# US 2021/0171372 A1 · Sulfur-doped micro zero-valent metal reducing agent and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0171372 A1
- Document ID: US20210171372A1
- Status: Published application
- Kind: A1
- Application number: 17/069,194
- Filed: 2020-10-13
- Published: 2021-06-10
- Earliest claimed: 2019-12-10
- Assignees: Korea University Research and Business Foundation
- Applicants: Korea University Research and Business Foundation
- Inventors: Jeehyeong KHIM; Mingcan CUI; Jongbok CHOI; Yonghyun LEE
- Web page: https://patentgrep.com/patent/US20210171372A1

## CPC

- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- C02F 1/705: {Reduction by metals}
- B22F 2009/043: {by ball milling}
- B22F 2301/30: Low melting point metals, i.e. Zn, Pb, Sn, Cd, In, Ga
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C02F 2101/36: containing halogen
- C02F 2103/06: Contaminated groundwater or leachate
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

Disclosed is a sulfur-doped micro zero-valent metal reducing agent containing a zero-valent metal, wherein a metal sulfide layer synthesized using a ball milling process may be formed on a surface of the zero-valent metal. In addition, disclosed is a method for preparing a sulfur-doped micro zero-valent metal reducing agent including, in a ball milling process using a ball milling apparatus composed of a jar, balls, and a body, a first step of preparing an inorganic mixture by mixing a zero-valent metal and sulfur with each other, and a second step of forming a metal sulfide layer synthesized on a surface of the zero-valent metal by putting the inorganic mixture into the jar together with the balls and performing ball milling.

## Claims

### Claim 1

A sulfur-doped micro zero-valent metal reducing agent containing a zero-valent metal, wherein a metal sulfide layer synthesized using a ball milling process is formed on a surface of the zero-valent metal.

### Claim 2 (depends on 1)

The sulfur-doped micro zero-valent metal reducing agent of claim 1, wherein the zero-valent metal includes zero-valent zinc,
wherein the metal sulfide layer includes zinc sulfide.

### Claim 3 (depends on 2)

The sulfur-doped micro zero-valent metal reducing agent of claim 2, wherein the metal sulfide layer is synthesized by a mechanochemical bonding reaction, wherein the zero-valent metal in a solid phase and sulfur in the solid phase react to form a new solid phase in the mechanochemical bonding reaction.

### Claim 4

A method for preparing a sulfur-doped micro zero-valent metal reducing agent, the method comprising:
in a ball milling process using a ball milling apparatus composed of a jar, balls, and a body,
a first step of preparing an inorganic mixture by mixing a zero-valent metal and sulfur with each other; and
a second step of forming a metal sulfide layer synthesized on a surface of the zero-valent metal by putting the inorganic mixture into the jar together with the balls and performing the ball milling.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first step includes:
mixing the micro zero-valent metal with the sulfur in a weight ratio of 1:0.2 to 1.

### Claim 6 (depends on 5)

The method of claim 5, wherein the second step includes:
performing the ball milling process for 2 to 4 hours at a rotation speed of 300 to 500 rpm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the second step includes:
mixing the balls with the inorganic mixture in a weight ratio of 1:5 to 15 in the ball milling process.