# US 2021/0171774 A1 · Compatibilizer precursor, methods, systems, and uses thereof, and formulations including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171774 A1
- Document ID: US20210171774A1
- Status: Published application
- Kind: A1
- Application number: 17/112,489
- Filed: 2020-12-04
- Published: 2021-06-10
- Earliest claimed: 2019-12-06
- Assignees: Building Materials Investment Corporation
- Applicants: Building Materials Investment Corporation
- Inventors: Denis Muki Tibah
- Web page: https://patentgrep.com/patent/US20210171774A1

## CPC

- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C08L 17/00: Compositions of reclaimed rubber
- C08L 91/00: Compositions of oils, fats or waxes; Compositions of derivatives thereof
- C08L 93/04: Rosin
- C09D 195/00: Coating compositions based on bituminous materials, e.g. asphalt, tar, pitch
- C08L 2205/035: containing four or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Some embodiments of the present disclosure relate to a method comprising mixing at least one compatibilizer precursor with at least one polymer, so as to result in a polymer concentrate and mixing the polymer concentrate with asphalt, so as to result in a polymer modified asphalt (“PMA”). Some embodiments of the present disclosure relate to formulations comprising a compatibilizer precursor, a polymer concentrate, PMA, or any combination thereof.

## Claims

### Claim 1

A method comprising:
mixing at least one compatibilizer precursor with at least one polymer, so as to result in a polymer concentrate,
wherein the at least one polymer is mixed with the at least one compatibilizer precursor in a weight ratio of the at least one polymer to the at least one compatibilizer precursor of 1:100 to 2:1;
mixing the polymer concentrate with asphalt, so as to result in a polymer modified asphalt (“PMA”).

### Claim 2 (depends on 1)

The method of claim 1, wherein the at least one compatibilizer precursor comprises at least one resin, at least one process oil, or any combination thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein the at least one resin comprises least one terpene resin, at least one petroleum resin, at least one hydrogenated rosin, at least one rosin milk, at least one petroleum resin emulsion, at least one terpene-phenolic resin, at least one hydrogenated petroleum resin, at least one aliphatic hydrocarbon resin, at least one hydrogenated aliphatic hydrocarbon resin, at least one aromatic modified aliphatic hydrocarbon resin, at least one hydrogenated aromatic modified aliphatic hydrocarbon resin, at least one polycyclopentadiene resin, at least one hydrogenated polycyclopentadiene resin, at least one cycloaliphatic hydrocarbon resin, at least one hydrogenated cycloaliphatic resin, cycloaliphatic/aromatic hydrocarbon resin, at least one hydrogenated cycloaliphatic/aromatic hydrocarbon resin, hydrogenated aromatic hydrocarbon resin, at least one maleic acid/anhydride modified tackifier, terpene modified aromatic and/or aliphatic hydrocarbon resin, at least one hydrogenated terpene modified aromatic and/or aliphatic hydrocarbon resin, at least one polyterpene resin, at least one hydrogenated polyterpene resin, at least one aromatic modified polyterpene resin, at least one hydrogenated aromatic modified polyterpene resin, at least one terpene-phenol resin, at least one hydrogenated terpene-phenol resin, at least one gum rosin resin, at least one hydrogenated gum rosin resin, at least one gum rosin ester resin, at least one wood rosin resin, at least one hydrogenated wood rosin resin, at least one rosin acid resin, at least one hydrogenated rosin acid resin, or any combination thereof.

### Claim 4 (depends on 2)

The method of claim 2, wherein the at least one process oil comprises at least one paraffinic oil, at least one petroleum extract, at least one vegetable oil, at least one naphthenic oil, at least one aromatic oil, at least one re-refined engine oil bottom (REOB), at least one engine oil residue (EOR), at least one re-refined heavy vacuum distillation bottom (RHVDB), at least one re-refined heavy vacuum distillation oil (RHVDO), at least one re-refined vacuum tower bottom (RVTB), at least one vacuum tower bottom (VTB), or any combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the at least one polymer comprises at least one polyolefin, oxidized polyethylene (OPE), polyethylene-polypropylene elastomer, ground tire rubber (GTR), isotactic polypropylene (IPP), atactic polypropylene (APP), styrene-butadiene-styrene (SBS) copolymer, a styrene-ethylene-butylene-styrene (SEBS) copolymer, polyvinyl butyral (PVB) or any combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the polymer concentrate has a softening point of at least 195° F. as measured according to ASTM D36.

### Claim 7 (depends on 1)

The method of claim 1, wherein the polymer concentrate has a softening point of 195° F. to 350° F. as measured according to ASTM D36.

### Claim 8 (depends on 1)

The method of claim 1, wherein the polymer concentrate has a penetration point (“PEN”) of at least 15 dmm as measured according to ASTM D5.

### Claim 9 (depends on 1)

The method of claim 1, wherein the polymer concentrate has a penetration point of 15 dmm to 200 dmm as measured according to ASTM D5.

