# US 2021/0171560 A1 · D-allose crystal and production method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171560 A1
- Document ID: US20210171560A1
- Status: Published application
- Kind: A1
- Application number: 17/116,039
- Filed: 2020-12-09
- Published: 2021-06-10
- Earliest claimed: 2019-12-10
- Assignees: Matsutani Chemical Industry Co., Ltd.
- Applicants: Matsutani Chemical Industry Co., Ltd.
- Inventors: Ryosuke NAKAGAWA
- Web page: https://patentgrep.com/patent/US20210171560A1

## CPC

- C07H 3/02: Monosaccharides
- C30B 7/08: by cooling of the solution
- A61K 31/7004: Monosaccharides having only carbon, hydrogen and oxygen atoms
- C07H 1/06: Separation; Purification
- C30B 29/58: Macromolecular compounds
- C07B 2200/13: Crystalline forms, e.g. polymorphs
- C07H: SUGARS; DERIVATIVES THEREOF; NUCLEOSIDES; NUCLEOTIDES; NUCLEIC ACIDS (derivatives of aldonic or saccharic acids C07C, C07D; aldonic acids, saccharic acids C07C59/105, C07C59/285; cyanohydrins C07C255/16; glycals C07D; compounds of unknown constitution C07G; polysaccharides, derivatives thereof C08B; DNA or RNA concerning genetic engineering, vectors, e.g. plasmids, or their isolation, preparation or purification C12N15/00; sugar industry C13)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- C07B: GENERAL METHODS OF ORGANIC CHEMISTRY; APPARATUS THEREFOR (preparation of carboxylic acid esters by telomerisation C07C67/47; telomerisation C08F)

## Abstract

High-purity hydrous D-allose crystals and a method of efficiently obtaining the crystals are provided. To a D-allose-containing solution having a purity of D-allose of at least 80% (g/g) in a solute, in a metastable region in a supersaturated state of 30° C. or less, D-allose seed crystals are added. Then, the temperature of the solution is lowered by 10° C. or more for cooling and crystallization to initially obtain “hydrous D-allose crystals”, and the crystallization water thereof is removed in a specified temperature zone to obtain novel “anhydrous D-allose crystals”.

## Claims

### Claim 1

A method for producing a hydrous D-allose crystal by adding a D-allose seed crystal to a D-allose-containing solution, comprising steps of providing a D-allose-containing solution having a purity of D-allose of at least 80% (g/g) in a solute,
adjusting the D-allose-containing solution to that in a metastable region in the supersaturated solution at 30° C. or less,
adding a D-allose seed crystal to said D-allose-containing solution and then cooling the D-allose-containing solution by lowering the temperature of the solution at least by 10° C. or more for crystallization of the hydrous D-allose crystal.

### Claim 2 (depends on 1)

The method for producing a hydrous D-allose crystal according to claim 1, wherein the metastable region of the D-allose-containing solution to which the D-allose seed crystal is added has a degree of supersaturation of 1.02 to 1.30.

### Claim 3 (depends on 1)

The method for producing a hydrous D-allose crystal according to claim 1, wherein the metastable region of the D-allose-containing solution to which the D-allose seed crystal is added has a relationship between Brix of the D-allose-containing solution and temperature (° C.) satisfying: 1.03×Temperature+23.10≤Brix≤0.94×Temperature+34.90.

### Claim 4 (depends on 1)

The method for producing a hydrous D-allose crystal according to claim 1, wherein the amount of the added D-allose seed crystal is in an amount of 1.0 to 3.0 mass % based on D-allose in the D-allose-containing solution.

### Claim 5 (depends on 4)

The method for producing a hydrous D-allose crystal according to claim 4, wherein yield of the hydrous D-allose crystal from the D-allose-containing solution is of 53% or more.

### Claim 6 (depends on 1)

A method for producing an anhydrous D-allose crystal, comprising steps of
preparing the hydrous D-allose crystal by the production method according to claim 1, and
drying the hydrous D-allose crystal at 30 to 65° C.

### Claim 7 (depends on 6)

The method for producing an anhydrous D-allose crystal according to claim 6, wherein the anhydrous D-allose crystal satisfies the following (A) and (B):
(A) a purity of 99% or more
(B) a repose angle of less than 46 degrees.

### Claim 8 (depends on 7)

The method for producing an anhydrous D-allose crystal according to claim 7, wherein the anhydrous D-allose crystal further satisfies the following (C):
(C) an aspect ratio of a particle of 1.0 to 10.

### Claim 9 (depends on 7)

The method for producing an anhydrous D-allose crystal according to claim 7, wherein the anhydrous D-allose crystal further satisfies the following (D):
(D) an average particle size of 200 to 800 μm.

### Claim 10 (depends on 2)

A method for producing an anhydrous D-allose crystal, comprising steps of
preparing the hydrous D-allose crystal by the production method according to claim 2, and
drying the hydrous D-allose crystal at 30 to 65° C.

### Claim 11

An anhydrous D-allose crystal satisfying the following (A) and (B):
(A) a purity of 99% or more (
B) a repose angle of less than 46 degrees.

### Claim 12 (depends on 11)

The anhydrous D-allose crystal according to claim 11, further satisfying the following (C):
(C) an aspect ratio of a particle of 1.0 to 10.

### Claim 13 (depends on 11)

The anhydrous D-allose crystal according to claim 11, further satisfying the following (D):
(D) an average particle size of 200 to 800 μm.