# US 2021/0172043 A1 · Carbon nano-reinforced aluminum-based conductor material and preparation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0172043 A1
- Document ID: US20210172043A1
- Status: Published application
- Kind: A1
- Application number: 17/106,195
- Filed: 2020-11-30
- Published: 2021-06-10
- Earliest claimed: 2019-11-29
- Assignees: University of Jinan
- Applicants: University of Jinan
- Inventors: Jinfeng LENG; Qingbo ZHOU
- Web page: https://patentgrep.com/patent/US20210172043A1

## CPC

- C22C 1/026: {Alloys based on aluminium}
- C22C 21/00: Alloys based on aluminium
- C22F 1/04: of aluminium or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A carbon nano reinforced aluminum matrix conductive composite and a preparation method thereof are provided. In the preparation method, nano silicon dioxide chemically grows on the surface of graphene oxide, reduced graphene oxide@silicon dioxide carbon nano powder is prepared and reduced in the process of high-temperature sintering, and the mixed powder is blown into a melt using an inert gas, and then stirred, purified and cast.

## Claims

### Claim 1

A carbon nano reinforced aluminum matrix conductive composite comprising the following alloy components in percentage by mass:
0.01˜0.07% of graphene,
0.1˜0.6% of Zr,
≤0.08% of Fe,
≤0.04% of Si,
≤0.01% of each of rest elements, and
the balance of Al.

### Claim 2 (depends on 1)

A preparation method of the carbon nano reinforced aluminum matrix conductive composite according to claim 1, comprising the following steps:
(1) putting an aluminum ingot into a resistance furnace when a temperature of a resistance furnace is raised to 400° C.;
(2) after the aluminum ingot is completely molten, adding Al-5Zr intermediate alloy under a condition that the temperature is raised to 710° C.˜730° C., and carrying out heat preservation on the melt;
(3) blowing graphene@silicon dioxide powder into the aluminum melt using argon while stirring, until the mixed powder is completely blown;
(4) blowing a 6AB refining agent from Pyrotek company using argon, wherein a mass of the added refining agent is 1.2% that of the aluminum melt;
(5) standing and carrying out heat preservation for 5 min, then adding Al-5% Ti—B wires, slagging, discharging, and carrying out water-cold semicontinuous casting to obtain a cast ingot;
(6) cutting off a head and tail of the cast ingot, turning surface scales, and then carrying out extrusion deformation; and
(7) using high-temperature solution and aging treatment to obtain the aluminum matrix composite.

### Claim 3 (depends on 2)

The preparation method according to claim 2, wherein in the step (3), the graphene is 1-5 layers of graphene, and has a particle size of 5˜20 microns.

### Claim 4 (depends on 2)

The preparation method according to claim 2, wherein a preparation method of reduced graphene oxide@silicon dioxide in the step (3) is as follows: KH-550 silane coupling agent solution is prepared, a ratio of ethanol to water is 1˜10:4˜16, a content of KH-550 in the solution is 0.1 vol. %˜1.5 vol. %, and hydrolysis is carried out for 2˜6 h under a condition of standing; graphene oxide is added in the solution so that a concentration of graphene is 0.2˜1.0 g/L, then silicon dioxide powder is added to undergo ultrasonic treatment for 60˜120 min, a particle size of the nano silicon dioxide powder is 10 nm˜50 nm, the solution is subjected to vacuum freeze drying, and then graphene oxide is subjected to reductive sintering for 1˜5 h at a sintering temperature of 1200° C.˜1500° C., so as to obtain the reduced graphene oxide@silicon dioxide composite powder.

### Claim 5 (depends on 4)

The preparation method according to claim 4, wherein in the graphene@silicon dioxide composite powder, a mass of silicon dioxide is 0.5˜5%.

### Claim 6 (depends on 2)

The preparation method according to claim 2, wherein in the step (6), a extrusion heating temperature is 400˜450° C., heat preservation time is 3˜5 h, an extrusion ratio is 20˜30:1, and an extrusion rate is 2.0˜5.0 mm/min.

### Claim 7 (depends on 2)

The preparation method according to claim 2, wherein in the step (7), a solution temperature is 570˜610° C., and heat preservation time is 2˜6 h; an aging temperature is 250˜350° C., and heat preservation time is 24˜72 h.