# US 2021/0171713 A1 · Mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171713 A1
- Document ID: US20210171713A1
- Status: Published application
- Kind: A1
- Application number: 17/105,050
- Filed: 2020-11-25
- Published: 2021-06-10
- Earliest claimed: 2019-12-05
- Assignees: Changsha University of Science and Technology
- Applicants: Changsha University of Science & Technology
- Inventors: BO LIANG; KAI SHI; JIANLONG ZHENG
- Web page: https://patentgrep.com/patent/US20210171713A1

## CPC

- C08G 73/026: {Wholly aromatic polyamines}
- C01B 33/40: Clays
- C08G 61/12: Macromolecular compounds containing atoms other than carbon in the main chain of the macromolecule
- C08K 3/346: {Clay}
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08G 2261/11: Homopolymers
- C08G 2261/3241: containing one or more nitrogen atoms as the only heteroatom, e.g. carbazole
- C08G 2261/43: Chemical oxidative coupling reactions, e.g. with FeCl3
- C08K 2201/011: Nanostructured additives
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial is disclosed. The method includes dispersing a montmorillonite material in an aqueous solution, stirring, concentrating and collecting a concentrated montmorillonite solution for use; adding dopamine hydrochloride to a buffer solution to prepare a dopamine hydrochloride solution, with a concentration of 0.2-1 g/mL, and adjusting the pH value of the dopamine hydrochloride solution; and adding the dopamine hydrochloride solution and the concentrated montmorillonite solution simultaneously into a ball mill jar to form a mixture, and then subjecting the mixture to a ball milling for 0.3-6 hours, pouring the mixture out of the ball mill jar, and subjecting to a solid-liquid separation by a centrifugation, and then washing a solid product with deionized water for 3-6 times, and removing water from the solid product, to obtain the polydopamine-modified montmorillonite nanomaterial.

## Claims

### Claim 1

A mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial, comprising:
dispersing a montmorillonite material in an aqueous solution, stirring, concentrating, and collecting a concentrated montmorillonite solution for use;
adding dopamine hydrochloride to a buffer solution to prepare a dopamine hydrochloride solution, with a concentration of 0.2-1 g/L, and adjusting a pH value of the dopamine hydrochloride solution; and
adding the dopamine hydrochloride solution and the concentrated montmorillonite solution simultaneously into a ball mill jar to form a mixture, then subjecting the mixture to a ball milling for 0.3-6 hours, pouring the mixture out of the ball mill jar, subjecting the mixture to a solid-liquid separation by a centrifugation, then washing a solid product with deionized water for 3-6 times, and removing water from the solid product, to obtain the polydopamine-modified montmorillonite nanomaterial.

### Claim 2 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, wherein dispersing the montmorillonite material in the aqueous solution, stirring, concentrating, and collecting the concentrated montmorillonite solution for use further comprises using a solid/liquid ratio of montmorillonite to deionized water is 1:50-100 g/mL.

### Claim 3 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, further comprising adding an oxidant to the dopamine hydrochloride solution, and the oxidant includes any one of hydrogen peroxide, copper sulfate, ammonium sulfate, and sodium periodate, and an amount of the oxidant is 6-20 wt %.

### Claim 4 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, further comprising adding a hydrogen peroxide and/or copper sulfate to the dopamine hydrochloride solution.

### Claim 5 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, wherein adding the dopamine hydrochloride solution and the concentrated montmorillonite solution simultaneously into the ball mill jar to form the mixture further comprises using a mass ratio of dopamine hydrochloride to montmorillonite of 1:1-1:2, and the pH value of the dopamine hydrochloride solution is 8-9.

### Claim 6 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, wherein then subjecting the mixture to a ball milling for 0.3-6 hours further comprises using zirconia beads which include zirconia beads having a diameter of 2 mm, 5 mm, 10 mm and 15 mm as grinding balls, with a mass ratio of grinding balls for each diameter of 4:8:20:5, a mass ratio of ball to material of 10-50:1, and with a rotation speed of 300-500 r/min.

### Claim 7 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, wherein subjecting the mixture to a ball milling for 0.3-6 hours further comprises removing water from the solid product by a lyophilization, and before the lyophilization a dilute solution with a solid substance concentration of 5-25 wt % is prepared with the substance to be lyophilized, and the lyophilization is carried out at a temperature of −40° C. to −50° C. for 24-72 hours.

### Claim 8 (depends on 1)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 1, wherein subjecting the mixture to a ball milling for 0.3-6 hours further comprises removing water from the solid product by a vacuum drying until that a constant weight of the product is achieved, and a resulting product is subjected to another ball milling, to obtain the polydopamine-modified montmorillonite nanomaterial.

### Claim 9 (depends on 8)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 8, wherein the vacuum drying is carried out at a temperature of 80-100° C. for 6-12 hours.

### Claim 10 (depends on 8)

The mechanical ball-milling method for preparing a polydopamine-modified montmorillonite nanomaterial of claim 8, wherein the another ball milling further comprises using zirconia beads which include zirconia beads having a diameter of 5 mm, 10 mm, 15 mm and 20 mm as grinding balls for 15-20 minutes, with a mass ratio of grinding balls for each diameter of 3:8:20:8, a ball-to-material weight ratio of 10-50:1, and a rotation speed of 300-500 r/min.