# US 2021/0172359 A1 · High Conductive Exhaust Components for Deposit Prevention & Mitigation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0172359 A1
- Document ID: US20210172359A1
- Status: Published application
- Kind: A1
- Application number: 16/770,905
- Filed: 2017-12-15
- Published: 2021-06-10
- Earliest claimed: 2017-12-15
- Assignees: Cummins Emission Solutions Inc.
- Applicants: Cummins Emission Solutions Inc.
- Inventors: Samuel Johnson; Stephen M. Holl; Matthew K. Volmerding; Timothy Paul Meyer; Andrew J. Albers; Shashank Mishra
- Web page: https://patentgrep.com/patent/US20210172359A1

## CPC

- F01N 3/2066: {Selective catalytic reduction [SCR]}
- F01N 3/208: {Control of selective catalytic reduction [SCR], e.g. by adjusting the dosing of reducing agent}
- F01N 3/28: Construction of catalytic reactors
- F01N 3/2807: {Metal other than sintered metal (F01N3/2832 and F01N3/2835 take precedence)}
- F01N 3/2825: {Ceramics (F01N3/2832, F01N3/2835 take precedence)}
- F01N 2240/40: a hydrolysis catalyst
- F01N 2610/02: the substance being ammonia or urea
- F01N 2610/102: after addition to exhaust gases, e.g. by a passively or actively heated surface in the exhaust conduit
- Y02T 10/12: Improving ICE efficiencies
- F01N: GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR MACHINES OR ENGINES IN GENERAL; GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR INTERNAL-COMBUSTION ENGINES (arrangements in connection with gas exhaust of propulsion units in vehicles B60K13/00; combustion-air intake silencers specially adapted for, or arranged on, internal-combustion engines F02M35/00; protecting against, or damping, noise in general G10K11/16)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

A decomposition reactor tube (DRT) for converting a reductant into ammonia includes an internal structure including a high-thermal conductivity material having a thermal conductivity greater than 20 W/(m·K), wherein the internal structure is at least one of the splash plate, a splash plate frame, a double wall, an outer wall, a mixer, and/or an exhaust assist port.

## Claims

### Claim 1

A decomposition reactor tube (DRT) for converting a reductant into ammonia, comprising:
an inlet configured to receive exhaust gas; and
an internal structure comprising a high-thermal conductivity material having a thermal conductivity greater than 20 W/(m·K),
wherein the internal structure is at least one of a splash plate, a splash plate frame, a double wall, an outer wall, a mixer, and/or an exhaust assist port.

### Claim 2 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material has a thermal conductivity of at least 100 W/(m·K).

### Claim 3 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material has a thermal diffusivity greater than 4.7 mm2·sec−1.

### Claim 4 (depends on 3)

The DRT according to claim 3, wherein the high-thermal conductivity material has a thermal diffusivity of at least 50 mm2·sec−1.

### Claim 5 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material has a yield strength of at least 300 MPa and a heat capacity of at least 700 J/kg·K.

### Claim 6 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material is chemically inert to diesel exhaust fluid (DEF) and urea-based compounds.

### Claim 7 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material comprises a ceramic material and/or a metal alloy material.

### Claim 8 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material comprises at least one ceramic material selected from the group consisting of silicon carbide, aluminum nitride, and/or pyrolytic graphite.

### Claim 9 (depends on 1)

The DRT according to claim 1, wherein the high-thermal conductivity material comprises a metal alloy material selected from the group consisting of an aluminum alloy, a magnesium-scandium alloy, and/or an aluminum-silicon-manganese-magnesium alloy.

### Claim 10 (depends on 1)

The DRT according to claim 1, wherein the internal structure is at a temperature of at least 130° C.

### Claim 11 (depends on 1)

The DRT according to claim 1, wherein the internal structure includes a hydrophobic surface coating.

### Claim 12 (depends on 11)

The DRT according to claim 11, wherein the hydrophobic surface coating comprises micro-features and/or nano-features on at least a portion of the internal structure of the DRT.

### Claim 13 (depends on 1)

The DRT according to claim 1, wherein the internal structure is a polished internal structure, a buffed internal structure, or a combination thereof.

### Claim 14

A method of using a decomposition reactor tube (DRT), comprising:
(a) injecting diesel engine fluid (DEF) into the DRT;
(b) impinging the DEF at an impinging location of an internal structure of the DRT, the impinging location being at a pre-impingement temperature and the DEF being at a first temperature less than the pre-impingement temperature;
(c) conductively transferring heat energy from the impinging location to the impinged DEF such that the DEF reaches a second temperature greater than the first temperature; and
(d) evaporating the impinged DEF from the impinging location of the DRT,
wherein the internal structure comprises a high-thermal conductivity material having a thermal conductivity greater than 20 W/(m·K).

### Claim 15 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material has a thermal conductivity of at least 100 W/(m·K).

### Claim 16 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material has a thermal diffusivity greater than 4.7 mm2·sec−1.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the high-thermal conductivity material has a thermal diffusivity of at least 50 mm2·sec−1.

### Claim 18 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material has a yield strength of at least 300 MPa and a heat capacity of at least 700 J/kg·K.

### Claim 19 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material comprises a ceramic material and/or a metal alloy material.

### Claim 20 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material comprises at least one ceramic material selected from the group consisting of silicon carbide, aluminum nitride, and/or pyrolytic graphite.

### Claim 21 (depends on 14)

The method according to claim 14, wherein the high-thermal conductivity material comprises a metal alloy material selected from the group consisting of an aluminum alloy, a magnesium-scandium alloy, and/or an aluminum-silicon-manganese-magnesium alloy.

### Claim 22 (depends on 14)

The method according to claim 14, further comprising:
applying a hydrophobic surface coating to the internal structure prior to the step of impinging the DEF.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the step of applying includes forming micro-features and/or nano-features on at least a portion of the internal structure of the DRT.

### Claim 24 (depends on 14)

The method according to claim 14, further comprising:
polishing and/or buffing the internal structure prior to the step of impinging the DEF.

### Claim 25 (depends on 14)

The method according to claim 14, wherein the pre-impingement temperature is at least 130° C.