# US 2021/0154646 A1 · Mesoporous composite catalysts containing bismuth silicate and transition metal oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0154646 A1
- Document ID: US20210154646A1
- Status: Published application
- Kind: A1
- Application number: 16/692,255
- Filed: 2019-11-22
- Published: 2021-05-27
- Earliest claimed: 2019-11-22
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Gazali TANIMU; Abdullah M. AITANI; Sachio ASAOKA
- Web page: https://patentgrep.com/patent/US20210154646A1

## CPC

- B01J 23/8437: {Bismuth}
- B01J 21/08: Silica
- B01J 37/0201: {Impregnation}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 5/48: with oxygen as an acceptor
- B01J 23/745: Iron
- B01J 23/75: Cobalt
- B01J 23/755: Nickel
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 2231/76: Dehydrogenation
- B01J 2523/54: Bismuth
- B01J 2523/842: Iron
- B01J 2523/845: Cobalt
- B01J 2523/847: Nickel
- C07C 2521/08: Silica
- C07C 2523/18: Arsenic, antimony or bismuth
- C07C 2523/20: Vanadium, niobium or tantalum
- C07C 2523/755: Nickel
- C07C 2523/843: Arsenic, antimony or bismuth
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Composite catalysts having bismuth silicate(s) (e.g. Bi2SiO5) and transition metal oxide(s) (e.g. nickel oxide) impregnated on mesoporous silica supports such as SBA-15, mesoporous silica foam, and silica sol. Methods of making and characterizing the composite catalysts as well as processes for oxidatively dehydrogenating alkanes (e.g. n-butane) and/or alkenes (e.g. 1-butene, 2-butene) to corresponding dienes (e.g. butadiene) employing the composite catalysts are also described.

## Claims

### Claim 1

A composite catalyst, comprising:
a mesoporous silica support which is at least one selected from the group consisting of SBA-15, mesoporous silica foam, and silica sol; and
a catalytic material comprising a bismuth silicate and a transition metal oxide impregnated on the mesoporous silica support,
wherein the composite catalyst is devoid of molybdenum.

### Claim 2 (depends on 1)

The composite catalyst of claim 1, wherein the bismuth silicate is Bi2SiO5.

### Claim 3 (depends on 1)

The composite catalyst of claim 1, wherein the transition metal oxide is at least one selected from the group consisting of nickel(II) oxide, iron(II) oxide, and cobalt(II) oxide.

### Claim 4 (depends on 1)

The composite catalyst of claim 1, wherein the transition metal oxide is nickel(II) oxide.

### Claim 5 (depends on 1)

The composite catalyst of claim 1, which comprises 5-40 wt % of bismuth atoms and 10-30 wt % of transition metal atoms, each relative to a weight of the mesoporous silica support.

### Claim 6 (depends on 1)

The composite catalyst of claim 1, wherein the catalytic material further comprises bismuth oxide.

### Claim 7 (depends on 1)

A method of preparing the composite catalyst of claim 1, the method comprising:
mixing a transition metal salt and a bismuth salt in a solvent to form a first mixture;
mixing the first mixture and the mesoporous silica support to form a second mixture;
drying the second mixture to form a dried mass; and
calcining the dried mass in air thereby producing the composite catalyst.

### Claim 8 (depends on 7)

The method of claim 7, wherein the transition metal oxide is nickel(II) oxide, and wherein the transition metal salt is nickel(II) nitrate.

### Claim 9 (depends on 7)

The method of claim 7, wherein the bismuth salt is bismuth(III) nitrate.

### Claim 10 (depends on 7)

The method of claim 7, wherein the solvent comprises water.

### Claim 11 (depends on 7)

The method of claim 7, wherein the second mixture is dried at a temperature ranging from 50° C. to 200° C.

### Claim 12 (depends on 7)

The method of claim 7, wherein the dried mass is calcined in air at a temperature ranging from 300° C. to 700° C.

### Claim 13 (depends on 1)

A process of oxidatively dehydrogenating an alkane and/or an alkene to a corresponding diene, the process comprising:
flowing a feed mixture comprising the alkane and/or the alkene, and an oxidant through a reactor loaded with the composite catalyst of claim 1, thereby forming the corresponding diene.

### Claim 14 (depends on 13)

The process of claim 13, wherein the alkane is n-butane, the alkene is a butene, and the corresponding diene is butadiene.

### Claim 15 (depends on 13)

The process of claim 13, wherein a molar ratio of the oxidant to a total amount of the alkane and/or the alkene ranges from 0.1:1 to 8:1.

### Claim 16 (depends on 13)

The process of claim 13, wherein the flowing is performed at a temperature ranging from 250° C. to 700° C.

### Claim 17 (depends on 13)

The process of claim 13, wherein the oxidant is O2.

### Claim 18 (depends on 14)

The process of claim 14, wherein the feed mixture comprises n-butane, and wherein the process has a butadiene yield of 10-20 wt % relative to a weight of n-butane.

### Claim 19 (depends on 14)

The process of claim 14, wherein the feed mixture comprises n-butane, and wherein the process further forms butenes with a molar ratio of butadiene to butenes ranging from 1:1 to 3:1.

### Claim 20

The process of 14, wherein the feed mixture comprises 2-butene, and wherein the process has a butadiene yield of 30-80 wt % relative to a weight of 2-butene.