# US 2021/0176835 A1 · Spray cooling furnace electrodes with a cooling liquid that contains surfactants

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0176835 A1
- Document ID: US20210176835A1
- Status: Published application
- Kind: A1
- Application number: 17/255,272
- Filed: 2019-10-15
- Published: 2021-06-10
- Earliest claimed: 2018-10-15
- Assignees: Chemtreat, Inc.
- Applicants: Chemtreat, Inc.
- Inventors: Joseph S. STRASSER; Jeffrey R. TANSKI
- Web page: https://patentgrep.com/patent/US20210176835A1

## CPC

- H05B 7/12: Arrangements for cooling, sealing or protecting electrodes
- C09K 5/00: Heat-transfer, heat-exchange or heat-storage materials, e.g. refrigerants; Materials for the production of heat or cold by chemical reactions other than by combustion
- C21B 13/12: in electric furnaces
- C21C 5/52: Manufacture of steel in electric furnaces {(C21C5/005 takes precedence)}
- C21C 5/5211: {in an alternating current [AC] electric arc furnace}
- F27B 3/24: Cooling arrangements
- F27B 14/06: heated electrically, e.g. induction crucible furnaces with or without any other source of heat (F27B14/04 takes precedence)
- F27B 14/08: Details specially adapted for crucible or pot furnaces
- F27D 9/00: Cooling of furnaces or of charges therein (casings, linings, walls or roofs incorporating cooling arrangements F27D1/12)
- F27B 2014/0837: {Cooling arrangements}
- F27D 2009/0016: {Water-spray}
- Y02P 10/20: Recycling
- Y02P 10/25: Process efficiency
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for cooling furnace electrodes using a cooling liquid containing surfactants. This method can be applied to electrodes used in electric arc furnaces and ladle metallurgy furnaces. The method can involve spraying the cooling liquid onto the electrode, thereby lowering the temperature of the electrode and reducing electrode consumption.

## Claims

### Claim 1

A method for cooling a furnace electrode, comprising:
mixing a surfactant with water to form a cooling liquid so that the surfactant is present in the cooling liquid in an amount in a range of from 10 mg/l to 5,000 mg/l, and
spraying at least a surface of the furnace electrode disposed adjacent a furnace with the cooling liquid to cool the furnace electrode.

### Claim 2 (depends on 1)

The method of claim 1, wherein the surfactant comprises nonylphenol or a nonylphenoxy group.

### Claim 3 (depends on 2)

The method of claim 2, wherein the surfactant further comprises an oxirane polymer.

### Claim 4 (depends on 2)

The method of claim 2, wherein the surfactant comprises nonylphenol.

### Claim 5 (depends on 1)

The method of claim 1, wherein the surface tension of the cooling liquid is in a range of from 54.9 mN/m to 69.5 mN/m at room temperature.

### Claim 6 (depends on 1)

The method of claim 1, wherein the surface tension of the cooling liquid is in a range of from 58.5 mN/m to 65.8 mN/m at room temperature.

### Claim 7 (depends on 1)

The method of claim 1, wherein the surfactant is present in the cooling liquid in an amount in a range of from 50 mg/l to 1,000 mg/l.

### Claim 8 (depends on 1)

The method of claim 1, wherein the surfactant is present in the cooling liquid in an amount in a range of from 100 mg/l to 700 mg/l.

### Claim 9 (depends on 1)

The method of claim 1, wherein the surfactant is present in the cooling liquid in an amount in a range of from 300 mg/l to 600 mg/l.

### Claim 10 (depends on 1)

The method of claim 1, wherein the furnace electrode is an electric arc furnace electrode or a ladle metallurgy furnace electrode.

### Claim 11 (depends on 1)

The method of claim 1, wherein a sufficient amount of the cooling liquid is applied to the surface of the furnace electrode so that the oxidative electrode consumption is reduced as compared to a like method in which water having no surfactant cools the furnace electrode.

### Claim 12 (depends on 10)

The method of claim 10, wherein the oxidative electrode consumption is reduced by 1.5 to 30 percent as compared to the like method.

### Claim 13 (depends on 1)

The method of claim 1, wherein the surface of the furnace electrode is heated to a temperature of at least 700° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the surface of the furnace electrode is heated to a temperature of at least 1200° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the cooling liquid forms a film on the surface of the furnace electrode.