# US 2021/0171391 A1 · Window manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171391 A1
- Document ID: US20210171391A1
- Status: Published application
- Kind: A1
- Application number: 16/940,819
- Filed: 2020-07-28
- Published: 2021-06-10
- Earliest claimed: 2019-12-10
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: Yuri KIM; WOOSUK SEO; MINKI KIM; Byeong-Beom KIM; Hoikwan LEE
- Web page: https://patentgrep.com/patent/US20210171391A1

## CPC

- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 23/0075: {Cleaning of glass (specially adapted to plate glass B08B11/00)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for manufacturing the window includes providing an initial window having a first compressive stress value and cleaning the initial window to provide a window having a second compressive stress value. The cleaning of the initial window includes acid cleaning the initial window by using acid, and alkali cleaning the initial window by using alkali after the acid cleaning. A linear relational expression is modeled between a difference between the first and second compressive stress values and a temperature and a holding time in the acid cleaning.

## Claims

### Claim 1

A method for manufacturing a window, the method comprising:
providing an initial window having a first compressive stress value; and
cleaning the initial window to provide a window having a second compressive stress value,
wherein the cleaning of the initial window comprises:
acid cleaning the initial window by using acid; and
alkali cleaning the initial window by using alkali after the acid cleaning,
wherein a difference between the first compressive stress value and the second compressive stress value satisfies following Equations 1 and 2:
ΔCS(MPa)=δ·t(min)+θ, [Equation 1]
ΔCS(MPa)=α·T(° C.)+β, [Equation 2]
wherein, in Equation 1, a following relational expression is satisfied: 0<γ≤10, and −300≤θ<0,
in Equation 2, a following relational expression is satisfied: 0<α≤10, and 0<β≤50,
in Equations 1 and 2, ΔCS is an absolute value of the difference between the first compressive stress value and the second compressive stress value, T is a temperature in the acid cleaning, and t is a holding time of the acid cleaning, and
in Equations 1 and 2, words in parentheses represent following units of corresponding parameters: a unit of ΔCS is megapascals (MPa), and a unit of T is degrees Celsius (° C.), and a unit of t is minutes (min).

### Claim 2 (depends on 1)

The method of claim 1, wherein the temperature T in the acid cleaning of the Equation 2 ranges of about 40° C. to about 70° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the holding time t in the acid cleaning of the Equation 1 ranges of about 1 minute to about 20 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the difference between the first compressive stress value and the second compressive stress value satisfies following Equation 3:
ΔCS(MPa)=ν·T(° C.)+ω·t(min)+γ, [Equation 3]
wherein, in Equation 3, a following relational expression is satisfied: 0<ν≤10, 0<ω≤20, and −150≤γ≤−50.

### Claim 5 (depends on 4)

The method of claim 4, wherein the difference between the first compressive stress value and the second compressive stress value satisfies following Equation 3-1:
ΔCS(MPa)=4T(° C.)+2t(min)+γ. [Equation 3-1]

### Claim 6 (depends on 1)

The method of claim 1, wherein the difference between the first compressive stress value and the second compressive stress value is proportional to a cleaning amount in the acid cleaning, and
the cleaning amount is a removal amount per a unit area of the initial window, which is removed from a surface of the initial window.

### Claim 7 (depends on 6)

The method of claim 6, wherein the cleaning amount satisfies following Equations 4 and 5:
LAB(mg/cm2)=δ′·t(min)+θ′ , [Equation 4]
LAB(mg/cm2)=α′·T(° C.)+β′, [Equation 5]
wherein, in Equation 4, a following relational expression is satisfied: 0<δ′≤5, and −300≤θ′<0,
in Equation 5, a following relational expression is satisfied: 0<α′≤0.05, and 0<β′≤0.5, and
in Equations 4 and 5, LAB is a cleaning amount, and mg/cm2in parentheses represent a unit of LAB: milligrams per square centimeter.

### Claim 8 (depends on 7)

The method of claim 7, wherein the cleaning amount satisfies following Equation 6:
LAB(mg/cm2)=ν·T(° C.)+ω·t(min)+γ′, [Equation 6]
wherein, in Equation 6, a following relational expression is satisfied: 0<ν′≤0.05, 0<ω′≤0.1, and −50≤γ′<0.

### Claim 9 (depends on 8)

The method of claim 8, wherein the cleaning amount satisfies following Equation 6-1:
LAB (mg/cm2)=0.01T(° C.)+0.02t(min)+γ′. [Equation 6-1]

### Claim 10 (depends on 6)

The method of claim 6, wherein the cleaning amount is a sum of a first cleaning amount in the acid cleaning and a second cleaning amount in the alkali cleaning,
the first cleaning amount ranges of about 30 percent by weight (wt %) to about 40 wt % based on a total weight of the cleaning amount, and
the second cleaning amount ranges of about 60 wt % to about 70 wt % based on the total weight of the cleaning amount.

