# US 2021/0155535 A1 · Coated glass article, method of making the same, and photovoltaic cell made therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0155535 A1
- Document ID: US20210155535A1
- Status: Published application
- Kind: A1
- Application number: 16/640,156
- Filed: 2018-08-31
- Published: 2021-05-27
- Earliest claimed: 2017-08-31
- Assignees: Pilkington Group Limited
- Applicants: Pilkington Group Limited
- Inventors: LILA RAJ DAHAL; DOUGLAS MARTIN NELSON; JUN NI; DAVID ALAN STRICKLER; SRIKANTH VARANASI
- Web page: https://patentgrep.com/patent/US20210155535A1

## CPC

- C03C 17/3417: {all coatings being oxide coatings}
- C03C 17/3452: {comprising a fluoride}
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 17/3488: {comprising a boride or phosphide}
- C03C 2217/211: SnO2
- C03C 2217/213: SiO2
- C03C 2217/24: Doped oxides
- C03C 2217/94: Transparent conductive oxide layers [TCO] being part of a multilayer coating
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A coated glass article includes a glass substrate. A coating is formed on the glass substrate. The coating includes a first coating layer. The first coating layer includes fluorine doped tin oxide. A second coating layer is provided between the glass substrate and the first coating layer. The second coating layer includes silicon dioxide and at least one of phosphorus and boron. The coated glass article exhibits a haze of 2.0% or less.

## Claims

### Claim at position 1

-30. (canceled)

### Claim 31

A coated glass article comprising:
a glass substrate; and
a coating formed on the glass substrate, wherein the coating comprises:
i. a first coating layer comprising fluorine doped tin oxide,
ii. a second coating layer provided between the glass substrate and the first coating layer, the second coating layer comprising silicon dioxide and at least one of phosphorus and boron,
wherein the coated glass article exhibits a haze of 2.0% or less.

### Claim 32 (depends on 31)

The coated glass article of claim 31, wherein the glass substrate is a soda-lime-silica glass and/or wherein the glass substrate comprises 0.15 weight % Fe2O3 (total iron) or less.

### Claim 33 (depends on 31)

The coated glass article of claim 31, wherein the coating is pyrolytic.

### Claim 34 (depends on 31)

The coated glass article of claim 31, wherein the first coating layer is deposited at a thickness of 150-1,000 nm.

### Claim 35 (depends on 31)

The coated glass article of claim 31, wherein the second coating layer (22) has a refractive index that is less than 1.8 and/or wherein the refractive index of the second coating layer is between 1.2 and 1.6.

### Claim 36 (depends on 31)

The coated glass article of claim 31, wherein the second coating layer comprises phosphorus and/or wherein the second coating layer comprises boron and/or wherein the second coating layer comprises phosphorus and boron.

### Claim 37 (depends on 31)

The coated glass article of claim 31, further comprising a third coating layer deposited directly on a major surface of the glass substrate, wherein the second coating layer is deposited directly on the third coating layer such that there are no intervening layers between the second coating layer and the third coating layer.

### Claim 38 (depends on 31)

The coated glass article of claim 31, further comprising an additional coating layer deposited directly on the first coating layer, wherein the additional coating layer is deposited directly on the first coating layer such that there are no intervening layers between the first coating layer and the additional coating layer.

### Claim 39 (depends on 31)

The coated glass article of claim 31, wherein the haze exhibited by the coated glass article is 0.5-2.0%.

### Claim 40 (depends on 31)

The coated glass article of claim 31, wherein the haze exhibited by the coated glass article is 1.6% or less and/or wherein the haze exhibited by the coated glass article is 0.5-1.6%.

### Claim 41 (depends on 31)

The coated glass article of claim 31, wherein the fluorine doped tin oxide comprises tin oxide that is less than fully doped with fluorine and/or wherein the fluorine doped tin oxide comprises tin oxide that is fully doped with fluorine.

### Claim 42 (depends on 34)

The coated glass article of claim 34, wherein the thickness of the first coating layer is 200-850 nm and/or wherein the thickness of the first coating layer is 250-500 nm.

### Claim 43 (depends on 37)

The coated glass article of claim 37, wherein the third coating layer comprises undoped tin oxide.

### Claim 44 (depends on 38)

The coated glass article of claim 38, wherein the additional coating layer is a fourth coating layer that forms an outer surface of the coated glass article.

### Claim 45 (depends on 38)

The coated glass article of claim 38, wherein the additional coating layer comprises undoped tin oxide.

### Claim 46 (depends on 31)

The coated glass article of claim 31, wherein the sheet resistance exhibited by the coating is 5-50 ohm/sq.

### Claim 47

A method of making a coated glass article, comprising:
providing a glass substrate; and
forming a coating on the glass substrate by depositing a first coating layer, wherein the first coating layer comprises fluorine doped tin oxide, and providing a second coating layer between the glass substrate and the first coating layer, wherein the second coating layer comprises silicon dioxide and at least one of phosphorus and boron,
wherein the coated glass article exhibits a haze of 2.0% or less.

### Claim 48 (depends on 47)

The method of claim 47, further comprising forming a gaseous mixture comprised of a silane compound, a first oxygen-containing molecule, a radical scavenger, and at least one of a phosphorus-containing compound and a boron-containing compound, directing the gaseous mixture toward and along the glass substrate, and reacting the gaseous mixture over the glass substrate to form the second coating layer on the glass substrate and/or further comprising depositing the first coating layer directly on the second coating layer such that there are no intervening layers between the first coating layer and the second coating layer.

### Claim 49 (depends on 47)

The method of claim 47, further comprising depositing a third coating layer that comprises undoped tin oxide directly on a major surface of the glass substrate, wherein the second coating layer is deposited directly on the third coating layer such that there are no intervening layers between the second coating layer and the third coating layer and/or further comprising depositing a fourth coating layer that comprises undoped tin oxide directly on the first coating layer, wherein the fourth coating layer is deposited directly on the first coating layer such that there are no intervening layers between the first coating layer and the fourth coating layer.

### Claim 50 (depends on 31)

A photovoltaic cell comprising the coated glass article of claim 31.