### Claim 10 (depends on 1)

The method of claim 1, wherein the polymer concentrate exhibits an elongation of 50% to 10,000% as tested according to ASTM D828.

### Claim 11 (depends on 1)

The method of claim 1, wherein the asphalt has a softening point of at least 100° F. as measured according to ASTM D36.

### Claim 12 (depends on 1)

The method of claim 1, wherein the asphalt has a softening point of 100° F. to 250° F. as measured according to ASTM D36.

### Claim 13 (depends on 1)

The method of claim 1, wherein the asphalt has a penetration point of at least 2 dmm as measured according to ASTM D5.

### Claim 14 (depends on 1)

The method of claim 1, wherein the asphalt has a penetration point of 1 dmm to 50 dmm as measured according to ASTM D5.

### Claim 15 (depends on 1)

The method of claim 1, wherein the polymer modified asphalt has a softening point of at least 120° F. as measured according to ASTM D36.

### Claim 16 (depends on 1)

The method of claim 1, wherein the polymer modified asphalt has a softening point of 120° F. to 300° F. as measured according to ASTM D36.

### Claim 17 (depends on 1)

The method of claim 1, wherein the polymer modified asphalt has a penetration point of at least 10 dmm as measured according to ASTM D5.

### Claim 18 (depends on 1)

The method of claim 1, wherein the polymer modified asphalt has a penetration point of 10 dmm to 50 dmm as measured according to ASTM D5.

### Claim 19 (depends on 1)

The method of claim 1, further comprising adding at least one filler, at least one additive, or any combination thereof to the polymer modified asphalt, so as to result in a filled polymer modified asphalt (“PMA”) coating.

### Claim 20 (depends on 19)

The method of claim 19, wherein the at least one filler, the at least one additive, or combination thereof, comprises transoctenamer rubber (TOR) a propylene-based elastomer, at least one wax, calcium carbonate, barium sulfate, calcium sulfate, talc, limestone, perlite, silica, fumed silica, precipitated silica, quartz, aluminum trihydrate, magnesium hydroxide, colemanite, titanium dioxide, snow white, fly ash, graphene nanoparticles, carbon black, recycled rubber tires, recycled shingles, recycled thermoplastic resins, basalt, roofing granules, clay, ammonium polyphosphate, graphite, or any combination thereof.

### Claim 21 (depends on 19)

The method of claim 19, wherein the filled PMA coating has a softening point of at least 200° F. as measured according to ASTM D36.

### Claim 22 (depends on 19)

The method of claim 19, wherein the filled PMA coating has a softening point of 200° F. to 320° F. as measured according to ASTM D36.

### Claim 23 (depends on 19)

The method of claim 19, wherein the filled PMA coating has a penetration point (“PEN”) of at least 5 dmm as measured according to ASTM D5.

### Claim 24 (depends on 19)

The method of claim 19, wherein the filled PMA coating has a penetration point (“PEN”) of 5 dmm to 40 dmm as measured according to ASTM D5.

### Claim 25 (depends on 1)

The method of claim 1, wherein mixing the at least one compatibilizer precursor with the at least one polymer is performed over a time period of 3 minutes to 90 minutes.

### Claim 26 (depends on 1)

The method of claim 1, wherein mixing the polymer concentrate with asphalt is performed over a time period of 45 minutes to 90 minutes.

### Claim 27 (depends on 1)

The method of claim 1, wherein the polymer concentrate is mixed with the asphalt in a weight ratio of the polymer concentrate to the asphalt of 1:50 to 1:1.

### Claim 28

A formulation consisting essentially of:
at least one polymer; and
at least one compatibilizer precursor;
wherein the at least one polymer is present in the formulation in a weight ratio of the at least one polymer to the at least one compatibilizer precursor of 1:100 to 2:1; and
wherein the formulation is a polymer concentrate.

### Claim 29

A formulation consisting essentially of:
at least one polymer;
at least one compatibilizer precursor;
asphalt;
optionally, at least one filler; and
optionally, at least one additive;
wherein the at least one polymer is present in the formulation in a weight ratio of the at least one polymer to the asphalt of 1:100 to 1:2;
wherein the at least one compatibilizer precursor is present in the formulation in a weight ratio of the at least one compatibilizer precursor to the asphalt of 1:50 to 1:1;
wherein the formulation is a polymer modified asphalt (PMA).

### Claim 30

A formulation comprising:
at least one polymer;
at least one compatibilizer precursor; and
asphalt;
wherein the at least one polymer is present in the formulation in a weight ratio of the at least one polymer to the asphalt of 1:100 to 1:2;
wherein the at least one compatibilizer precursor is present in the formulation in a weight ratio of the at least one compatibilizer precursor to the asphalt of 1:50 to 1:1; and
wherein the formulation is a polymer modified asphalt (PMA).

### Claim 31 (depends on 28)