# US 2021/0175490 A1 · Low-temperature preparation of cathode active material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175490 A1
- Document ID: US20210175490A1
- Status: Published application
- Kind: A1
- Application number: 16/769,216
- Filed: 2018-12-10
- Published: 2021-06-10
- Earliest claimed: 2017-12-08
- Assignees: Nederlandse Organisatie voor toegepast-natuurwetenschappelijk onderzoek TNO
- Applicants: Nederlandse Organisatie voor toegepast-natuurwetenschappelijk onderzoek TNO
- Inventors: Evert Jonathan VAN DEN HAM
- Web page: https://patentgrep.com/patent/US20210175490A1

## CPC

- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/052: Li-accumulators
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention discloses a method of preparing a current collector surface enriched with cathode active material. The method comprises preparing a precursor solution by dissolving at least two metal salts and one or more organic acids in a first solvent, adding one or more basic compounds and one or more non-metallic salts to the precursor solution, diluting the precursor solution by adding a second solvent, preparing a surface-treated current collector by disposing at least part of the diluted precursor solution on a current collector surface material, and heating the surface -treated current collector at a temperature of 500 ° C. or less under an oxidative or inert atmosphere, thereby decomposing the diluted precursor solution.

## Claims

### Claim 1

A method of preparing a current collector surface enriched with cathode active material comprising the following steps:
a) preparing a precursor solution by dissolving at least two metal salts and one or more organic acids in a first solvent, said metal salts comprising lithium, and one or more selected from the group consisting of aluminium, cobalt, manganese and nickel;
b) adding one or more basic compounds and one or more non-metallic salts to the precursor solution;
c) diluting the precursor solution obtained in step b) by adding a second solvent;
d) preparing a surface-treated current collector by disposing at least part of the diluted precursor solution on a current collector surface material;
e) heating the surface-treated current collector at a temperature of 500° C. or less under an oxidative or inert atmosphere, thereby decomposing the diluted precursor solution.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal salts comprise a lithium cation, and additionally one or more cations selected from the group of manganese, cobalt, aluminium and nickel, and one or more anions selected from the group consisting of acetate, acetylacetates, alkoxide, chloride, citrate, glycolate, hydroxide, nitrate, and oxalate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by one of the following chemical formulae in which oxygen has been omitted,
LiyCoz wherein 0.1<y<2.0, and 0.1<z<2.0,
LiyMnz wherein 0.1<y<2.0 and 0.1<z<2.0,
LixNiyMnz wherein 0.1<x<2.0, 0.1<y<2.0 and 0.1<z<2.0,
LiwNixCoyAlz wherein 0.1<w<2.0, 0.1<x<2.0, 0.1<y<1.0 and 0<z<1.0, or
LiwNixMnyCoz wherein 0.1<w<2.0, 0.1<x<2.0, 0<y<1.0 and 0<z<1.0.

### Claim 4 (depends on 3)

The method of claim 3, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by the following chemical formula in which oxygen has been omitted,
LiyCoz, wherein
0.1<y<1.5, and 0.5<z<1.5, or 0.1<z<1.0.

### Claim 5 (depends on 3)

The method of claim 3, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by the following chemical formula in which oxygen has been omitted,
LiyMnz, wherein
0.1<y<1.5, and 0.5<z<1.5.

### Claim 6 (depends on 3)

The method of claim 3, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by the following chemical formula in which oxygen has been omitted,
LixNiyMnz, wherein
0.5<x<1.5, or 0.1<x<1.0,
0.2<y<1.2, or 0.1<y<1.0, and
0.8<z<1.2, or 0.1<z<1.0

### Claim 7 (depends on 3)

The method of claim 3, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by the following chemical formula in which oxygen has been omitted,
LiwNixCoyAlz, wherein
0.5<w<1.5, or 0.1<w<1.0,
0.2<x<1.2, or 0.1<x<1.0,
0.1<y<0.5, and
0<z<0.5.

