# US 2021/0175224 A1 · TVS Diode and Assembly Having Asymmetric Breakdown Voltage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0175224 A1
- Document ID: US20210175224A1
- Status: Published application
- Kind: A1
- Application number: 17/111,690
- Filed: 2020-12-04
- Published: 2021-06-10
- Earliest claimed: 2019-12-06
- Assignees: Littelfuse Semiconductor (Wuxi) Co., Ltd.
- Applicants: Littelfuse Semiconductor (Wuxi) Co., Ltd.
- Inventors: Jianfei ZENG; CAI Yingda
- Web page: https://patentgrep.com/patent/US20210175224A1

## CPC

- H10D 89/611: {using diodes as protective elements}
- H10D 8/021: {of breakdown diodes}
- H10D 8/041: {of multilayer diodes}
- H10D 8/25: Zener diodes
- H10D 8/422: {PN diodes having the PN junctions in mesas}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In one embodiment, an asymmetric TVS device may include a semiconductor substrate, comprising an inner region, the inner region having a first polarity, and a first surface region, disposed on a first surface of the semiconductor substrate, the first surface region comprising a second polarity, opposite the first polarity. The asymmetric TVS device may also include a second surface region, comprising the second polarity, and disposed on a second surface of the semiconductor substrate, opposite the first surface, wherein the first surface region comprises a first dopant concentration, and wherein the second surface region comprises a second dopant concentration, greater than the first dopant concentration.

## Claims

### Claim 1

An asymmetric transient voltage suppression (TVS) device, comprising:
a semiconductor substrate, the semiconductor substrate comprising an inner region, the inner region having a first polarity;
a first surface region, disposed on a first surface of the semiconductor substrate, the first surface region comprising a second polarity, opposite the first polarity; and
a second surface region, comprising the second polarity, and disposed on a second surface of the semiconductor substrate, opposite the first surface,
wherein the first surface region comprises a first dopant concentration, and wherein the second surface region comprises a second dopant concentration, greater than the first dopant concentration.

### Claim 2 (depends on 1)

The asymmetric TVS device of claim 1, the inner region having an N-type polarity.

### Claim 3 (depends on 1)

The asymmetric TVS device of claim 1, wherein the inner region and first surface region comprise a first TVS diode, having a first breakdown voltage, and wherein the inner region and the second surface region comprise a second TVS diode of opposite polarity to the first TVS diode, and having a second breakdown voltage, different from the first breakdown voltage.

### Claim 4 (depends on 3)

The asymmetric TVS device of claim 3, the first breakdown voltage being in a range of 15V to 20 V, and the second breakdown voltage being in a range of 30 V to 35 V.

### Claim 5 (depends on 1)

The asymmetric TVS device of claim 1, the first dopant concentration comprising a range of 8E19/cm3, and the second dopant concentration comprising 2E19/cm3.

### Claim 6 (depends on 1)

The asymmetric TVS device of claim 1, the first surface region comprising a first surface area, the second surface region comprising a second surface area, the same as the first surface area.

### Claim 7

A method of forming an asymmetric transient voltage suppression (TVS) device, comprising:
providing a semiconductor substrate, the semiconductor substrate comprising a first dopant of a first polarity, and defining a first surface and a second surface, opposite the first surface;
performing a first oxidation process of the semiconductor substrate, wherein a first oxide layer forms on the first surface and a second oxide layer forms on the second surface;
removing the first oxide layer from at least a first region of the first surface of the semiconductor substrate;
performing a first doping process, wherein the first doping process generates a first surface region on the first surface, having a first concentration of a second dopant of second polarity, opposite the first polarity;
performing a second oxidation process of the semiconductor substrate, wherein a third oxide layer forms over the first region on the first surface;
removing the second oxide layer from at least a second region of the second surface; and
performing a second doping process, wherein the second doping process generates a second surface region on the second surface, having a second concentration of a second dopant of second polarity, greater than the first concentration.

### Claim 8 (depends on 7)

The method of claim 7, wherein the semiconductor substrate comprises an n-type polarity, and wherein the first surface region and the second surface region comprise a p-type polarity.

### Claim 9 (depends on 8)

The method of claim 8, wherein the semiconductor substrate comprises an n-type inner region, characterized by the n-type polarity, after the performing the first doping process and the performing the second doping process.

### Claim 10 (depends on 9)

The method of claim 9, wherein the n-type inner region and first surface region comprise a first TVS diode, having a first breakdown voltage, and wherein the n-type inner region and the second surface region comprise a second TVS diode of opposite polarity to the first TVS diode, and having a second breakdown voltage, different from the first breakdown voltage.

### Claim 11 (depends on 10)

The method of claim 10, the first breakdown voltage being in a range of 15 V to 20 V, and the second breakdown voltage being in a range of 30 V to 35 V.

### Claim 12 (depends on 7)

The method of claim 7, the first dopant concentration comprising a range of 8E19/cm3, and the second dopant concentration comprising a range of 2E19/cm3.

### Claim 13 (depends on 7)

The method of claim 7, the first surface region comprising a first surface area, and the second surface region comprising a second surface area, the same as the first surface area.

### Claim 14 (depends on 7)

The method of claim 7, wherein the performing the first doping process comprises depositing a first dopant layer, having a first layer thickness, and performing a first drive in anneal, and
wherein the performing the second doping process comprises depositing a second dopant layer, having a second layer thickness, and performing a second drive in anneal.

### Claim 15 (depends on 14)

The method of claim 14, wherein the performing the first layer thickness is different from the second layer thickness.

### Claim 16 (depends on 14)

The method of claim 14, wherein the first drive in anneal is different from the second drive in anneal.

### Claim 17

An asymmetric transient voltage suppression (TVS) device, comprising:
a semiconductor substrate, the semiconductor substrate comprising inner region, the inner region having a first polarity;
a first surface region, disposed on a first surface of the semiconductor substrate, the first surface region comprising a second polarity; and
a second surface region, comprising the second polarity, and disposed on a second surface of the semiconductor substrate, opposite the first surface,
wherein the first surface region and the inner region define a first TVS diode having a first polarity, and a first breakdown voltage, and
wherein the second surface region and the inner region define a second TVS diode having a second polarity, and a second breakdown voltage, greater than the first breakdown voltage.

### Claim 18 (depends on 17)

The asymmetric TVS device of claim 17, comprising a mesa structure.

### Claim 19 (depends on 17)

The asymmetric TVS device of claim 17, comprising a planar structure.