# US 2021/0172085 A1 · SiC SUBSTRATE AND SiC SINGLE CRYSTAL MANUFACTURING METHOD

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0172085 A1
- Document ID: US20210172085A1
- Status: Published application
- Kind: A1
- Application number: 17/113,220
- Filed: 2020-12-07
- Published: 2021-06-10
- Earliest claimed: 2019-12-09
- Assignees: Showa Denko K.K.
- Applicants: Showa Denko K.K.
- Inventors: Akihiro MATSUSE
- Web page: https://patentgrep.com/patent/US20210172085A1

## CPC

- C30B 29/36: Carbides
- C30B 23/02: Epitaxial-layer growth
- C30B 23/066: {Heating of the material to be evaporated}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A SiC substrate contains tantalum or niobium of which the content is equal to or more than 3×1014 cm−3 and equal to or less than 1×1015 cm−3, and nitrogen of which the content is equal to or more than 1×1016 cm −3 and equal to or less than 1×1020 cm−3.

## Claims

### Claim 1

A SiC substrate comprising:
tantalum or niobium of which a content is equal to or more than 3×1014 cm−3 and equal to or less than 1×1015 cm−3; and
nitrogen of which a content is equal to or more than 1×1016 cm−3 and equal to or less than 1×1020 cm−3.

### Claim 2 (depends on 1)

The SiC substrate according to claim 1, wherein
a content of aluminum is less than 1×1016 cm−3.

### Claim 3 (depends on 1)

The SiC substrate according to claim 1, wherein
a content of boron is less than 1×1016 cm−3.

### Claim 4 (depends on 1)

The SiC substrate according to claim 1, wherein
a content of a heavy metal element is less than 1×1014 cm−3.

### Claim 5 (depends on 1)

The SiC substrate according to claim 1, wherein
content ratio of tantalum or niobium differ between those on a first surface and a second surface perpendicular to a thickness direction.

### Claim 6 (depends on 1)

The SiC substrate according to claim 1, further comprising:
a first surface and a second surface perpendicular to a thickness direction,
wherein a content ratio of tantalum or niobium decreases toward the second surface from the first surface.

### Claim 7

A SiC single crystal manufacturing method using a sublimation method in which a single crystal is grown by recrystallizing a gas sublimated from a raw material on a surface of a seed crystal, wherein
the raw material contains tantalum or niobium.

### Claim 8 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
a concentration of tantalum or niobium in the raw material is substantially constant.

### Claim 9 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
a concentration of tantalum or niobium on a surface of the raw material which faces the seed crystal is lower than a concentration of tantalum or niobium inside the raw material.

### Claim 10 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
the tantalum or niobium is deposited on a surface of a SiC raw material.

### Claim 11 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
a concentration of tantalum or niobium on a surface of the raw material which faces the seed crystal is higher than a concentration of tantalum or niobium inside the raw material.

### Claim 12 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
a concentration of tantalum or niobium at the center is higher than a concentration of tantalum or niobium in the outer side when the raw material is seen in a plan view.

### Claim 13 (depends on 7)

The SiC single crystal manufacturing method according to claim 7, wherein
an amount of the tantalum or niobium added is equal to or more than 1 wt % and equal to or less than 8 wt %.

### Claim 14

A SiC single crystal manufacturing method using a sublimation method in which a single crystal is grown by recrystallizing a gas sublimated from a raw material on a surface of a seed crystal, wherein
the raw material is sublimated on the environment in which powder or plate-like tantalum or niobium is positioned between the raw material and the seed crystal.

### Claim 15 (depends on 14)

The SiC single crystal manufacturing method according to claim 14, wherein
the SiC single crystal manufacturing method is a SiC single crystal manufacturing method using a crucible including a protrusion portion that protrudes toward an axial center of the crucible from an inner surface, and
the raw material is sublimated on the environment in which the powder or plate-like tantalum or niobium is positioned on the protrusion portion.