# US 2021/0197266 A1 · Method for producing nickel powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0197266 A1
- Document ID: US20210197266A1
- Status: Published application
- Kind: A1
- Application number: 16/080,363
- Filed: 2017-02-08
- Published: 2021-07-01
- Earliest claimed: 2016-02-29
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Shin-ichi Heguri; Yoshitomo Ozaki; Osamu Ikeda; Yohei Kudo
- Web page: https://patentgrep.com/patent/US20210197266A1

## CPC

- B22F 9/26: using gaseous reductors
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 2201/013: Hydrogen
- B22F 2301/15: Nickel or cobalt
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

Provided is a method for controlling generation of scaling in a reaction vessel to reduce time and cost required for removal of the scaling in the process of producing nickel powder from a solution containing a nickel ammine sulfate complex. This is a method for producing nickel powder, including: adding, to the solution containing the nickel ammine sulfate complex, seed crystals in an amount of 0.3 times or more and 3 times or less the weight of nickel in the solution to form a slurry; and blowing hydrogen gas into the slurry to reduce a nickel complex ion and to thereby form a nickel precipitate.

## Claims

### Claim 1

A method of producing nickel powder, comprising:
adding, to a solution containing a nickel ammine sulfate complex, seed crystals having a particle size of 1 to 20 μm in an amount of 0.3 to 3 times a weight of nickel in the solution to form a slurry;
charging the slurry into a reaction vessel, maintaining a liquid phase portion occupied by the slurry and a gaseous phase portion other than the liquid phase portion within the reaction vessel;
blowing hydrogen gas into the slurry to reduce a nickel complex ion and to thereby produce and recover nickel powder in which a nickel precipitate is formed on a surface of the seed crystals; and
performing hydrogen reduction by adding the solution containing the nickel ammine sulfate complex to the recovered nickel powder in which the nickel precipitate is formed on the surface of the seed crystals and blowing hydrogen gas into the nickel powder to precipitate nickel on the nickel precipitate and to thereby produce grown nickel powder.

### Claim 2 (depends on 1)

The method of producing nickel powder according to claim 1, wherein a polyacrylate salt dispersant is added to the slurry in an amount of 0.5 to 5% based on the weight of the seed crystals added to the slurry.

### Claim 3 (depends on 1)

The method of producing nickel powder according to claim 1, wherein the hydrogen reduction is repeated to precipitate on the nickel precipitate and to thereby obtain further grown nickel powder.

### Claim 4 (depends on 1)

The method of producing nickel powder according to claim 1, wherein a temperature of the slurry is 150 to 200° C. when hydrogen gas is blown into the slurry.

### Claim 5 (depends on 1)

The method of producing nickel powder according to claim 1, wherein a pressure of the gaseous phase portion in the reaction vessel is in a range of 1.0 to 4.0 MPa when hydrogen gas is blown into the slurry.

### Claim 6 (depends on 1)

The method of producing nickel powder according to claim 1, wherein the seed crystals are nickel powder having the particle size of 1 to 20 μm.

### Claim 7 (depends on 1)

The method of producing nickel powder according to claim 1, wherein the hydrogen reduction is repeated to precipitate on the nickel precipitate and to thereby obtain further grown nickel powder.

### Claim 8 (depends on 1)

The method of producing nickel powder according to claim 1, wherein a temperature of the slurry is 150 to 200° C. when hydrogen gas is blown into the slurry.

### Claim 9 (depends on 1)

The method of producing nickel powder according to claim 1, wherein a pressure of the gaseous phase portion in the reaction vessel is in a range of 1.0 to 4.0 MPa when hydrogen gas is blown into the slurry.

### Claim 10 (depends on 1)

The method of producing nickel powder according to claim 1, wherein the seed crystals are nickel powder having the particle size of 1 to 20 μm.