### Claim 8 (depends on 3)

The method of claim 3, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by the following chemical formula in which oxygen has been omitted,
LiwNixMnyCoz, wherein
0.5<w<1.5,
0.1<x<1.2,
0<y<0.5, or 0.1<y<1.0, and
0<z<0.5, or z=1−x−y.

### Claim 9 (depends on 1)

The method of claim 1, wherein the molar ratio of metals present in the precursor solution, precursor solution obtained in step b), and diluted precursor solution is represented by one of the following chemical formulas in which oxygen has been omitted: LiCo, LiMn, LiMn2, Li2Mn, LiNiMn, LiNi0.8Co0.15Al0.05, LiNi0.8Mn0.1Co0.1, LiNi1/3Mn1/3Co1/3 and Li[Li0.2Mn0.54Ni0.13Co0.13].

### Claim 10 (depends on 1)

The method of claim 1, wherein the first solvent comprises one or more selected from the group consisting of ammonia, t-butanol, n-butanol, n-propanol, iso-propanol, nitromethane, ethanol, methanol, 2-methoxyethanol, acetic acid, formic acid, and water.

### Claim 11 (depends on 1)

The method of claim 1, wherein the second solvent comprises one or more selected from the group consisting of ammonia, t-butanol, n-butanol, n-propanol, iso-propanol, nitromethane, ethanol, methanol, 2-methoxyethanol, acetic acid, formic acid, and water.

### Claim 12 (depends on 1)

The method of claim 1, wherein the organic acid comprises one or more selected from the group consisting of citric acid, aconitic acid, tricarballylic acid, trimesic acid, propionic acid, glycolic acid, lactic acid, malic acid, and mandelic acid.

### Claim 13 (depends on 1)

The method of claim 1, wherein the organic acid is selected from the group consisting of glycolic acid, propionic acid, lactic acid, malic acid, tartaric acid, and mandelic acid.

### Claim 14 (depends on 1)

The method of claim 1, wherein the organic acid is glycolic acid.

### Claim 15 (depends on 1)

The method of claim 1, wherein the one or more organic acids are added to the metal salts in step a) in a molar ratio between organic acid and metal salts of 5:1 to 1:3.

### Claim 16 (depends on 1)

The method of claim 1, wherein the basic compound comprises one or more selected from the group consisting of ammonia, aluminium hydroxide, lithium hydroxide, nickel hydroxide, or pyridine.

### Claim 17 (depends on 1)

The method of claim 1, wherein the basic compound comprises ammonia.

### Claim 18 (depends on 1)

The method of claim 1, wherein the one or more basic compounds are added in step b) in an amount sufficient to obtain a precursor solution in a pH range of 5 to 9.

### Claim 19 (depends on 1)

The method of claim 1, wherein the one or more non-metallic salts comprise one or more selected from the group of ammonium nitrate, ammonium perchlorate, ammonium permanganate or ammonium sulphate.

### Claim 20 (depends on 1)

The method of claim 1, wherein the one or more non-metallic salts are added in step b) in a molar ratio between anion of the non-metallic salt and organic acid of the precursor solution in the range of 8:1 to 1:8.

### Claim 21 (depends on 1)

The method of claim 1, wherein the second solvent is added to the precursor solution in step c) in a volumetric ratio of 1:1 or less.

### Claim 22 (depends on 1)

The method of claim 1, wherein the diluted precursor solution of step d) is disposed on the surface of a current collector material selected from the group consisting of platinum, nickel, titanium nitride, gold, copper, tantalum, aluminium, tantalum nitride, indium tin oxide, antimony tin oxide, fluorine doped tin oxide, and aluminium doped zinc oxide.

### Claim 23 (depends on 1)

A current collector surface enriched with cathode active material obtainable by the method of claim 1.

### Claim 24 (depends on 23)

A coating comprising the current collector surface of claim 23, wherein said coating has less than 0.5% of binder material, based on total weight of the coating.