# US 2021/0175449 A1 · Organic thin film transistor and method of manufacturing organic thin film transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175449 A1
- Document ID: US20210175449A1
- Status: Published application
- Kind: A1
- Application number: 17/182,900
- Filed: 2021-02-23
- Published: 2021-06-10
- Earliest claimed: 2018-08-24
- Assignees: FUJIFILM Corporation
- Applicants: FUJIFILM Corporation
- Inventors: Eijiro IWASE
- Web page: https://patentgrep.com/patent/US20210175449A1

## CPC

- H10K 10/88: Passivation; Containers; Encapsulations
- H10K 71/50: Forming devices by joining two substrates together, e.g. lamination techniques
- H10K 10/466: {Lateral bottom-gate IGFETs comprising only a single gate}
- H10K 71/80: using temporary substrates
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are an organic thin film transistor having high bendability and high stability in air and a method of manufacturing the organic thin film transistor. The organic thin film transistor includes: a gas barrier layer consisting of a resin layer and an inorganic layer; a transistor element that is formed on one main surface side of the gas barrier layer and includes a gate electrode, an insulating film, an organic semiconductor layer, a source electrode, and a drain electrode; and a sealing layer that is laminated on a side of the transistor element opposite to the gas barrier layer through an adhesive layer, in which a thickness of the resin layer in the gas barrier layer is less than a thickness ranging from the inorganic layer to the sealing layer in the gas barrier layer.

## Claims

### Claim 1

An organic thin film transistor comprising:
a gas barrier layer consisting of a resin layer and an inorganic layer;
a transistor element that is formed on one main surface side of the gas barrier layer and includes a gate electrode, an insulating film, an organic semiconductor layer, a source electrode, and a drain electrode; and
a sealing layer that is laminated on a side of the transistor element opposite to the gas barrier layer through an adhesive layer,
wherein a thickness of the resin layer in the gas barrier layer is less than a thickness ranging from the inorganic layer to the sealing layer in the gas barrier layer.

### Claim 2 (depends on 1)

The organic thin film transistor according to claim 1,
wherein the sealing layer is a gas barrier layer consisting of a resin layer and an inorganic layer,
a thickness of the resin layer in at least one of the gas barrier layers on both sides of the transistor element is less than a thickness ranging from the inorganic layer of one gas barrier layer to the inorganic layer of another gas barrier layer.

### Claim 3 (depends on 2)

The organic thin film transistor according to claim 2,
wherein thicknesses of the resin layers in the gas barrier layers on both sides of the transistor element are less than the thickness ranging from the inorganic layer of one gas barrier layer to the inorganic layer of another gas barrier layer.

### Claim 4 (depends on 1)

The organic thin film transistor according to claim 1,
wherein a substrate that is peelable from the gas barrier layer is provided on a surface of the gas barrier layer opposite to the transistor element.

### Claim 5 (depends on 1)

The organic thin film transistor according to claim 1,
wherein a ratio of the thickness of the resin layer in the gas barrier layer to the thickness ranging from the inorganic layer to the sealing layer in the gas barrier layer is in a range of 0.01 to 0.9.

### Claim 6 (depends on 1)

The organic thin film transistor according to claim 1,
wherein the inorganic layer of the gas barrier layer consists of silicon nitride.

### Claim 7 (depends on 1)

The organic thin film transistor according to claim 1,
wherein a thickness of the inorganic layer in the gas barrier layer is 50 nm or less.

### Claim 8 (depends on 1)

The organic thin film transistor according to claim 1,
wherein the thickness of the resin layer in the gas barrier layer is in a range of 0.1 μm to 2 μm.

### Claim 9 (depends on 1)

The organic thin film transistor according to claim 1,
wherein a thickness of the adhesive layer is in a range of 2.1 μm to 10 μm.

### Claim 10 (depends on 1)

The organic thin film transistor according to claim 1,
wherein a glass transition temperature of the resin layer in the gas barrier layer is 200° C. or higher.

### Claim 11 (depends on 1)

The organic thin film transistor according to claim 1,
wherein the resin layer in the gas barrier layer includes a bisphenol structure.

### Claim 12 (depends on 1)

The organic thin film transistor according to claim 1,
wherein the resin layer in the gas barrier layer includes polyarylate.

### Claim 13

A method of manufacturing an organic thin film transistor, the method comprising:
a transistor forming step of forming a transistor element on a first gas barrier layer of a transfer type gas barrier film including a substrate and the first gas barrier layer, the transistor element including a gate electrode, an insulating film, an organic semiconductor layer, a source electrode, and a drain electrode, the first gas barrier layer including a resin layer and an inorganic layer, the resin layer being peelable from the substrate, and the inorganic layer being formed on the resin layer;
a bonding step of bonding a transfer type gas barrier film including a substrate and a second gas barrier layer to the transistor element through an adhesive layer, the second gas barrier layer including a resin layer and an inorganic layer, the resin layer being peelable from the substrate, the inorganic layer being formed on the resin layer, and the transfer type gas barrier film being bonded such that the inorganic layer side faces the transistor element; and
a peeling step of peeling the substrate from each of the two transfer type gas barrier films,
wherein in the bonding step, the transfer type gas barrier film is bonded such that at least one of a thickness of the resin layer in the first gas barrier layer or a thickness of the resin layer in the second gas barrier layer is less than a thickness ranging from the inorganic layer of the first gas barrier layer to the inorganic layer of the second gas barrier layer.

### Claim 14 (depends on 2)

The organic thin film transistor according to claim 2,
wherein a substrate that is peelable from the gas barrier layer is provided on a surface of the gas barrier layer opposite to the transistor element.

### Claim 15 (depends on 2)

The organic thin film transistor according to claim 2,
wherein a ratio of the thickness of the resin layer in the gas barrier layer to the thickness ranging from the inorganic layer to the sealing layer in the gas barrier layer is in a range of 0.01 to 0.9.

### Claim 16 (depends on 2)

The organic thin film transistor according to claim 2,
wherein the inorganic layer of the gas barrier layer consists of silicon nitride.

### Claim 17 (depends on 2)

The organic thin film transistor according to claim 2,
wherein a thickness of the inorganic layer in the gas barrier layer is 50 nm or less.

### Claim 18 (depends on 2)

The organic thin film transistor according to claim 2,
wherein the thickness of the resin layer in the gas barrier layer is in a range of 0.1 μm to 2 μm.

### Claim 19 (depends on 2)

The organic thin film transistor according to claim 2,
wherein a thickness of the adhesive layer is in a range of 2.1 μm to 10 μm.

### Claim 20 (depends on 2)

The organic thin film transistor according to claim 2,
wherein a glass transition temperature of the resin layer in the gas barrier layer is 200° C. or higher.