# US 2021/0171706 A1 · Polyester resin, preparation method thereof, and resin molded article formed therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171706 A1
- Document ID: US20210171706A1
- Status: Published application
- Kind: A1
- Application number: 16/065,368
- Filed: 2016-12-12
- Published: 2021-06-10
- Earliest claimed: 2015-12-24
- Assignees: SK Chemicals Co., Ltd.
- Applicants: SK Chemicals Co., Ltd.
- Inventors: Su-Min LEE; Yoo Jin LEE; Kyu-Chan HAN
- Web page: https://patentgrep.com/patent/US20210171706A1

## CPC

- C08G 63/183: Terephthalic acids
- C08G 63/672: Dicarboxylic acids and dihydroxy compounds
- C08G 63/16: Dicarboxylic acids and dihydroxy compounds
- C08G 63/18: the acids or hydroxy compounds containing carbocyclic rings
- C08G 63/181: Acids containing aromatic rings
- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G 63/80: Solid-state polycondensation
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided are a polyester resin having high heat resistance and degree of crystallinity, a preparation method thereof, and a resin molded article formed therefrom, the resin molded article having superior heat resistance and mechanical strength and maintaining high transparency.

## Claims

### Claim 1

A polyester resin having a structure, wherein acid moieties derived from a dicarboxylic acid or a derivative thereof and diol moieties derived from diol are repeated by polymerization of the dicarboxylic acid or the derivative thereof comprising a terephthalic acid or a derivative thereof and diol comprising isosorbide,
the polyester resin comprising 7 to 20 mol % of the diol moieties derived from isosorbide with respect to the total diol moieties derived from diol,
having an intrinsic viscosity of 0.85 dl/g or more, which is measured at 35° C. after dissolving the polyester resin in ortho chloro phenol at a concentration of 1.2 g/dl at 150° C. for 15 minutes, a glass transition temperature of 87° C. or higher, and enthalpy of fusion of 40 J/g or more, which is measured during 1st scan by differential scanning calorimetry (DSC).

### Claim 2 (depends on 1)

The polyester resin of claim 1, wherein the enthalpy of fusion is 50 J/g or more, which is measured during 1st scan by differential scanning calorimetry (DSC).

### Claim 3 (depends on 1)

The polyester resin of claim 1, wherein the dicarboxylic acid or the derivative thereof comprises 0 mol % to 50 mol % of one or more selected from the group consisting of C8 to C14 aromatic dicarboxylic acid or a derivative thereof and C4 to C12 aliphatic dicarboxylic acid or a derivative thereof as other dicarboxylic acid or derivative thereof than the terephthalic acid or the derivative thereof, with respect to the total dicarboxylic acid or derivative thereof.

### Claim 4 (depends on 1)

The polyester resin of claim 1, wherein an amount of the diol moieties derived from isosorbide is 7 mol % to 11 mol % with respect to the total diol moieties derived from diol.

### Claim 5 (depends on 1)

The polyester resin of claim 1, wherein an amount of the moieties derived from diethylene glycol is 6 mol % or less with respect to the total diol moieties derived from diol.

### Claim 6 (depends on 1)

The polyester resin of claim 1, wherein haze of a specimen having a thickness of 6 mm obtained from the polyester resin is less than 1%, as measured in accordance with ASTM D1003-97.

### Claim 7 (depends on 1)

The polyester resin of claim 1, wherein heat deflection temperature (HDT) is 75° C. or higher.

### Claim 8 (depends on 1)

The polyester resin of claim 1, wherein a number average molecular weight is 15,000 g/mol to 50,000 g/mol.

### Claim 9 (depends on 1)

The polyester resin of claim 1, wherein the polyester resin is used in bottles, hot fill jars, high-pressure containers, sheets, stretched films, or fibers.

### Claim 10 (depends on 1)

A method of preparing the polyester resin of claim 1, the method comprising:
(a) carrying out an esterification reaction or an ester exchange reaction of (i) a dicarboxylic acid or a derivative thereof comprising a terephthalic acid or a derivative thereof and (ii) diol comprising 7 mol % or more of isosorbide with respect to the total diol;
(b) carrying out a polycondensation reaction of a product resulting from the esterification reaction or ester exchange reaction until intrinsic viscosity as measured at 35° C. after dissolving the product in ortho chloro phenol at a concentration of 1.2 g/dl at 150° C. for 15 minutes reaches 0.40 dl/g to 0.60 dl/g;
(c) crystallizing a polymer prepared by the polycondensation reaction; and
(d) carrying out solid phase polymerization of the crystallized polymer until intrinsic viscosity as measured at 35° C. after dissolving the polymer in ortho chloro phenol at a concentration of 1.2 g/dl at 150° C. for 15 minutes reaches 0.85 dl/g or more.

### Claim 11 (depends on 10)

The method of preparing the polyester resin of claim 10, wherein part of the (ii) diol is injected during reaction.

### Claim 12 (depends on 10)

The method of preparing the polyester resin of claim 10, wherein a polycondensation catalyst, a stabilizer, an orthochromatic agent, a crystallizing agent, an antioxidant, or a branching agent is added to a slurry before the starting of the (a) esterification reaction or ester exchange reaction, or to a product after the completion of the reaction.

### Claim 13 (depends on 10)

The method of preparing the polyester resin of claim 10, wherein the crystallized polymer is subjected to solid phase polymerization for 30 hrs or longer in the (d) solid phase polymerization.

### Claim 14 (depends on 1)

A resin molded article formed from the polyester resin of claim 1.