# US 2021/0175411 A1 · Micro-vibration sensor and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175411 A1
- Document ID: US20210175411A1
- Status: Published application
- Kind: A1
- Application number: 16/771,190
- Filed: 2019-10-31
- Published: 2021-06-10
- Earliest claimed: 2018-11-08
- Assignees: Jilin University
- Applicants: Jilin University
- Inventors: Zhiwu HAN; Kejun WANG; Honglie SONG; Junqiu ZHANG; Daobing CHEN; Linpeng LIU; Binjie ZHANG; Tao SUN; Dakai WANG; Changchao ZHANG
- Web page: https://patentgrep.com/patent/US20210175411A1

## CPC

- H10N 30/072: by laminating or bonding of piezoelectric or electrostrictive bodies
- G01H 11/08: using piezoelectric devices
- H10N 30/067: Forming single-layered electrodes of multilayered piezoelectric or electrostrictive parts
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G01H: MEASUREMENT OF MECHANICAL VIBRATIONS OR ULTRASONIC, SONIC OR INFRASONIC WAVES

## Abstract

A micro-vibration sensor and preparation method thereof. The method includes a metal sheet is coated with first curing material, and first curing material is cured into first cured layer; piezoelectric thin film element is attached to edge of first cured layer; one side, attached with piezoelectric thin film element, of first cured layer is vertically placed into second curing material, and second curing material is cured into second cured layer; and metal sheet is removed to obtain micro-vibration sensor. Due to fact that piezoelectric thin film element is arranged at a crack tip, during micro-vibration, stress in stress field of crack tip is rapidly increased due to crack stress deformation, and stress signal is efficiently converted into electric signal; and micro-vibration sensor has characteristics of being low in detection limit and high in accuracy.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A preparation method for a micro-vibration sensor, comprising:
coating a first curing material onto a metal sheet, and curing the first curing material into a first cured layer;
sticking a piezoelectric thin film element onto an edge of the first cured layer;
placing a side of the first cured layer having the piezoelectric thin film element stuck vertically into a second curing material, and curing the second curing material into a second cured layer; and
removing the metal sheet, and obtaining the micro-vibration sensor.

### Claim 17 (depends on 16)

The preparation method according to claim 16, wherein the piezoelectric thin film element is formed by packaging after connecting an electrode onto each of both sides of a piezoelectric thin film.

### Claim 18 (depends on 17)

The preparation method according to claim 17, wherein the piezoelectric thin film is made of material selected from the group consisting of a polyvinylidene fluoride, a zinc oxide, a piezoelectric material of PbTiO3, a piezoelectric crystal or a piezoelectric ceramic.

### Claim 19 (depends on 17)

The preparation method according to claim 17, wherein the electrode is formed by depositing, evaporating, sputtering or brushing an electrode material onto the piezoelectric thin film.

### Claim 20 (depends on 19)

The preparation method according to claim 19, wherein the electrode material is selected from the group consisting of copper, silver, titanium, gold, aluminum, indium tin oxide, graphene or graphite.

### Claim 21 (depends on 16)

The preparation method according to claim 16, wherein the first curing material is selected from the group consisting of epoxy resin, polydimethylsiloxane or ultraviolet curing adhesive.

### Claim 22 (depends on 16)

The preparation method according to claim 16, wherein the second curing material is selected from the group consisting of epoxy resin, siloxane or ultraviolet curing adhesive.

### Claim 23 (depends on 16)

The preparation method according to claim 16, wherein a thickness of the metal sheet is 20-200 μm.

### Claim 24 (depends on 16)

The preparation method according to claim 16, wherein the metal sheet is an aluminum sheet, and the step of removing the metal sheet comprises adopting a ferric chloride solution to remove the aluminum sheet.

### Claim 25 (depends on 16)

The preparation method according to claim 16, wherein a thickness of the first cured layer is 20-200 μm.

### Claim 26 (depends on 16)

The preparation method according to claim 16, wherein in the micro-vibration sensor, the second cured layer has a crack formed.

### Claim 27 (depends on 26)

The preparation method according to claim 26, wherein a tip of the crack forms a near-tip stress field.

### Claim 28 (depends on 27)

The preparation method according to claim 27, wherein the piezoelectric thin film element is located at the near-tip stress field.

### Claim 29 (depends on 27)

The preparation method according to claim 27, wherein the tip of the crack forms a circular arc shape.

### Claim 30 (depends on 16)

A micro-vibration sensor, wherein prepared by adopting the preparation methods for the micro-vibration sensor according to claim 16.