# US 2021/0171749 A1 · Improving rheological properties of thermoplastic polyolefin compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171749 A1
- Document ID: US20210171749A1
- Status: Published application
- Kind: A1
- Application number: 17/052,233
- Filed: 2019-05-17
- Published: 2021-06-10
- Earliest claimed: 2018-05-18
- Assignees: Abu Dhabi Polymers Co. Ltd (Borouge) LLC.; Borealis AG
- Applicants: Abu Dhabi Polymers Co. Ltd (Borouge) LLC.; Borealis AG
- Inventors: Ashish KUMAR; Joel FAWAZ; Umesh Balkrishna GADGOLI; Senthil Kumar KALIAPPAN
- Web page: https://patentgrep.com/patent/US20210171749A1

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08J 5/18: Manufacture of films or sheets
- C08K 5/3415: Five-membered rings
- C08J 3/24: Crosslinking, e.g. vulcanising, of macromolecules (mechanical aspects B29C35/00; crosslinking agents C08K)
- C08K 5/17: Amines; Quaternary ammonium compounds
- C08K 2201/019: the composition being defined by the absence of a certain additive
- C08L 2203/16: used for films
- C08L 2203/18: used for pipes
- C08L 2207/04: Thermoplastic elastomer
- C08L 2207/062: HDPE
- F16L 9/12: of plastics with or without reinforcement (F16L9/16 - F16L9/22 take precedence)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

The present invention relates to process for preparing a thermoplastic polyolefin composition comprising a) providing a reactive polyolefin composition comprising a polyolefin resin and a rheology modifier, which is free of peroxide initiator; b) heating the reactive polyolefin composition to a temperature of 180° C. to 300° C.; and c) subjecting the reactive polyolefin composition to a specific energy of equal to or more than 0.15 kWh/kg to obtain the thermoplastic polyolefin composition, the thermoplastic polyolefin composition obtainable by said process, an article comprising said thermoplastic polyolefin composition and the use of a rheology modifier, which is free of peroxide initiator, in said reactive polyolefin composition for increasing the viscosity at a constant shear stress of 747 Pa of the thermoplastic polyolefin composition, eta747 (Comp), by reacting the polyolefin resin and the rheology modifier at a temperature in the range of from 180° C. to 300° C. and a specific energy equal to or greater than 0.15 kWh/kg.

## Claims

### Claim 1

A reactive polyolefin composition, which is a precursor to a thermoplastic polyolefin composition, comprising:
(A) a polyolefin resin; and
(B) a rheology modifier, which is free of a peroxide initiator,
wherein the polyolefin resin (A) and the rheology modifier (B) are reactive to form the thermoplastic polyolefin composition at a temperature in the range of from 180° C. to 300° C. and a specific energy equal to or greater than 0.15 kWh/kg.

### Claim 2 (depends on 1)

The reactive polyolefin composition according to claim 1, wherein the rheology modifier (B) is a cyclic imide derivative and/or wherein the polyolefin resin (A) and the rheology modifier (B) are reactive to form the thermoplastic polyolefin in a compounder and/or wherein the thermoplastic polyolefin composition is formed by compounding.

### Claim 3 (depends on 1)

The reactive polyolefin composition according to claim 1, wherein the rheology modifier (B) is present in the reactive polyolefin composition in an amount of up to 0.5 wt %, based on the total amount of the reactive polyolefin composition or wherein the rheology modifier (B) is present in the reactive polyolefin composition in an amount in the range of 50 to 2000 ppm, based on the total amount of the reactive polyolefin composition.

### Claim 4 (depends on 1)

The reactive polyolefin composition according to claim 1, wherein the polyolefin resin (A) is selected from a polyethylene resin, a polypropylene resin and blended mixtures thereof.

### Claim 5 (depends on 1)

The reactive polyolefin composition according to claim 1, wherein the polyolefin resin (A) is unimodal, bimodal or multimodal and/or wherein the polyolefin resin (A) is a polyethylene resin selected from linear low density polyethylene (LLDPE) resin, medium density polyethylene (HDPE) resin and high density polyethylene (HDPE) resin.

### Claim 6 (depends on 1)

The reactive polyolefin composition according to claim 1, wherein the reactive polyolefin composition is free of peroxide radical initiation agents or any other coagents.

### Claim 7 (depends on 1)

A process for preparing a thermoplastic polyolefin composition comprising:
a) providing a reactive polyolefin composition according to claim 1;
b) heating the reactive polyolefin composition to a temperature of 180° C. to 300° C.; and
c) subjecting the reactive polyolefin composition to a specific energy of equal to or more than 0.15 kWh/kg to obtain the thermoplastic polyolefin composition.

### Claim 8 (depends on 7)

The process according to claim 7, wherein process steps (b) and (c) are carried out simultaneously in a compounder.

### Claim 9 (depends on 8)

The process according to claim 8, wherein the compounder is an extruder and the extruder is operated at a mixer speed in the range of from 200 to 750 rpm.

### Claim 10 (depends on 7)

The process according to claim 7, wherein the specific energy is provided by shearing force.

### Claim 11 (depends on 7)

The process according to claim 7, wherein the thermoplastic polyolefin composition has a viscosity at a constant shear stress of 747 Pa, eta747 (Comp), which is at least 10% higher than the viscosity at a constant shear stress of 747 Pa of the polyolefin composition based on polyolefin resin (A) without the rheology modifier (B), eta747 (A).

### Claim 12 (depends on 7)

The process according to claim 7, wherein the thermoplastic polyolefin composition has a complex viscosity at a shear rate of 0.05 rad/s, eta0.05 (Comp), which is at least 5% higher than the complex viscosity at a shear rate of 0.05 rad/s of the polyolefin composition based on polyolefin resin (A) without the rheology modifier (B), eta0.05 (A), and/or wherein the thermoplastic polyolefin composition has a melt flow rate MFR5 (Comp), which is not more than 90% of the melt flow rate of the polyolefin composition based on polyolefin resin (A) without the rheology modifier (B), MFR5 (A), and/or wherein the thermoplastic polyolefin composition has a flow rate ratio FRR21/5 (Comp), which is at least 1.0% higher than the flow rate ratio of the polyolefin composition based on polyolefin resin (A) without the rheology modifier (B), FRR21/5 (A), and/or wherein the thermoplastic polyolefin composition has a flow rate ratio FRR21/5 (Comp), which is in the range from 0.5% to 35% higher than the flow rate ratio of the polyolefin composition based on polyolefin resin (A) without the rheology modifier (B), FRR21/5 (A), and/or wherein the thermoplastic polyolefin composition has a flow rate ratio FRR21/5 (Comp), which is between 5 and 55.

### Claim 13 (depends on 7)

A thermoplastic polyolefin composition prepared by the process according to claim 7.

### Claim 14 (depends on 13)

An article comprising the thermoplastic polyolefin composition according to claim 13.

### Claim 15

(canceled)