- Inventors: Pengfei GU
- Web page: https://patentgrep.com/patent/US20210175360A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 64/01: Manufacture or treatment
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present disclosure relates to a TFT and a method for manufacturing the TFT. The method includes forming an active layer; forming a gate electrode insulating layer on the active layer; forming a gate electrode on the gate electrode insulating layer; forming an interlayer insulating layer on the gate electrode to cover the gate electrode and the active layer, so that an interface between the interlayer insulating layer and the active layer possesses a donor-like defect state; forming a via hole in the interlayer insulating layer so that the active layer is exposed; and forming a source electrode and a drain electrode on the interlayer insulating layer, so that the source electrode and the drain electrode are electrically coupled to the active layer through the via hole, respectively.

## Claims

### Claim 1

A method for manufacturing a thin film transistor, comprising:
forming an active layer;
forming a gate electrode insulating layer on the active layer;
forming a gate electrode on the gate electrode insulating layer;
forming an interlayer insulating layer on the gate electrode to cover the gate electrode and the active layer so that an interface between the interlayer insulating layer and the active layer possesses a donor-like defect state;
forming a via hole in the interlayer insulating layer so that the active layer is exposed; and
forming a source electrode and a drain electrode on the interlayer insulating layer so that the source electrode and the drain electrode are electrically coupled to the active layer through the via hole, respectively.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising:
making a portion of the active layer that is in contact with the interlayer insulating layer conductive by an annealing process.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of forming the interlayer insulating layer comprises:
depositing a material of the interlayer insulating layer on the gate electrode, so that an oxygen content in the interlayer insulating layer is lower than an oxygen content of a standard stoichiometric ratio, wherein the oxygen content of the standard stoichiometric ratio represents the oxygen content in the interlayer insulating layer obtained by calculating chemical composition of a material of the interlayer insulating layer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the step of forming the interlayer insulating layer comprises:
co-depositing two or more sources on the gate electrode to form an insulating oxide;
calculating a supply amount of the two or more sources based on a chemical reaction equation by using reaction of the two or more sources to generate the insulating oxide, according to the standard stoichiometric ratio of the insulating oxide;
controlling the supply amount of the source with a high oxygen content of the two or more sources below the calculated supply amount.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the step of forming the interlayer insulating layer comprises:
co-depositing N2O and SiH4 on the gate electrode, wherein a volume flow ratio of the N2O to the SiH4 is about 30:1 or even lower.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the volume flow ratio of the N2O to the SiH4 is about 10:1 or even lower.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the support amount of the source is controlled by changing film-forming parameters of a depositing process.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the active layer comprises IGZO.

### Claim 9

A thin film transistor (TFT), comprising:
a substrate;
an active layer, formed on the substrate;
a gate electrode insulating layer, formed on the active layer and covering a portion of the active layer;
a gate electrode, formed on the gate electrode insulating layer;
an interlayer insulating layer, formed on the gate electrode and covering the gate electrode and the active layer; and
a source electrode and a drain electrode, formed on the interlayer insulating layer, and electrically coupled to the active layer through a via hole formed in the interlayer insulating layer,
wherein an interface between the interlayer insulating layer and the active layer possesses a donor-like defect state.

### Claim 10 (depends on 9)

The TFT according to claim 9, wherein the donor-like defect state comprises an oxygen vacancy.

### Claim 11 (depends on 10)

The TFT according to claim 10, wherein the interlayer insulating layer comprises an insulating oxide, wherein an oxygen content in the insulating oxide is lower than an oxygen content calculated according to a standard stoichiometric ratio of the insulating oxide, wherein the oxygen content calculated according to the standard stoichiometric ratio of the insulating oxide represents an oxygen content in the interlayer insulating layer obtained by calculating chemical composition of the insulating oxide.

### Claim 12 (depends on 10)

The TFT according to claim 10, wherein the interlayer insulating layer is formed by co-depositing N2O and SiH4, wherein a volume flow ratio of the N2O to the SiH4 is about 30:1 or even lower.

### Claim 13 (depends on 12)

The TFT according to claim 12, wherein the volume flow ratio of the N2O to the SiH4 is about 10:1 or even lower.

### Claim 14 (depends on 9)

The TFT according to claim 9, wherein the active layer comprises IGZO.

### Claim 15 (depends on 5)

The method according to claim 5, wherein the volume flow ratio of the N2O to the SiH4 is within a range of about 30:1 to 10:1.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the volume flow ratio of the N2O to the SiH4 is within a range of about 20:1 to 10:1.

### Claim 17 (depends on 12)

The TFT according to claim 12, wherein the volume flow ratio of the N2O to the SiH4 is within a range of about 30:1 to 10:1.

### Claim 18 (depends on 17)

The TFT according to claim 17, wherein the volume flow ratio of the N2O to the SiH4 is within a range of about 20:1 to 10:1.

### Claim 19 (depends on 5)

The method according to claim 5, wherein the support amount of the source is controlled by changing film-forming parameters of a depositing process.

### Claim 20 (depends on 6)

The method according to claim 6, wherein the support amount of the source is controlled by changing film-forming parameters of a depositing process.