# US 2021/0171719 A1 · Linear polydimethylsiloxane-polyoxyalkylene block copolymers of the structure type aba

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171719 A1
- Document ID: US20210171719A1
- Status: Published application
- Kind: A1
- Application number: 17/048,709
- Filed: 2019-05-07
- Published: 2021-06-10
- Earliest claimed: 2018-05-17
- Assignees: Evonik Operations GmbH
- Applicants: Evonik Operations GmbH
- Inventors: Wilfried Knott; Horst Dudzik; Frauke Henning
- Web page: https://patentgrep.com/patent/US20210171719A1

## CPC

- C08G 77/08: characterised by the catalysts used
- C08G 77/10: Equilibration processes
- C08G 77/14: containing silicon bound to oxygen-containing groups
- C08G 77/18: to alkoxy or aryloxy groups
- C08G 77/46: containing polyether sequences
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Equilibrated trifluoromethanesulfonic acid-acidified α,ω-diacetoxypolydimethylsiloxanes, processes for the production thereof and SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers of the structure type ABA and a process for the production thereof are described, wherein the production of SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers of the structure type ABA is effected by reacting trifluoromethanesulfonic acid-acidified acetoxysiloxane with polyetherols optionally in the presence of buffer mixtures and optionally an additional condensation catalyst and optionally in the presence of an inert solvent.

## Claims

### Claim 1

A process for producing trifluoromethanesulfonic acid-acidified equilibrated α,ω-diacetoxypolydimethylsiloxanes, wherein cyclic siloxanes comprising D4 and/or D5, are reacted with acetic anhydride using trifluoromethanesulfonic acid as catalyst and with addition of acetic acid.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the trifluoromethanesulfonic acid is employed in amounts of from 0.1 to 0.3 percent by mass based on the reaction matrix consisting of acetic anhydride and cyclic siloxanes.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the reaction is performed in a temperature range of from 140° C. to 160° C. and over a period of from 4 to 8 hours.

### Claim 4 (depends on 1)

The process according to claim 1, wherein acetic acid is added in amounts of from 0.4 to 3.5 percent by weight, based on the reaction matrix consisting of acetic anhydride and cyclic siloxanes.

### Claim 5

A trifluoromethanesulfonic acid-acidified, equilibrated α,ω-diacetoxypolydimethylsiloxanes of general formula
where R=methyl,
which have an average chain length determined by 29Si-NMR spectroscopy of 0≤X≤250 and contain from 0.1 to 0.3 percent by mass of trifluoromethanesulfonic acid and from 5 to 43 val % of free acetic anhydride based on the acetic anhydride equivalent chemically bonded in the α,ω-diacetoxypolydimethylsiloxane.

### Claim 6 (depends on 5)

The trifluoromethanesulfonic acid-acidified, equilibrated α,ω-diacetoxypolydimethylsiloxanes according to claim 5, wherein they have an average chain length determined by 29Si-NMR spectroscopy of 10<X<30.

### Claim 7

(canceled)

### Claim 8 (depends on 5)

The process for producing SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers of the structure type ABA, wherein trifluoromethanesulfonic acid-acidified, equilibrated α,ω-diacetoxypolydimethylsiloxane, preferably according to claim 5, is reacted with polyether monools in the presence of buffer mixtures and optionally an additional condensation catalyst and in the presence of an inert solvent.

### Claim 9 (depends on 8)

The process according to claim 8, wherein the amount of the base employed for treating the polyether monool in the buffer mixture is measured such that it corresponds at least to the stoichiometric equivalent, preferably at least to the 2-fold stoichiometric equivalent, of the trifluoromethanesulfonic acid present in the α,ω-diacetoxypolydimethylsiloxane.

