# US 2021/0197314 A1 · Method for Reducing the Thickness of Solid-State Layers Provided with Components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0197314 A1
- Document ID: US20210197314A1
- Status: Published application
- Kind: A1
- Application number: 16/606,540
- Filed: 2018-01-15
- Published: 2021-07-01
- Earliest claimed: 2017-04-20
- Assignees: Siltectra GmbH
- Applicants: Siltectra GmbH
- Inventors: Marko Swoboda; Ralf Rieske; Christian Beyer; Jan Richter
- Web page: https://patentgrep.com/patent/US20210197314A1

## CPC

- H10P 95/112: {leaving a reusable substrate, e.g. epitaxial lift off}
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/40: taking account of the properties of the material involved
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- B28D 5/0011: {with preliminary treatment, e.g. weakening by scoring}
- C30B 31/20: Doping by irradiation with electromagnetic waves or by particle radiation
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- B23K 2101/40: Semiconductor devices
- B23K 2103/56: {being semiconducting}
- C30B 29/36: Carbides
- H10D 8/60: Schottky-barrier diodes
- H10D 30/66: Vertical DMOS [VDMOS] FETs
- H10D 62/8325: {Silicon carbide}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The invention relates to a method for separating at least one solid-state layer (4) from at least one solid (1). The method according to the invention includes the steps of: producing a plurality of modifications (9) by means of laser beams in the interior of the solid (1) in order to form a separation plane (8); producing a composite structure by arranging or producing layers and/or components (150) on or above an initially exposed surface (5) of the solid (1), the exposed surface (5) being part of the solid-state layer (4) to be separated; introducing an external force into the solid (1) in order to create stresses in the solid (1), the external force being so great that the stresses cause a crack to propagate along the separation plane (8), wherein the modifications for forming the separation plane (8) are produced before the composite structure is produced.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A method of separating a solid-state layer from a solid-state body, comprising:
generating a plurality of modifications by laser beams within the solid-state body to form a detachment region;
after generating the plurality of modifications, generating a composite structure by arranging or generating layers and/or components on or above an initially exposed surface of the solid-state body, wherein the exposed surface is part of the solid-state layer to be separated; and
introducing an external force into the solid-state body to generate stresses in the solid-state body or generating an internal force in the solid-state body, wherein a strength of the external or internal force is sufficient for crack propagation to occur along the detachment region.

### Claim 19 (depends on 18)

The method of claim 18, wherein introducing the external force into the solid-state body comprises:
arranging a receiving layer on an exposed surface of the composite structure or of the solid-state layer to be separated, wherein the receiving layer comprises a polymer material;
subjecting the receiving layer to thermal stress for generation of stresses in the solid-state body, including cooling the receiving layer to a temperature below ambient temperature,
wherein the cooling comprises subjecting the polymer material of the receiving layer to a glass transition,
wherein the stresses cause a crack to propagate in the solid-state body along the detachment region,
wherein the first solid-state layer separates from the solid-state body along the crack.

### Claim 20 (depends on 18)

The method of claim 18, further comprising:
disposing a diffractive optical element (DOE) in a pathway of the laser radiation prior to penetration of the laser radiation into the solid-state body, wherein the laser radiation is split by the DOE into multiple light pathways for generation of multiple foci.

### Claim 21 (depends on 20)

The method of claim 20, wherein the DOE brings about an image field curvature over a length of 200 μm of not more than 50 μm, not more than 30 μm, not more than 10 μm, not more than 5 μm, or not more than 3 μm.

### Claim 22 (depends on 20)

The method of claim 20, wherein the DOE simultaneously generates 2 or more foci to change one or more material properties of the solid-state body.

### Claim 23 (depends on 18)

The method of claim 18, further comprising:
moving the solid-state body relative to a laser exposure device;
successively generating the laser beams by the laser exposure device for generating at least one modification in each case; and
adjusting the laser exposure device for defined focusing of the laser beams and/or for adjustment of laser energy, depending on at least one parameter.

### Claim 24 (depends on 18)

The method of claim 18, wherein the laser beams penetrate into the solid-state body via a planar surface of the solid-state body, wherein at least one of the laser beams is inclined relative to the planar surface of the solid-state body such that the at least one laser beam enters the donor substrate at an angle other than 0° or 180° to a longitudinal axis of the solid-state body, wherein the at least one laser beam is focused to generate a modification in the solid-state body.

### Claim 25 (depends on 18)

The method of claim 18, further comprising:
removing material from the solid-state body proceeding from a surface extending in a circumferential direction of the solid-state body in a direction of the center of the solid-state body.

