# US 2021/0176865 A1 · Method for repairing a fine line

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0176865 A1
- Document ID: US20210176865A1
- Status: Published application
- Kind: A1
- Application number: 17/110,501
- Filed: 2020-12-03
- Published: 2021-06-10
- Earliest claimed: 2019-12-04
- Assignees: Guangdong University of Technology
- Applicants: Guangdong University of Technology
- Inventors: Chengqiang CUI; Guannan YANG; Guangdong XU; Yu ZHANG; Xin CHEN
- Web page: https://patentgrep.com/patent/US20210176865A1

## CPC

- H05K 3/225: {Correcting or repairing of printed circuits (H05K1/0292, H05K3/222, H05K3/288, H05K3/4685 take precedence)}
- H05K 1/097: {Inks comprising nanoparticles and specially adapted for being sintered at low temperature (H05K1/095 takes precedence)}
- H05K 3/0055: {After-treatment, e.g. cleaning or desmearing of holes}
- H05K 3/26: Cleaning or polishing of the conductive pattern
- H05K 3/288: {Removal of non-metallic coatings, e.g. for repairing}
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H05K 2201/0272: Mixed conductive particles, i.e. using different conductive particles, e.g. differing in shape
- H05K 2203/0104: for patterning or coating
- H05K 2203/0126: Dispenser, e.g. for solder paste, for supplying conductive paste for screen printing or for filling holes
- H05K 2203/013: Inkjet printing, e.g. for printing insulating material or resist
- H05K 2203/025: Abrading, e.g. grinding or sand blasting
- H05K 2203/0278: Flat pressure, e.g. for connecting terminals with anisotropic conductive adhesive
- H05K 2203/0789: Aqueous acid solution, e.g. for cleaning or etching
- H05K 2203/0796: Oxidant in aqueous solution, e.g. permanganate
- H05K 2203/107: Using laser light
- Y10T 29/49165: by forming conductive walled aperture in base
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for repairing a fine line is provided. Nano metal particles are filled in a defect of a circuit board. The nano metal particles in the defect are irradiated by a laser, or heated, such that the nano metal particles in the defect are metallurgically bonded to an original line of the circuit board. A surface of the circuit board is cleaned to remove residual nano metal particles on parts of the circuit board where metallurgical bonding is not performed, thereby completing line repairing of the circuit board.

## Claims

### Claim 1

A method for repairing a fine line, comprising:
1) filling nano metal particles in a defect of a circuit board;
2) irradiating, by a laser, or heating, the nano metal particles in the defect, such that the nano metal particles in the defect are metallurgically bonded to an original line of the circuit board; and
3) cleaning a surface of the circuit board to remove residual nano metal particles on parts of the circuit board where metallurgical bonding is not performed, thereby completing line repairing of the circuit board;
wherein in step 1), after the nano metal particles are filled in the defect, a light-transmitting plate covers the defect, and a downward force is applied to the light-transmitting plate; and
in step 2), during the irradiation by the laser, the laser is focused on the nano metal particles under the light-transmitting plate.

### Claim 2 (depends on 1)

The method of claim 1, wherein in step 3), the step of cleaning the surface of the circuit board comprises:
cleaning the surface of the circuit board using an organic solution; heating the circuit board according to the degree of removal of the residual nano metal particles; or
cleaning the surface of the circuit board using an oxidizing solution to oxidize the residual nano metal particles on the surface of the circuit board; and cleaning the surface of the circuit board using an acid solution to remove the residual nano metal particles on the surface of the circuit board.

### Claim 3 (depends on 1)

The method of claim 1, wherein the nano metal particles are sent to the defect by inert gas; or
a liquid or a paste prepared by adding the nano metal particles into a solvent is sent to the defect by a spray nozzle or a drip nozzle.

### Claim 4 (depends on 3)

The method of claim 3, wherein the solvent comprises one or more of ethylene glycol, ethanol and terpineol; the solvent is 0-80% by weight of the paste; and during the preparation of the liquid or the paste, an organic reducing agent comprising aldehydes or alcohols and a soldering flux comprising rosin are added.

### Claim 5 (depends on 1)

The method of claim 1, wherein in step 2), an arc-shaped protrusion is provided at an upper surface of the light-transmitting plate; when the nano metal particles are irradiated using the laser, the laser is focused on the nano metal particles under the light-transmitting plate through the arc-shaped protrusion.

### Claim 6 (depends on 1)

The method of claim 1, wherein a surface of the nano metal particles is coated with one or more of polyvinylpyrrolidone, imidazole, 2-phenylimidazole and benzimidazole.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nano metal particles are a mixture of particles with the same particle size; or
the nano metal particles are a mixture of nano-sized particles with different particle sizes; or
the nano metal particles are a mixture of nano-sized particles and micron-sized particles.

### Claim 8 (depends on 6)

The method of claim 6, wherein the nano metal particles are a mixture of particles with the same particle size ranging from 1 nm to 5000 nm; and the nano metal particles have the same shape, being spherical, linear, flake-shaped or irregularly-shaped; or
the nano metal particles are a mixture of particles having different shapes and different particle sizes.

### Claim 9 (depends on 1)

The method of claim 1, wherein the nano metal particles comprise one or more of nano copper particles, nano silver particles, nano silver-coated copper particles, nano silver-coated copper flakes and nano copper-silver alloy particles.

### Claim 10 (depends on 1)

The method of claim 1, wherein when the nano metal particles are irradiated by the laser in step 2), the laser is a continuous laser or a pulsed laser with a wavelength of 0.01 μm-20 μm; a pulse width of the pulsed laser is in the order of picoseconds, femtoseconds or nanoseconds; and the laser is a single pulse-type laser or a multiple pulse-type laser.

### Claim 11 (depends on 3)

The method of claim 3, wherein in step 2), when the laser irradiates the liquid or paste prepared by adding the nano metal particles into the solvent, the liquid or paste is irradiated by the laser; or
the liquid or paste on the defect is preheated and dried using a laser with first energy lower than preset energy, so as to reduce an organic content in the liquid or paste; and then the liquid or paste is irradiated by a laser with second energy higher than the preset energy, so that the liquid or paste in the defect is metallurgically bonded to the original line.