### Claim 10 (depends on 8)

The process according to claim 8, wherein the polyether monool is initially treated with buffer mixtures and optionally an additional α,ω-diacetoxypolydimethylsiloxane,
and then using an azeotrope-forming solvent the liberated acetic acid and the acetic acid that may be present in the system is thermally removed together with the solvent and the obtained SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymer is neutralized by addition of an auxiliary base, filtered and end stabilized.

### Claim 11 (depends on 8)

The process according t claim 8, wherein a condensation catalyst is used for reacting the equilibrated α,ω-diacetoxypolydimethylsiloxane with polyether monools,
wherein condensation catalysts employed are Brönsted acids,
wherein the condensation catalyst, in particular the trichloroacetic acid, is in the range from 0.1 to 0.7 percent by mass, based on the total amount of the reactants provided for the SiOC-bond forming reaction, namely α,ω-diacetoxypolydimethylsiloxane and polyether monool.

### Claim 12 (depends on 8)

The process according to claim 8, wherein the employed buffer mixtures contain at least proportions of the condensation catalyst and particularly preferably contain the condensation catalyst in the form of a salt.

### Claim 13 (depends on 8)

The process according to claim 8, wherein the buffer mixtures comprise sodium trichloroacetate and acetic acid or sodium acetate and acetic acid.

### Claim 14 (depends on 8)

The process according to claim 8, wherein solvents employed are aromatic,
or
in that the process is operated solventlessly.

### Claim 15 (depends on 8)

The process according to claim 8, wherein the replacement of the acetoxy groups bonded to the α,ω-diacetoxypolydimethylsiloxane by reaction with polyether monools to afford SiOC-bonded, linear polyether siloxanes is effected in the presence of solvents by intimate mixing of the reactants with stirring at reaction temperatures of from 20° C. to 90° C. and from 30 minutes to 8 hours,
and/or,
in that the removal of the acetic acid liberated during the reaction between α,ω-diacetoxypolydimethylsiloxane and polyether monools and the acetic acid that may be present in the system is preferably effected by distillation at temperatures between 60° C. and 90° C. with application of an auxiliary vacuum.

### Claim 16 (depends on 8)

The process according to claim 8, wherein the molar ratio of the reactants is preferably measured such that at least 1 mol of polyether-bonded OH functionality is employed per mol of acetoxy group of the α,ω-diacetoxypolydimethylsiloxane.

### Claim 17 (depends on 8)

The linear SiOC-bonded polydimethylsiloxane-polyoxyalkylene block copolymers of the structure type ABA obtainable according to claim 8 and the use thereof as a surfactant additive in noncorrosive cleaning solutions, as defoamers, as foam stabilizers, wetting agents, paint and flow additives and as demulsifiers.

### Claim 18 (depends on 1)

The process according to claim 1, wherein acetic acid is added in amounts of from 1.0 to 1.5 percent by weight, based on the reaction matrix consisting of acetic anhydride and cyclic siloxanes.

### Claim 19 (depends on 5)

The trifluoromethanesulfonic acid-acidified, equilibrated α,ω-diacetoxypolydimethylsiloxanes according to claim 5, wherein they have an average chain length determined by 29Si-NMR spectroscopy of 10<X<20.

### Claim 20 (depends on 8)

The process according to claim 8, wherein a condensation catalyst is used for reacting the equilibrated α,ω-diacetoxypolydimethylsiloxane with polyether monools,
wherein condensation catalysts employed are acids selected from the group consisting of simple mineral acids and methanesulfonic acid, phosphoric acid, phosphonic acids and/or else acidic salt-like compounds such as triflate salts, bismuth triflate, and/or any Lewis-acidic compounds such as tin and organotin compounds, titanate esters, tetraalkoxy titanates, zinc acetylacetonate, zinc acetate, trispentafluorophenylborane and trichloroacetic acid,
wherein the condensation catalyst, in particular the trichloroacetic acid, is in the range from 0.2 to 0.5 percent by mass, based on the total amount of the reactants provided for the SiOC-bond forming reaction, namely α,ω-diacetoxypolydimethylsiloxane and polyether monool.