### Claim 26 (depends on 18)

The method of claim 18, wherein the solid-state body has crystal lattice planes inclined relative to a planar main surface, wherein the planar main surface forms a boundary on one side in a longitudinal direction of the solid-state body, wherein a crystal lattice plane normal is inclined in a first direction relative to a main surface normal, wherein the modifications are a change in a material property of the solid-state body, wherein the change in the material property forms a linear design at least in sections in the solid-state body by changing a site of penetration of the laser beams, wherein the change in the material property is generated in a generation plane or in the detachment region, wherein the crystal lattice planes of the solid-state body are in an inclined alignment relative to the generation plane or the detachment region, wherein the linear design is inclined relative to a cutting line that arises at a point of intersection between the generation plane or the detachment region and the crystal lattice plane, wherein the changed material property results in tearing of the solid-state body in a form of subcritical cracks, wherein the external force introduced into the solid-state body connects the subcritical cracks such that the solid-state layer detaches from the solid-state body with connection of the subcritical cracks.

### Claim 27 (depends on 18)

The method of claim 18, wherein the laser beams are generated with pulse lengths of less than 5 ns, and wherein the laser beams are generated with pulse energies between 100 nJ and 1 mJ.

### Claim 28 (depends on 18)

The method of claim 18, wherein the detachment region describes at least a three-dimensional outline and/or wherein the detachment region is uneven within the solid-state body.

### Claim 29 (depends on 18)

The method of claim 18, wherein a first parameter is an average refractive index of a material of the solid-state body or a refractive index of the material of the solid-state body in a region of the solid-state body to be traversed to generate a defined modification by the laser beams, and wherein a second parameter is a processing depth in the region of the solid-state body to be traversed to generate the defined modification by the laser beams.

### Claim 30 (depends on 29)

The method of claim 29, further comprising:
determining the first parameter by spectral reflection; and/or
determining the second parameter by determining topography using a confocal-chromatic distance sensor,
wherein data for the first parameter and for the second parameter are provided in a data storage device and sent to a control device at least prior to the generation of the modifications,
wherein the control device adjusts a laser exposure device that generates the laser beans as a function of a respective location of the modification to be produced,
wherein the control device, for adjustment of the laser exposure device, processes distance data to give a distance parameter,
wherein the distance parameter gives the distance of the respective location at which laser beams generate the respective modification by being introduced into the solid-state body at a time of generation of the modification from the laser exposure device,
wherein the distance data are detected by a sensor device.

### Claim 31 (depends on 30)

The method claim 30, wherein the laser exposure device is adjusted as a function of a determination of the first parameter and of the second parameter during the generation of the modification, by determining the refractive index and determining the topography.

### Claim 32 (depends on 18)

The method of claim 18, further comprising:
generating a second group of modifications by additional laser beams to define a second detachment plane, wherein the detachment plane and the second detachment plane are in an orthogonal alignment relative to one another; and
dividing the solid-state layer separated from the solid-state body along the second detachment plane to individualize solid-state elements.

### Claim 33 (depends on 18)

The method of claim 18, further comprising:
pressing at least one pressurizing element of a pressurizing device against at least a predetermined proportion of a stress generation layer for pressing of the stress generation layer onto the surface of the solid-state body,
wherein the pressurizing element is pressed against the stress generation layer at least during thermal stress on the stress generation layer and/or during crack propagation.

### Claim 34 (depends on 18)

The method of claim 18, further comprising:
varying a beam property of the laser beams prior to penetration into the solid-state body,
wherein the beam property is an intensity distribution at a focal point of the laser beams,
wherein the beam property is varied by a spatial light modulator and/or by at least DOE,
wherein the spatial light modulator and/or the DOE is disposed in a beam path of the laser beams between the solid-state body and a radiation source of the laser beams.

### Claim 35 (depends on 18)

The method of claim 18, wherein the modifications in the solid-state body are generated prior to generation or arrangement of a metallic contact layer.

### Claim 36

A solid-state body, comprising:
a detachment region within the solid-state body, the detachment region formed from laser-radiation induced modifications;
a region formed from high-temperature treatment; and
one or more layers and/or one or more components disposed or generated in the region.

### Claim 37

A multicomponent arrangement, comprising:
a solid-state layer comprising at least 50% by mass of SiC, wherein the solid-state layer, in a region of a first surface, has modifications or modification constituents that generate compressive stresses, wherein the modifications are amorphized constituents of the solid-state layer, wherein the modifications are at a shorter distance from, or form part of, the first surface than from a second surface, wherein the second surface is formed parallel to the first surface, wherein the first surface is planar; and
a metal layer generated on the first surface of the solid-state layer.