# US 2021/0172046 A1 · Chemical activation of self-passivating metals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0172046 A1
- Document ID: US20210172046A1
- Status: Published application
- Kind: A1
- Application number: 17/112,076
- Filed: 2020-12-04
- Published: 2021-06-10
- Earliest claimed: 2019-12-06
- Assignees: Swagelok Company
- Applicants: Swagelok Company
- Inventors: Cyprian Adair William Illing; Peter C. Williams; Christina Semkow; Todd Johns
- Web page: https://patentgrep.com/patent/US20210172046A1

## CPC

- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/22: of ferrous surfaces
- C21D 1/06: Surface hardening
- C23C 8/26: of ferrous surfaces
- C23C 8/30: Carbo-nitriding
- C23C 8/32: of ferrous surfaces
- C23C 8/34: more than one element being applied in more than one step
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A method for treating a workpiece made from a self-passivating metal and having a Beilby layer is disclosed. The method comprises exposing the workpiece to the vapors produced by heating a reagent having a guanidine [HNC(NH2)2] moiety and complexed with HCl to activate the workpiece for low temperature interstitial surface hardening.

## Claims

### Claim 1

A method for treating a workpiece made from a self-passivating metal and having a Beilby layer comprising:
exposing the workpiece to the vapors produced by heating a reagent having a guanidine [HNC(NH2)2] moiety and complexed with HCl to activate the workpiece for low temperature interstitial surface hardening.

### Claim 2 (depends on 1)

The method of claim 1, wherein the exposing the workpiece surface hardens the workpiece in addition to activating the workpiece.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
maintaining a reaction vessel containing the workpiece at a temperature of 700° C. or less during the exposing; and
wherein the workpiece forming a surface layer that has a carbon concentration of 5 to 15 atomic % and a nitrogen concentration of 5 to 15 atomic % but is substantially free of coarse carbide or coarse nitride precipitates.

### Claim 4 (depends on 3)

The method of claim 3, wherein:
forming the surface layer comprises forming fine carbide precipitates in the surface layer; and
the nitrogen in the surface layer is present primarily as at least one of interstitial nitrogen and fine nitride precipitates.

### Claim 5 (depends on 4)

The method of claim 4, wherein:
forming the fine carbide precipitates does not substantially degrade corrosion resistance provided by a surface passivation layer in the workpiece; and
the surface passivation layer includes chromium oxide.

### Claim 6 (depends on 1)

The method of claim 1 wherein at least one of:
the exposing is performed for a time period of 2 hours or fewer;
the exposing is performed for a time period of 2 minutes or fewer;
maintaining a reaction vessel containing the workpiece at a temperature of 700° C. or less during the exposing;
the reagent includes at least one of Dimethylbiguanide HCl, Guanidine HCl, Biguanide HCl, and Melamine HCl; and
the low temperature interstitial surface hardening occurs simultaneously with the exposing.

### Claim 7 (depends on 1)

The method of claim 1, wherein the case-hardened layer is less than 30 μm thick and comprises:
an outer sublayer that is rich in interstitial nitrogen; and
an inner sublayer that is rich in interstitial carbon.

### Claim 8 (depends on 7)

The method of claim 7, wherein the case-hardened layer is less than 20 μm thick.

### Claim 9 (depends on 1)

The method of claim 1, wherein the low temperature interstitial surface hardening includes at least one of carburizing, nitriding, and nitrocarburization.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reagent includes at least one of an oxygen-free nitrogen halide salt and a non-polymeric N/C/H compound.

### Claim 11 (depends on 1)

The method of claim 1, wherein exposing occurs with the workpiece in a reaction vessel at a distance of 8 inches (20 cm) or more from the reagent.

### Claim 12

A method for producing a case-hardened component in continuous conveyer belt production comprising:
purging an atmosphere of the continuous conveyer belt with gas;
while maintaining the atmosphere at a temperature of 700° C. or less:
placing an untreated component on the continuous conveyer belt;
exposing the workpiece to the vapors produced by heating a reagent having a guanidine [HNC(NH2)2] moiety and complexed with HCl; and
maintaining the exposure to vapors of the reagent over a period of less than 2 hours, whereby the component is activated and surfaced hardened from exposure to the vapors.

### Claim 13 (depends on 12)

The method of claim 12, further comprising:
while maintaining the atmosphere at a temperature of 700° C. or less:
placing a plurality of additional untreated components on the continuous conveyer belt;
exposing the additional components, while on the continuous conveyer belt, to the vapors to activate the additional components; and
performing low temperature surface hardening on the additional components over a period of less than 2 hours.

