# US 2021/0175501 A1 · Method for preparing iron nitrate oxyhydroxide, cathode containing iron nitrate oxyhydroxide prepared thereby for lithium secondary battery, and lithium secondary battery comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175501 A1
- Document ID: US20210175501A1
- Status: Published application
- Kind: A1
- Application number: 16/771,039
- Filed: 2019-06-25
- Published: 2021-06-10
- Earliest claimed: 2018-07-10
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Suenghoon HAN; Seongji YE
- Web page: https://patentgrep.com/patent/US20210175501A1

## CPC

- H01M 4/523: {for non-aqueous cells (H01M4/525 takes precedence)}
- H01M 4/625: {Carbon or graphite}
- C01G 49/00: Compounds of iron
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/364: {as mixtures}
- H01M 4/38: of elements or alloys
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2002/84: by UV- or VIS- data
- C01P 2004/03: obtained by SEM
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/40: Electric properties
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing an iron oxyhydroxynitrate, a positive electrode for a lithium secondary battery including the iron oxyhydroxynitrate prepared therefrom, and a lithium secondary battery including the same. The positive electrode for the lithium secondary battery containing the iron oxyhydroxynitrate includes the iron oxyhydroxynitrate represented by the following Formula 1: FeO(NO3)x(OH)1-x, wherein 0<x<1. [Formula 1]

## Claims

### Claim 1

A positive electrode for a lithium secondary battery comprising:
an iron oxyhydroxynitrate represented by the following Formula 1:
FeO(NO3)x(OH)1-x, wherein 0<x<1. [Formula 1]

### Claim 2 (depends on 1)

The positive electrode for the lithium secondary battery according to claim 1, wherein a content of the iron oxyhydroxynitrate is 0.1 parts by weight to 15 parts by weight relative to 100 parts by weight of a base solid material comprising an active material, an electrically conductive material and a binder contained in the positive electrode for the lithium secondary battery.

### Claim 3 (depends on 1)

The positive electrode for the lithium secondary battery according to claim 1, wherein the iron oxyhydroxynitrate is in a form of particles having a particle diameter of 50 nm to 200 nm.

### Claim 4 (depends on 1)

The positive electrode for the lithium secondary battery according to claim 1, wherein the iron oxyhydroxynitrate is crystalline.

### Claim 5 (depends on 1)

The positive electrode for the lithium secondary battery according to claim 1, wherein the iron oxyhydroxynitrate shows X-ray diffraction (XRD) peaks of planes (310) and (520) at 2θ=35.2±0.2° and 61.3±0.2°, respectively.

### Claim 6 (depends on 1)

The positive electrode for the lithium secondary battery according to claim 1, further comprising an active material, an electrically conductive material, and a binder, wherein the active material comprises a sulfur-carbon composite.

### Claim 7 (depends on 6)

The positive electrode for the lithium secondary battery according to claim 6, wherein the sulfur-carbon composite has a sulfur content of 60 parts by weight to 80 parts by weight based on 100 parts by weight of the sulfur-carbon composite.

### Claim 8

A method for preparing an iron oxyhydroxynitrate comprising the steps of:
(1) dissolving Fe(NO3)3.9H2O in a mixed solvent comprising an aqueous solvent and an organic solvent to prepare a Fe(NO3)3.9H2O solution; and
(2) drying the Fe(NO3)3.9H2O solution to obtain a compound represented by the following Formula 1:
FeO(NO3)x(OH)1-x, wherein 0<x<1. [Formula 1]

### Claim 9 (depends on 8)

The method for preparing the iron oxyhydroxynitrate according to claim 8, wherein a concentration of the Fe(NO3)3.9H2O solution in step (1) is 0.5 M to 2.5 M.

### Claim 10 (depends on 8)

The method for preparing the iron oxyhydroxynitrate according to claim 8, wherein the drying in step (2) is carried out at a temperature of 70° C. to 90° C. for 18 hours to 36 hours.

### Claim 11 (depends on 8)

The method for preparing the iron oxyhydroxynitrate according to claim 8, wherein the aqueous solvent and the organic solvent are mixed at a weight ratio of 30:70 to 70:30.

### Claim 12 (depends on 8)

The method for preparing the iron oxyhydroxynitrate according to claim 8, wherein the iron oxyhydroxynitrate is in a form of particles having a particle diameter of 50 nm to 200 nm.

### Claim 13 (depends on 1)

A lithium secondary battery comprising: the positive electrode for the lithium secondary battery of claim 1; a negative electrode; a separator interposed therebetween; and an electrolyte.

### Claim 14 (depends on 13)

The lithium secondary battery according to claim 13, wherein the positive electrode comprises sulfur.