# US 2021/0171829 A1 · Method for synthesizing perovskite quantum dot film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171829 A1
- Document ID: US20210171829A1
- Status: Published application
- Kind: A1
- Application number: 16/747,504
- Filed: 2020-01-20
- Published: 2021-06-10
- Earliest claimed: 2019-12-04
- Assignees: National Taiwan University of Science and Technology; National Taiwan Normal University; National Taiwan University
- Applicants: National Taiwan University of Science and Technology; National Taiwan Normal University; National Taiwan University
- Inventors: Chih-Hao Chiang; Ting-You Li; Meng-Lin Tsai; Ya-Ju Lee; Hsiang-Chieh Lee
- Web page: https://patentgrep.com/patent/US20210171829A1

## CPC

- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K 11/7704: {Halogenides (C09K11/7701 takes precedence)}
- C09K 11/025: {non-luminescent particle coatings or suspension media}
- C09K 11/664: {Halogenides (C09K11/661 takes precedence)}
- C09K 11/665: {with alkali or alkaline earth metals}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Provided is a method for synthesizing a perovskite quantum dot film, including: preparing a cellulose nanocrystal (CNC) solution, wherein the CNC solution includes a plurality of CNCs with sulfate groups; preparing a precursor solution; mixing the CNC solution and the precursor solution to form a mixed solution; and filtering and drying the mixed solution to form a perovskite quantum dot film.

## Claims

### Claim 1

A method for synthesizing a perovskite quantum dot film, comprising:
preparing a cellulose nanocrystal (CNC) solution, wherein the CNC solution comprises a plurality of CNCs with sulfate groups;
preparing a precursor solution;
mixing the CNC solution and the precursor solution to form a mixed solution; and
filtering and drying the mixed solution to form a perovskite quantum dot film.

### Claim 2 (depends on 1)

The method for synthesizing the perovskite quantum dot film according to claim 1, wherein preparing the CNC solution comprises:
dissolving CNC powder in water to form a first solution; and
dissolving the first solution in an organic solvent to form the CNC solution.

### Claim 3 (depends on 2)

The method for synthesizing the perovskite quantum dot film according to claim 2, wherein flexibility and a tensile property of the perovskite quantum dot film increase with an increase of a water content of the first solution.

### Claim 4 (depends on 1)

The method for synthesizing the perovskite quantum dot film according to claim 1, wherein the perovskite quantum dot film comprises a plurality of perovskite quantum dots uniformly distributed among the CNCs.

### Claim 5 (depends on 4)

The method for synthesizing the perovskite quantum dot film according to claim 4, wherein the sulfate groups of the CNCs are connected with the perovskite quantum dots to improve stability of the perovskite quantum dot film.

### Claim 6 (depends on 4)

The method for synthesizing the perovskite quantum dot film according to claim 4, wherein the perovskite quantum dot is represented by the following formula (1):
ABX3 (1),
wherein A comprises an inorganic cation or an organic amine, the inorganic cation comprises Li, Na, K, Rb, Cs or a combination thereof, and the organic amine comprises ammonia, methylamine, formamidine acetate, formamidine amine, formamidine, ethylenediamine, dimethylamine, imidazole, acetamidine, propylamine, isopropylamine, trimethylenediamine, ethylamine, butylamine, isobutylamine, tert-butylamine, diethylamine, 5-aminovaleric acid, 2-thiophene methylamine, hexylamine, aniline, benzylamine, phenylethylamine, octylamine, decylamine, dodecylamine, tetradecylamine, hexadecylamine, octadecylamine, eicosamine or a combination thereof; B comprises Cd, Co, Cr, Cu, Fe, Ge, Pb, Sn or a combination thereof; and X comprises halogen.

### Claim 7 (depends on 6)

The method for synthesizing the perovskite quantum dot film according to claim 6, wherein preparing the precursor solution comprises:
providing a first precursor comprising A and X;
providing a second precursor comprising B and X; and
adding the first precursor and the second precursor into an organic solvent and uniformly mixing the first precursor, the second precursor and the organic solvent.

### Claim 8 (depends on 7)

The method for synthesizing the perovskite quantum dot film according to claim 7, wherein a wavelength of light emitted by the perovskite quantum dots increases with an increase of a concentration of the precursor solution.

### Claim 9 (depends on 1)

The method for synthesizing the perovskite quantum dot film according to claim 1, wherein each CNC has a length of 100 nm to 300 nm and a width of 3 nm to 20 nm.

### Claim 10 (depends on 1)

The method for synthesizing the perovskite quantum dot film according to claim 1, wherein a molecular weight of the CNC is 14700 to 27850.