# US 2021/0175503 A1 · Positive-electrode active material precursor for nonaqueous electrolyte secondary battery including nickel-cobalt-manganese carbonate composite, manufacturing method thereof, and method for manufacturing positive-electrode active material for nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175503 A1
- Document ID: US20210175503A1
- Status: Published application
- Kind: A1
- Application number: 17/181,233
- Filed: 2021-02-22
- Published: 2021-06-10
- Earliest claimed: 2016-01-06
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Satoshi Matsumoto; Shuuzou Ozawa; Kikoo Uekusa
- Web page: https://patentgrep.com/patent/US20210175503A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/06: Carbonates
- C01G 53/502: containing lithium and cobalt
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/34: hollow
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/025: {with shapes other than plane or cylindrical}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive-electrode active material precursor for a nonaqueous electrolyte secondary battery, contains a nickel-cobalt-manganese carbonate composite represented by a general formula of NixCoyMnzMtCO3 where x+y+z+t=1, 0.05≤x≤0.3, 0.1≤y≤0.4, 0.55≤z≤0.8, and 0≤t≤0.1 are satisfied; and M represents one or more additive elements selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, and W. The positive-electrode active material precursor includes secondary particles having an average particle diameter greater than or equal to 4 μm and less than or equal to 9 μm. The secondary particle includes a sparse central portion and a dense outer shell portion outside of the central portion, formed of primary particles.

## Claims

### Claim 1

A positive-electrode active material precursor for a nonaqueous electrolyte secondary battery, the positive-electrode active material precursor comprising:
a nickel-cobalt-manganese carbonate composite represented by a general formula of NixCoyMnzMtCO3 where x+y+z+t=1, 0.05≤x≤0.3, 0.1≤y≤0.4, 0.55≤z≤0.8, and 0≤t≤0.1 are satisfied; and M represents one or more additive elements selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, and W,
wherein the positive-electrode active material precursor includes secondary particles having an average particle diameter greater than or equal to 4 μm and less than or equal to 9 μm, and
wherein the secondary particle includes a sparse central portion and a dense outer shell portion outside of the central portion, formed of primary particles.

### Claim 2 (depends on 1)

The positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 1, wherein the additive elements M in the general formula of the nickel-cobalt-manganese carbonate composite include Mo, and
wherein a content ratio of Mo among metal components in the nickel-cobalt-manganese carbonate composite is greater than or equal to 0.5 at % and less than or equal to 5 at %.

### Claim 3

A method for manufacturing a positive-electrode active material precursor for a nonaqueous electrolyte secondary battery containing a nickel-cobalt-manganese carbonate compound represented by a general formula of NixCoyMnzMtCO3 where x+y+z+t=1, 0.05≤x≤0.3, 0.1≤y≤0.4, 0.55≤z≤0.8, and 0≤t≤0.1 are satisfied; and M represents one or more additive elements selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, and W, the method comprising:
an initial aqueous solution preparation process of preparing an initial aqueous solution that contains an ammonium ion supplier and water, in which a pH value is controlled to be greater than or equal to 9.0 and less than or equal to 12.0 by an alkaline aqueous solution at a reference reaction temperature of 25° C., and a liquid temperature is set greater than or equal to 25° C. and less than or equal to 50° C.;
a nucleation process of forming nuclei by adding and mixing, under presence of carbonate ions, an aqueous solution that contains nickel as a metal component, an aqueous solution that contains cobalt as a metal component, an aqueous solution that contains manganese as a metal component, and an ammonium ion supplier, with the initial aqueous solution so as to form a mixed aqueous solution; and
a nucleus growth process of growing the nuclei by adding and mixing, under presence of carbonate ions, an aqueous solution that contains nickel as a metal component, an aqueous solution that contains cobalt as a metal component, an aqueous solution that contains manganese as a metal component, and an ammonium ion supplier, with the mixed aqueous solution formed in the nucleation process,
wherein in the nucleation process, a pH value of the mixed aqueous solution is controlled to be greater than or equal to 8.0 at the reference reaction temperature of 25° C., by adding an alkaline aqueous solution,
wherein in the nucleus growth process, the pH value of the mixed aqueous solution is controlled to be greater than or equal to 6.0 and less than or equal to 7.5 at the reference reaction temperature of 25° C., by adding the alkaline aqueous solution, and
wherein the nucleation process takes a time greater than or equal to 1/20 and less than or equal to 3/10 of a combined time of the nucleation process and the nucleus growth process, to add the aqueous solution that contains nickel as the metal component, the aqueous solution that contains cobalt as the metal component, the aqueous solution that contains manganese as the metal component, and the ammonium ion supplier, to the initial aqueous solution.

### Claim 4 (depends on 3)

The method for manufacturing the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 3, wherein the ammonium ion supplier is either of an ammonium carbonate aqueous solution, ammonia water, an ammonium chloride aqueous solution, or an ammonium sulfate aqueous solution, and
wherein the alkaline aqueous solution is an aqueous solution of one or more substances selected from among sodium carbonate, sodium bicarbonate, potassium carbonate, sodium hydroxide, and potassium hydroxide.

### Claim 5 (depends on 3)

The method for manufacturing the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 3, wherein after completion of the nucleation process and before starting the nucleus growth process, an acid aqueous solution of either sulfuric acid, nitric acid, or hydrochloric acid is added to the mixed aqueous solution so as to lower the pH value of the mixed aqueous solution.

### Claim 6 (depends on 3)

The method for manufacturing the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 3, wherein during processes ranging from the initial aqueous solution preparation process to the nucleus growth process, an ammonia concentration of the initial aqueous solution and the mixed aqueous solution is controlled to be greater than or equal to 3 g/L and less than or equal to 15 g/L.

### Claim 7 (depends on 3)

The method for manufacturing the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 3, the method further comprising:
a coating process of coating the secondary particles contained in the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery obtained in the nucleus growth process, with the additive element.

### Claim 8 (depends on 3)

A method for manufacturing a positive-electrode active material for a nonaqueous electrolyte secondary battery, the method comprising:
a heat treatment process of applying heat treatment to the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery obtained by the method for manufacturing the positive-electrode active material precursor for the nonaqueous electrolyte secondary battery as claimed in claim 3, at a temperature greater than or equal to 105° C. and less than or equal to 600° C.;
a mixing process of adding and mixing a lithium compound in particles obtained in the heat treatment process, to form a lithium mixture; and
a sintering process of sintering the lithium mixture in an oxidizing atmosphere at a temperature greater than or equal to 600° C. and less than or equal to 1000° C.