# US 2021/0175377 A1 · Monocrystalline Germanium Wafers, Method for Preparing the Same, Method for Preparing Ingots and Use of Monocrystalline Wafers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175377 A1
- Document ID: US20210175377A1
- Status: Published application
- Kind: A1
- Application number: 16/770,902
- Filed: 2018-07-09
- Published: 2021-06-10
- Earliest claimed: 2017-12-08
- Assignees: Beijing Tongmei Xtal Technology Co., Ltd.
- Applicants: Beijing Tongmei Xtal Technology Co., Ltd.
- Inventors: Rajaram SHETTY; Yuanli WANG; Yvonne ZHOU; Weiguo LIU; Sung-Nee George CHU
- Web page: https://patentgrep.com/patent/US20210175377A1

## CPC

- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- H10F 77/1223: characterised by the dopants
- C30B 11/006: {Controlling or regulating}
- C30B 29/08: Germanium
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- H10F 10/142: comprising multiple PN homojunctions, e.g. tandem cells
- H10F 10/144: comprising only Group III-V materials, e.g. GaAs,AlGaAs, or InP photovoltaic cells
- H10F 71/125: {The active layers comprising only Group II-VI materials, e.g. CdS, ZnS or CdTe}
- H10F 71/1276: {comprising growth substrates not made of Group III-V materials}
- Y02E 10/543: Solar cells from Group II-VI materials
- Y02E 10/544: Solar cells from Group III-V materials
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A monocrystalline germanium wafer that increases the open-circuit voltage of multijunction solar cells, a method for preparing the monocrystalline germanium wafer and a method for preparing an ingot from which the monocrystalline germanium wafer is prepared. The monocrystalline germanium wafer that increases the open-circuit voltage of the bottom cell of multijunction solar cells is prepared by adjusting the amounts of the co-dopants silicon and gallium in the monocrystalline germanium wafer, the ratio of silicon to gallium in the preparation of the monocrystalline germanium.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A monocrystalline germanium wafer that increases open-circuit voltage of a bottom cell of multijunction solar cells, wherein the monocrystalline germanium wafer comprises co-dopants silicon and gallium, with silicon having an atomic concentration of from 1×1014 atoms/cc to 1×1019 atoms/cc and gallium having an atomic concentration of from 1×1016 atoms/cc to 1×1020 atoms/cc.

### Claim 12 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein silicon has an atomic concentration of from 2×1014 atoms/cc to 8×1018 atoms/cc, and gallium has an atomic concentration of from 2×1016 atoms/cc to 9×1019 atoms/cc.

### Claim 13 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein silicon has an atomic concentration of from 3×1014 atoms/cc to 7×1018 atoms/cc, and gallium has an atomic concentration of from 2×1016 atoms/cc to 8×1019 atoms/cc.

### Claim 14 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the ratio of atomic concentration of silicon to atomic concentration of gallium is 1:10-20.

### Claim 15 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the ratio of atomic concentration of silicon to atomic concentration of gallium is 1:8-19.

### Claim 16 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the ratio of atomic concentration of silicon to atomic concentration of gallium is 1:6-18.

### Claim 17 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the monocrystalline germanium wafer has a thickness of 100-700 μm.

### Claim 18 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the monocrystalline germanium wafer has a thickness of 100-500 μm.

### Claim 19 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the monocrystalline germanium wafer has a thickness of 100-200 μm.

### Claim 20 (depends on 11)

The monocrystalline germanium wafer according to claim 11, wherein the monocrystalline germanium wafer has a thickness of 120-140 μm.

### Claim 21

A method for preparing a monocrystalline germanium wafer that increases open-circuit voltage of multijunction solar cells, comprising
1) cutting an initial monocrystalline germanium wafer from a monocrystalline germanium ingot containing silicon and gallium, wherein the initial monocrystalline germanium wafer obtained by cutting has a silicon atomic concentration of from 1×1014 atoms/cc to 10×1018 atoms/cc, a gallium atomic concentration of from 1×1016 atoms/cc to 10×1019 atoms/cc, and a thickness of 200-800 μm;
2) edging the initial monocrystalline germanium wafer obtained in step 1);
3) subjecting the initial monocrystalline germanium wafer edged in step 2) to surface treatment; and
4) subjecting the initial monocrystalline germanium wafer surface-treated in step 3) to rough polishing and then to finish polishing to obtain a monocrystalline germanium wafer product, wherein the resulting monocrystalline germanium wafer product has a thickness of 100-700 μm.

### Claim 22 (depends on 21)

The method for preparing a monocrystalline germanium wafer according to claim 21, wherein the ratio of atomic concentration of silicon to atomic concentration of gallium is 1:10-20.

### Claim 23 (depends on 21)

The method for preparing a monocrystalline germanium wafer according to claim 21, wherein the monocrystalline germanium wafer has a thickness of 100-700 μm.

### Claim 24

A method for preparing a monocrystalline germanium ingot that increases open-circuit voltage of multijunction solar cells, comprising
1) loading a first raw germanium material, co-dopants silicon and gallium, and optionally a liquid sealer into a crucible comprising a seed well holding a seed crystal;
2) loading a second raw germanium material into a loading container for supplementing the first raw germanium material,
3) placing the crucible described in step 1) and the loading container described in step 2) in a quartz tube and sealing the quartz tube under vacuum;
4) placing the quartz tube with the crucible and the loading container described in step 3) into a crystal growth furnace having a movable quartz tube support that supports said quartz tube;
5) melting the first raw germanium material to create a first melt, melting the second raw germanium material to create a second melt and then adding all of the melted second raw germanium material in the loading container into the crucible;
6) cooling the melt in the crucible obtained in step 5) and controlling a temperature gradient and cooling rate of the melt so that the melt crystallizes when in contact with the seed crystal and forms a monocrystalline germanium ingot; and
7) cooling the monocrystalline germanium ingot;
wherein the co-dopants silicon and gallium added in step 1) are in such amounts that within an effective length of the resulting monocrystalline germanium ingot, silicon has an atomic concentration of from 1×1014 atoms/cc to 1×1019 atoms/cc, and gallium has an atomic concentration of from 1×1016 atoms/cc to 1×1020 atoms/cc.

### Claim 25 (depends on 24)

The method for preparing a monocrystalline germanium ingot according to claim 24, wherein the ratio of atomic concentration of silicon to atomic concentration of gallium is 1:10-20.

### Claim 26 (depends on 24)

The method for preparing a monocrystalline germanium ingot according to claim 24, wherein when the melt crystallizes when in contact with the seed crystal and forms a monocrystalline germanium ingot in step 6), a temperature gradient of 0.3 to 2.5° C./cm is created in an ingot growth zone.

### Claim 27 (depends on 24)

The method for preparing a monocrystalline germanium ingot according to claim 24, wherein when the melt crystallizes when in contact with the seed crystal and forms a monocrystalline germanium ingot in step 6), a temperature gradient of 0.5 to 2.0° C./cm is created in an ingot growth zone.

### Claim 28 (depends on 24)

The method for preparing a monocrystalline germanium ingot according to claim 24, wherein when the melt crystallizes when in contact with the seed crystal and forms a monocrystalline germanium ingot in step 6), a temperature gradient of 1.0 to 1.5° C./cm is created in an ingot growth zone.