### Claim 11 (depends on 1)

The method of claim 1, wherein the providing of the initial window comprises:
providing a base glass; and
toughening the provided base glass,
wherein the base glass comprises lithium alumino-silicate (LAS)-based glass or sodium alumino-silicate (NAS)-based glass.

### Claim 12 (depends on 11)

The method of claim 11, wherein the toughening of the base glass comprises chemically toughening of the base glass by using toughening molten salt containing at least one of KNO3 KNO3 or NaNO3 NaNO3.

### Claim 13 (depends on 12)

The method of claim 12, wherein the toughening of the base glass is performed at a temperature of about 350° C. to about 450° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the acid cleaning comprises providing an acid cleaning solution containing at least one of a nitric acid (HNO3), a sulfuric acid (H2SO4), or a hydrochloric acid (HCl).

### Claim 15 (depends on 1)

The method of claim 1, wherein the alkali cleaning comprises providing an alkali cleaning solution containing at least one of sodium hydroxide (NaOH) or potassium hydroxide (KOH).

### Claim 16

A method for manufacturing a window, the method comprising:
providing an initial window chemically toughened;
acid cleaning the initial window by using an acid cleaning solution to provide an intermediate window; and
alkali cleaning the intermediate window by using an alkali cleaning solution to provide a final window, wherein a first compressive stress value of the initial window and a second compressive stress value of the final window satisfy following Equations 1 and 2:
ΔCS(MPa)=δ·t(min)+θ, [Equation 1]
ΔCS(MPa)=α·T(° C.)+β, [Equation 2]
wherein, in Equations 1 and 2, ΔCS is an absolute value of a difference between the first compressive stress value and the second compressive stress value, and words in parentheses represent following units of corresponding parameters: a unit of ΔCS is megapascals (MPa), and a unit of T is degrees Celsius (° C.), and a unit of t is minutes (min),
in Equation 1, a following relational expression is satisfied: 0<δ≤10, −300≤θ<0, and 1 minute≤t≤20 minutes, and
in Equation 2, a following relational expression is satisfied: 0<α≤10, 0<β≤50, and 40° C.≤T≤70° C.

### Claim 17 (depends on 16)

The method of claim 16, wherein the intermediate window comprises a void defined by eluting an alkali metal from the initial window.

### Claim 18 (depends on 17)

The method of claim 17, wherein the intermediate window comprises:
a base layer in which a ratio of silicon content to the alkali metal is substantially the same as a ratio of the silicon content to the alkali metal in the initial window; and
an intermediate layer which is formed on a surface of the base layer and of which a ratio of the silicon content to the alkali metal ions is greater than the ratio of the silicon content to the alkali metal ions in the base layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein a ratio of the void in the intermediate layer is greater than a ratio of the void in the base layer.

### Claim 20 (depends on 18)

The method of claim 18, wherein the initial window has a thickness of about 500 micrometers (μm) to about 800 μm, and the intermediate layer has a thickness of about 0.2 μm to about 0.5 μm.

### Claim 21 (depends on 18)

The method of claim 18, wherein the final window is formed by removing the intermediate layer from the intermediate window.

### Claim 22 (depends on 16)

The method of claim 16, wherein an absolute value of a difference between the first compressive stress value and the second compressive stress value is proportional to a cleaning amount, and the cleaning amount is a difference in weight between the initial window and the final window.

### Claim 23 (depends on 22)

The method of claim 22, wherein the cleaning amount satisfies following Equations 4 and 5:
LAB(mg/cm2)=δ′·t(min)+θ′ , [Equation 4]
LAB(mg/cm2)=α′·T(° C.)+β′, [Equation 5]
wherein, in Equation 4, a following relational expression is satisfied: 0<δ′≤5, and −300≤θ′<0,
in Equation 5, a following relational expression is satisfied: 0<α′≤0.05, and 0<β′≤0.5, and
in Equations 4 and 5, LAB is the cleaning amount, and mg/cm2 in parentheses represent a unit of LAB: milligrams per square centimeter.

### Claim 24 (depends on 16)

The method of claim 16, wherein the difference between the first compressive stress value and the second compressive stress value satisfies following Equation 3-1:
ΔCS(MPa)=4T(° C.)+2t(min)+γ. [Equation 3-1]