# US 2021/0171727 A1 · Elastic sulfonated styrene diene block copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171727 A1
- Document ID: US20210171727A1
- Status: Published application
- Kind: A1
- Application number: 16/770,666
- Filed: 2018-12-06
- Published: 2021-06-10
- Earliest claimed: 2017-12-07
- Assignees: Rensselaer Polytechnic Institute
- Applicants: Rensselaer Polytechnic Institute
- Inventors: Chulsung BAE
- Web page: https://patentgrep.com/patent/US20210171727A1

## CPC

- C08J 5/2231: {based on macromolecular compounds obtained by reactions involving unsaturated carbon-to-carbon bonds}
- C08F 8/04: Reduction, e.g. hydrogenation
- C08F 8/06: Oxidation
- C08F 8/34: Introducing sulfur atoms or sulfur-containing groups
- C08F 8/36: Sulfonation; Sulfation
- C08F 36/06: Butadiene
- C08F 36/08: Isoprene
- C08K 5/37: Thiols
- C08L 25/08: Copolymers of styrene (C08L29/08, C08L35/06, C08L55/02 take precedence)
- C08L 53/025: {modified}
- C08L 65/02: Polyphenylenes
- C08L 71/12: Polyphenylene oxides
- C08L 81/06: Polysulfones; Polyethersulfones
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- H01M 8/1072: by chemical reactions, e.g. in situ polymerisation or in situ crosslinking
- H01M 8/1088: Chemical modification, e.g. sulfonation
- C08J 2353/02: of vinyl aromatic monomers and conjugated dienes
- C08L 2312/00: Crosslinking
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The electrochemical energy conversion system include an anode, a cathode, and a proton exchange membrane disposed between the anode and the cathode. The proton exchange membrane includes a polymer having a hard block polymer, a soft block polymer, and one or more hydrophilic functional groups attached to the soft block polymer. The glass transition temperature of the hard block polymer is higher than a glass transition temperature of the soft block polymer, such that the hard block polymer is non-elastic and the soft block polymer is elastic at a desired operating temperature. The hydrophilic functional groups are attached to the soft block polymer via a thiol-ene reaction to modify double bonds in the soft block polymer. The swellable functional groups are selectively connected to the soft domains of the block copolymers, so that when the membrane swells (under hydration or gas adsorption), the stress is effectively absorbed by the soft domain and the impact on overall mechanical properties is minor, resulting in more durable membranes.

## Claims

### Claim 1

A proton exchange membrane material comprising a polymer according to formula I:
wherein R1 a hard block polymer, R2 is a soft block polymer, and R3 includes one or more hydrophilic functional groups;
wherein a glass transition temperature of the hard block polymer is higher than a glass transition temperature of the soft block polymer.

### Claim 2 (depends on 1)

The material according to claim 1, wherein the glass transition temperature of the hard block polymer is greater than or equal to 100° C.

### Claim 3 (depends on 1)

The material according to claim 1, wherein the hard block polymer is polystyrene, p-tert-butylstyrene, polysulfone, poly(phenylene oxide), poly(phenylene), or combinations thereof.

### Claim 4 (depends on 1)

The material according to claim 1, wherein the soft block polymer is polybutadiene, polyisoprene, or combinations thereof.

### Claim 5 (depends on 1)

The material according to claim 1, wherein the hydrophilic functional group is a sulfonate group.

### Claim 6 (depends on 1)

The material according to claim 1, wherein the hydrophilic functional group is attached to the soft block polymer via a thiol-ene reaction to modify a double bond in the soft block polymer.

### Claim 7 (depends on 1)

The material according to claim 1, wherein the polymer includes the structure according to formula II:
wherein a is about 20 mol % and b is about 80 mol %.

### Claim 8

A method of making a proton exchange membrane material, the method comprising:
providing a reaction medium including a copolymer chain, the copolymer chain including a hard block polymer and a soft block polymer;
attaching a functional group to the soft block polymer;
saturating the soft block polymer; and
oxidizing the functional group.

### Claim 9 (depends on 8)

The method according to claim 8, wherein attaching a functional group to the soft block polymer includes:
performing a thiol-ene reaction to attach a thioester group to the soft block polymer.

### Claim 10 (depends on 8)

The method according to claim 8, wherein saturating the soft block polymer includes:
hydrogenating the soft block polymer;
crosslinking the copolymer chain with other copolymer chains;
or combinations thereof.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the glass transition temperature of the hard block polymer is higher than a glass transition temperature of the soft block polymer.

### Claim 12 (depends on 8)

The method according to claim 8, wherein a glass transition temperature of the hard block polymer is greater than or equal to 100° C.

### Claim 13 (depends on 8)

The method according to claim 8, wherein the hard block polymer is polystyrene, p-tert-butylstyrene, polysulfone, poly(phenylene oxide), poly(phenylene), or combinations thereof.

### Claim 14 (depends on 8)

The method according to claim 8, wherein the soft block polymer is polybutadiene, polyisoprene, or combinations thereof.

### Claim 15 (depends on 9)

The method according to claim 9, wherein oxidizing the functional group includes:
oxidizing the sulfur of the thioester group to a sulfonate.

### Claim 16 (depends on 8)

The method according to claim 8, wherein the material includes the structure according to formula II:
wherein a is about 20 mol % and b is about 80 mol %.

### Claim 17

An electrochemical energy conversion system comprising:
an anode;
a cathode; and
a proton exchange membrane disposed between the anode and the cathode, the proton exchange membrane including a polymer according to formula I:
wherein R1 a hard block polymer, R2 is a soft block polymer, and R3 includes one or more hydrophilic functional groups;
wherein a glass transition temperature of the hard block polymer is higher than a glass transition temperature of the soft block polymer.

### Claim 18 (depends on 17)

The system according to claim 17, wherein the hard block polymer is a polystyrene, p-tert-butylstyrene, polysulfone, poly(phenylene oxide), poly(phenylene), or combinations thereof; the soft block polymer is polybutadiene, polyisoprene, or combinations thereof.

### Claim 19 (depends on 17)

The system according to claim 17, wherein the hydrophilic functional group is a sulfonate group.

### Claim 20 (depends on 17)

The system according to claim 17, wherein the polymer includes the structure according to formula II: