# US 2021/0162708 A1 · Anti-fog mirror apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0162708 A1
- Document ID: US20210162708A1
- Status: Published application
- Kind: A1
- Application number: 17/171,791
- Filed: 2021-02-09
- Published: 2021-06-03
- Earliest claimed: 2014-10-31
- Assignees: MCS Industries, Inc.
- Applicants: MCS Industries, Inc.
- Inventors: Dallas Aaron KOHLER
- Web page: https://patentgrep.com/patent/US20210162708A1

## CPC

- B32B 7/10: at least one layer having inter-reactive properties
- B32B 7/00: Layered products characterised by the relation between layers; Layered products characterised by the relative orientation of features between layers, or by the relative values of a measurable parameter between layers, i.e. products comprising layers having different physical, chemical or physicochemical properties; Layered products characterised by the interconnection of layers
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/00: Layered products essentially comprising sheet glass, or glass, slag, or like fibres
- B32B 27/00: Layered products comprising {a layer of} synthetic resin {(fibrous or filamentary layer made of a synthetic resin B32B5/02; particulate layer made of a synthetic resin B32B5/16; foamed layer made of a synthetic resin B32B5/18)}
- B32B 27/06: as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a layer of a particular substance B32B9/045; next to a bituminous or tarry layer B32B11/046; next to a water setting substance layer B32B13/12; next to a metal layer B32B15/08; next to a glass layer B32B17/10; next to a layer formed of natural mineral fibres or particles B32B19/045; next to a wood layer B32B21/08; next to a cellulosic plastic layer B32B23/08; next to a natural or synthetic rubber layer B32B25/08)}
- B32B 27/08: of synthetic resin
- B32B 27/18: characterised by the use of special additives
- B32B 27/302: {comprising aromatic vinyl (co)polymers, e.g. styrenic (co)polymers}
- B32B 27/304: {comprising vinyl halide (co)polymers, e.g. PVC, PVDC, PVF, PVDF}
- B32B 27/308: {comprising acrylic (co)polymers}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/322: {comprising halogenated polyolefins, e.g. PTFE}
- B32B 27/34: comprising polyamides
- B32B 27/36: comprising polyesters
- B32B 27/40: comprising polyurethanes
- B32B 38/162: {Cleaning}
- B32B 37/02: characterised by a sequence of laminating steps, e.g. by adding new layers at consecutive laminating stations
- B32B 38/10: Removing layers, or parts of layers, mechanically or chemically
- B32B 38/1875: {Tensioning}
- B32B 2250/03: 3 layers
- B32B 2250/04: 4 layers
- B32B 2250/24: All layers being polymeric
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2307/40: having particular optical properties
- B32B 2307/412: Transparent
- B32B 2307/416: Reflective
- B32B 2307/584: Scratch resistance
- B32B 2307/71: Resistive to light or to UV
- B32B 2307/7145: Rot proof, resistant to bacteria, mildew, mould, fungi
- B32B 2307/728: Hydrophilic
- B32B 2307/73: Hydrophobic
- B32B 2307/732: Dimensional properties
- B32B 2309/02: Temperature
- B32B 2309/65: Dust free, e.g. clean room
- B32B 2551/08: Mirrors
- B32B 2571/00: Protective equipment
- Y10T 428/2495: Thickness [relative or absolute]
- Y10T 428/24967: Absolute thicknesses specified
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Described herein is a mirror apparatus comprising: a reflective substrate; and an anti-fog complex comprising: an adhesive layer atop the substrate; a first polymeric layer atop the pressure sensitive adhesive layer; and a second polymeric layer atop the first polymeric layer. Methods of making the mirror apparatus are also disclosed.

## Claims

### Claim 1

A mirror apparatus having a first major surface opposite a second major surface, the mirror apparatus comprising:
a reflective substrate having an upper surface opposite a lower surface, the reflective substrate comprising:
a transparent base layer having an upper surface opposite a lower surface, the transparent base layer formed of glass;
a back coating applied to the lower surface of the transparent base layer, the back coating formed of a reflective material; and
the upper surface of the reflective substrate comprising the upper surface of the transparent base layer;
an anti-fog complex having an upper surface opposite a lower surface, the anti-fog complex comprising:
a first polymeric layer having an upper surface opposite a lower surface, the first polymeric layer comprising polymethyl methacrylate;
an adhesive layer having an upper surface opposite a lower surface, the adhesive layer formed of a pressure sensitive adhesive composition; and
the lower surface of the anti-fog complex comprising the lower surface of the adhesive layer;
wherein the reflective substrate has a thickness as measured between the upper surface and the lower surface of the reflective substrate, the thickness of the reflective substrate ranging from about 2.5 mm to about 3.5 mm;
wherein the first polymeric layer has a thickness as measured between the upper surface and the lower surface of the first polymeric layer;
wherein the adhesive layer has a thickness as measured between the upper surface and the lower surface of the adhesive layer, the thickness of the adhesive layer ranging from about 20 microns to about 30 microns; and
wherein a ratio of the thickness of the adhesive layer to the thickness of the first polymeric layer ranges from about 0.2:1 to about 1.25:1;
wherein the upper surface of the reflective substrate is adhesively bonded to the lower surface of the anti-fog complex by the adhesive layer; and
wherein the first major surface of the mirror apparatus comprises the upper surface of the anti-fog complex.

### Claim 2 (depends on 1)

The mirror apparatus according to claim 1, wherein the ratio of the thickness of the adhesive layer to the thickness of the first polymeric layer is about 0.2.

### Claim 3 (depends on 1)

The mirror apparatus according to claim 1, wherein the thickness of the adhesive layer ranges from about 20 microns to about 25 microns.

### Claim 4 (depends on 1)

The mirror apparatus according to claim 1, wherein the thickness of the reflective substrate ranges from about 2.75 mm to about 3.25 mm.

### Claim 5 (depends on 1)

The mirror apparatus according to claim 1, wherein the upper surface of the reflective substrate contacts the lower surface of the adhesive layer.

### Claim 6 (depends on 1)

The mirror apparatus according to claim 1, wherein the upper surface of the adhesive layer contacts the lower surface of the polymeric layer.

### Claim 7 (depends on 1)

The mirror apparatus according to claim 1, wherein the first polymeric layer is thermoplastic.

### Claim 8 (depends on 1)

The mirror apparatus according to claim 1, wherein the anti-fog complex does not contain any intervening layers between the first polymeric layer and the adhesive layer.

### Claim 9 (depends on 1)

The mirror apparatus according to claim 1, wherein the anti-fog complex comprises sulfur-containing compounds.

### Claim 10 (depends on 1)

The mirror apparatus according to claim 1, wherein the anti-fog complex comprises nitrogen-containing compounds.

### Claim 11 (depends on 1)

The mirror apparatus according to claim 1, wherein the mirror exhibits a scratch/dig ratio between 120/80 and 10/5.

### Claim 12 (depends on 1)

The mirror apparatus according to claim 1, wherein the mirror exhibits a yellow index rating greater than or equal to 4.

### Claim 13 (depends on 1)

The mirror apparatus according to claim 1, wherein the mirror exhibits a visible light reflectance greater than 75%.

### Claim 14 (depends on 1)

The mirror apparatus according to claim 1, wherein the second major surface of the mirror apparatus comprises the back coating.

### Claim 15

A mirror apparatus having a first major surface opposite a second major surface, the mirror apparatus comprising:
a reflective substrate having an upper surface opposite a lower surface, the reflective substrate comprising:
a transparent base layer having an upper surface opposite a lower surface, the transparent base layer formed of glass;
a back coating applied to the lower surface of the transparent base layer, the back coating formed of a reflective material; and
the upper surface of the reflective substrate comprising the upper surface of the transparent base layer;
an anti-fog matrix having an upper surface opposite a lower surface, the anti-fog matrix comprising:
an adhesive component;
a first polymeric component comprising polymethyl methacrylate;
a second polymeric component; and
wherein the reflective substrate has a thickness as measured between the upper surface and the lower surface of the reflective substrate, the thickness of the reflective substrate ranging from about 2.5 mm to about 3.5 mm;
wherein the upper surface of the reflective substrate is adhesively bonded to the lower surface of the anti-fog complex by the adhesive component; and
wherein the first major surface of the mirror apparatus comprises the upper surface of the anti-fog complex; and
wherein at least two of the adhesive component, the first polymeric component, and the second polymeric component are present on the upper surface of the anti-fog matrix.

### Claim 16 (depends on 15)

The mirror apparatus of claim 15, wherein the adhesive component is a pressure sensitive adhesive or a thermally activated adhesive.

### Claim 17 (depends on 15)

The mirror apparatus of claim 15, wherein the second polymeric layer component comprises a polyurethane.

### Claim 17 (depends on 15)

The mirror apparatus according to claim 15, wherein the first polymeric component is thermoplastic.

### Claim 18 (depends on 15)

The mirror apparatus according to claim 15, wherein the thickness of the reflective substrate ranges from about 2.75 mm to about 3.25 mm.

### Claim 18 (depends on 15)

The mirror apparatus according to claim 15, wherein the anti-fog complex comprises sulfur-containing compounds.

### Claim 19 (depends on 15)

The mirror apparatus according to claim 15, wherein the anti-fog complex comprises nitrogen-containing compounds.

### Claim 20

A mirror apparatus having a first major surface opposite a second major surface, the mirror apparatus comprising:
a reflective substrate having an upper surface opposite a lower surface, the reflective substrate comprising:
a transparent base layer having an upper surface opposite a lower surface, the transparent base layer formed of glass;
a back coating applied to the lower surface of the transparent base layer, the back coating formed of a reflective material; and
the upper surface of the reflective substrate comprising the upper surface of the transparent base layer;
an anti-fog complex having an upper surface opposite a lower surface, the anti-fog complex comprising:
a first polymeric layer having an upper surface opposite a lower surface, the first polymeric layer comprising polymethyl methacrylate;
an adhesive layer having an upper surface opposite a lower surface; and
the lower surface of the anti-fog complex comprising the lower surface of the adhesive layer, and the anti-fog complex further comprising polyurethane;
wherein the reflective substrate has a thickness as measured between the upper surface and the lower surface of the reflective substrate, the thickness of the reflective substrate ranging from about 2.75 mm to about 3.25 mm;
wherein the first polymeric layer has a thickness as measured between the upper surface and the lower surface of the first polymeric layer;
wherein the adhesive layer has a thickness as measured between the upper surface and the lower surface of the adhesive layer, the thickness of the adhesive layer ranging from about 20 microns to about 25 microns; and
wherein a ratio of the thickness of the adhesive layer to the thickness of the first polymeric layer is about 0.2:1;
wherein the upper surface of the reflective substrate is adhesively bonded to the lower surface of the anti-fog complex by the adhesive layer; and
wherein the first major surface of the mirror apparatus comprises the upper surface of the anti-fog complex.