### Claim 14

A mixture of a first reagent and a second reagent for activating and/or hardening of an alloy, wherein the mixture forms an azeotrope of the first and second reagents and wherein at least one of the reagents includes a guanide-containing reagent.

### Claim 15 (depends on 14)

The mixture of claim 14 having an evaporation point that is lower than the evaporation point of the first reagent.

### Claim 16 (depends on 15)

The mixture of claim 15 wherein at least one of the first and second reagents comprises melamine.

### Claim 17 (depends on 16)

The mixture of claim 16 wherein at least one of the first and second reagents comprises at least one of Biguanide HCl, Dimethylbiguanide HCl, and Guanidine HCl.

### Claim 18 (depends on 14)

The mixture of claim 14 wherein a weight ratio of the first reagent to the second reagent in the mixture is one of 5 to 95%, 10 to 90%, 25 to 75%, and 50 to 50%.

### Claim 19 (depends on 14)

The mixture of claim 14 wherein:
the mixture is formed by fusing or melting the first and second reagent below a boiling point of the first reagent and a boiling point of the second reagent; and
the mixture further includes a petroleum distillate and the petroleum distillate is evaporated leaving a dry mixture of the first and second reagents.

### Claim 20 (depends on 1)

The method of claim 1, further comprising:
applying a heating protocol during the exposing that ramps from a lower to a higher temperature during the exposing to enhance decomposition of the reagent and/or surface harden the workpiece.

### Claim 21 (depends on 20)

The method of claim 20, wherein the lower temperature is approximately 450° C. or greater and the higher temperature is approximately 550° C. or less.

### Claim 22 (depends on 20)

The method of claim 20, wherein the heating protocol is as follows:
maintain a temperature of substantially 470° C. for approximately 30 minutes;
ramp the temperature from approximately 470° C. to approximately 480° C.;
maintain a temperature of 480° C. for approximately 15 minutes;
ramp the temperature from approximately 480° C. to approximately 500° C.; and
maintain a temperature of 500° C. for approximately 15 minutes.

### Claim 23 (depends on 20)

The method of claim 20, wherein the ramping from a lower to a higher temperature includes pulsing the temperature.

### Claim 24 (depends on 20)

The method of claim 20, wherein the heating protocol is as follows:
maintain a temperature of substantially 500° C. for approximately 15 minutes;
ramp the temperature from approximately 500° C. to approximately 480° C.;
maintain a temperature of 480° C. for approximately 15 minutes;
ramp the temperature from approximately 480° C. to approximately 470° C.; and
maintain a temperature of 470° C. for approximately 30 minutes.

### Claim 25

A method for treating a workpiece made from a self-passivating metal and having a Beilby layer comprising:
exposing the workpiece, at an exposing temperature below a temperature at which coarse nitride and/or coarse carbide precipitates form in the workpiece, to vapors produced by heating one or more non-polymeric N/C/H compounds to activate the workpiece for low temperature interstitial surface hardening, wherein the one or more N/C/H compounds:
(a) is solid or liquid at 25° C. and atmospheric pressure;
(b) has a molecular weight of ≤5,000 Daltons; and
(c) can be either uncomplexed or complexed with a hydrohalide acid, and further wherein:
(i) if the non-polymeric N/C/H compound is uncomplexed, any halogen atoms replace one or more labile hydrogen atoms of the non-polymeric N/C/H compound, and
(ii) if the non-polymeric N/C/H compound is complexed, any halogen atoms form a part of the hydrohalide complexing acid.

### Claim 26 (depends on 25)

The method of claim 25, wherein at least one of:
the exposing temperature is between 500-700° C.;
the non-polymeric N/C/H compound has a molecular weight of ≤500 Daltons; and
an exposing time is 1 hour or less.

### Claim 27 (depends on 25)

The method of claim 25, wherein the self-passivating metal comprises at least one of:
a titanium-based alloy;
an iron-based, nickel-based, cobalt based or manganese-based alloys which contains at least 10 wt. % Cr; and
a stainless steel containing 10 to 40 wt. % Ni and 10 to 35 wt. % C.

### Claim 28 (depends on 25)

The method of claim 25, wherein the exposing temperature is about 600° C. or less.

### Claim 29 (depends on 25)

The method of claim 25, wherein the exposing temperature is about 550° C. or less.

### Claim 30 (depends on 1)

A workpiece made according the method of claim 1.

### Claim 31 (depends on 12)

A workpiece made according to the method of claim 12.

### Claim 32 (depends on 25)

A workpiece made according to the method of claim 25.