# US 2021/0171767 A1 · Thermoplastic compositions having good stability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171767 A1
- Document ID: US20210171767A1
- Status: Published application
- Kind: A1
- Application number: 16/771,722
- Filed: 2018-12-17
- Published: 2021-06-10
- Earliest claimed: 2017-12-19
- Assignees: Covestro Deutschland AG
- Applicants: Covestro Deutschland AG
- Inventors: Andreas Seidel; Helmut Werner Heuer; Rolf Wehrmann
- Web page: https://patentgrep.com/patent/US20210171767A1

## CPC

- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08L 69/005: {Polyester-carbonates}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The invention relates to a composition for production of a thermoplastic moulding compound, wherein the composition comprises or consists of at least the following constituents: A) 30% to 94% by weight of a polymer or polymer mixture consisting of at least one representative selected from aromatic polycarbonate and aromatic polyestercarbonate and optionally additionally comprising aromatic polyester, B) 5% to 65% by weight of rubber-based graft polymer B.1, optionally in a mixture with rubber-free vinyl (co)polymer B.2, C) 0.001% to 1% by weight of at least one ester of a sulfonic acid, D) 0% to 30% by weight of one or more polymer additives, and to a process for producing the moulding compound, to the moulding compound itself, to the use of the composition or of the moulding compound for production of moulded articles and to the moulded articles themselves.

## Claims

### Claim 1

A thermoplastic moulding composition, wherein the composition comprises:
A) 30% to 94% by weight of a polymer or polymer mixture comprising an aromatic polycarbonate or an aromatic polyestercarbonate and optionally further comprising an aromatic polyester,
B) 5% to 65% by weight of rubber-based graft polymer B.1, optionally in a mixture with rubber-free vinyl (co)polymer B.2,
C) 0.001% to 1% by weight of at least one ester of a sulfonic acid,
D) 0% to 30% by weight of one or more polymer additives.

### Claim 2 (depends on 1)

The composition of claim 1, wherein component A is an aromatic polycarbonate.

### Claim 3 (depends on 1)

The composition of claim 1, wherein component C is selected from at least one compound of the formulae (XI) to (XVI)
where R12 in the formulae (XI) to (XVI) is in each case independently C6- to C20-aryl or C7- to C12-aralkyl.

### Claim 4 (depends on 1)

The composition of claim 1, wherein component C is the sulfonic ester of formula (XVII)

### Claim 5 (depends on 1)

The composition of claim 1 comprising:
50-75% by weight of component A,
20-45% by weight of component B,
0.005-0.05% by weight of component C and
0.2-5% by weight of component D.

### Claim 6 (depends on 1)

The composition of claim 1, wherein component B has a lithium content of <1 mg/kg.

### Claim 7 (depends on 1)

The composition of claim 1, wherein component D comprises at least one additive selected from the group consisting of lubricants and demoulding agents, stabilizers, flowability promoters, compatibilizers, and dyes and pigments.

### Claim 8 (depends on 1)

The composition according to of claim 1, wherein component A has a proportion of phenolic OH end groups of at least 200 mg/kg.

### Claim 9

A process for producing an impact-modified thermoplastic moulding compound comprising:
A) 30% to 94% by weight of a polymer or polymer mixture consisting of at least one of an aromatic polycarbonate and aromatic polyestercarbonate and optionally further comprising an aromatic polyester,
B) 5% to 65% by weight of a rubber-based graft polymer B.1, optionally in a mixture with rubber-free vinyl (co)polymer B.2, and
D) 0% to 30% by weight of one or more polymer additives,
wherein the components are mixed with one another and melted and interdispersed at a temperature of 200 to 350° C. in a compounding unit,
wherein component C is added to the composition, an ester of a sulfonic acid in a concentration of 0.001% to 1% by weight, and
wherein components A, B, C and D and any further components of the composition are mixed in a single step, or alternatively, component C is first premixed in a first step with the entirety or a portion of component A at room temperature or at an elevated temperature.

### Claim 10 (depends on 9)

The process of claim 9, wherein component A is aromatic polycarbonate and/or aromatic polyestercarbonate containing Fries structures of at least one of the formulae (IV) to (VII)
in which the phenyl rings may each independently be mono- or di-substituted by C1-C8-alkyl, or halogen, and
where A is
a single bond, C1 to C5-alkylene, C2 to C5-alkylidene, C5 to C6-cycloalkylidene, —O—, —SO—, —CO—, —S—, —SO2—, C6 to C12-arylene, onto which further aromatic rings optionally containing heteroatoms may be fused,
or a radical of formula (II) or (III)
wherein
R5 and R6 can be chosen individually for each X1 and are independently hydrogen or C1 to C6-alkyl,
X1 is carbon and
m represents an integer from 4 to 7,
with the proviso that, on at least one X1 atom, R5 and R6 are both alkyl, and
wherein component A contains structural units (IV) to (VII) in an amount that adds up to 50 to 10 000 mg/kg, based on the sum total of the proportions by weight of the polycarbonates and polyestercarbonates present in component A.

### Claim 11 (depends on 9)

The process of claim 9, wherein component C is selected from at least one compound of the formulae (XI) to (XVI)
where R12 in the formulae (XI) to (XVI) is in each case independently C6- to C20-aryl or C7- to C12-aralkyl.

### Claim 12 (depends on 9)

The process of claim 9, wherein component B contains lithium in a concentration of >1 mg/kg.

### Claim at position 13

13-15. (canceled)