a melt viscosity η of from 10 to 125 Pa·s.

### Claim 16 (depends on 1)

The process of claim 1, further comprising: placing the composite article as recovered in step (h) into a second mold and subsequently at least partially overmolding, via injection molding, the surface of the composite article with a second polymer composition wherein, during the overmolding, the temperature difference between the injected second polymer composition and the composite article is lower than 175° C., preferably lower than 150° C., and more preferably lower than 125° C.

### Claim 17

(canceled)

### Claim 18

(canceled)