# US 2021/0140012 A1 · Process for the recovery of rare earths

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0140012 A1
- Document ID: US20210140012A1
- Status: Published application
- Kind: A1
- Application number: 17/046,936
- Filed: 2019-05-02
- Published: 2021-05-13
- Earliest claimed: 2018-05-03
- Assignees: Arafura Resources Limited
- Applicants: Arafura Resources Limited
- Inventors: Alexander Dean Elliot
- Web page: https://patentgrep.com/patent/US20210140012A1

## CPC

- C01F 11/46: Sulfates (dehydration of gypsum {for the production of calcium sulfate cements} C04B11/02)
- C01B 25/324: {Preparation from a reaction solution obtained by acidifying with an acid other than orthophosphoric acid}
- C01F 11/468: {Purification of calcium sulfates}
- C01F 17/206: oxide or hydroxide being the only anion
- C01F 17/235: Cerium oxides or hydroxides
- C01F 17/271: Chlorides
- C01F 17/282: Sulfates
- C22B 1/06: Sulfating roasting
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/10: Hydrochloric acid {, other halogenated acids or salts thereof}
- C22B 3/38: containing phosphorus
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 59/00: Obtaining rare earth metals
- Y02P 10/20: Recycling
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for the precipitation of rare earth sulphate, the method including subjecting a crude rare earth sulphate solution to precipitation in the presence of a water soluble, volatile, organic compound to produce a rare earth sulphate precipitate and an acidic supernatant. The organic compound is preferably selected from the group consisting of methanol, ethanol, iso-propanol, tert-butanol, acetone or mixtures thereof, and is preferably methanol. Preferably, the organic compound is used in the precipitation at a weight ratio of between 0.25:1 to 1.5:1, and preferably 0.5:to 1.25:1, with the crude sulphate solution.

## Claims

### Claim 1

A method for the precipitation of rare earth sulphate, the method including subjecting a crude rare earth sulphate solution to precipitation in the presence of a water soluble, volatile, organic compound to produce a rare earth sulphate precipitate and an acidic supernatant.

### Claim 2 (depends on 1)

The precipitation method of claim 1, wherein the water soluble, volatile, organic compound is selected from the group consisting of methanol, ethanol, iso-propanol, tert-butanol, acetone or mixtures thereof.

### Claim 3 (depends on 2)

The precipitation method of claim 2, wherein the water soluble, volatile, organic compound is methanol.

### Claim 4 (depends on 3)

The precipitation method of claim 3, wherein methanol is used in precipitation at a weight ratio of between 0.25:1 and 1.5:1 with the sulphate solution.

### Claim 5 (depends on 1)

The precipitation method of claim 1, wherein prior to precipitation the sulphate solution has a free sulphuric acid concentration above 5% w/w.

### Claim 6 (depends on 1)

The precipitation method of claim 1, wherein precipitation occurs at a temperature in the range of 30 to 85° C. with a residence time in the range of 5 to 120 minutes.

### Claim 7 (depends on 1)

The precipitation method of claim 1, wherein the organic compound is recovered from the acidic supernatant by distillation resulting in recovered organic compound and a dilute mixed acid solution, with the recovered organic compound being recycled for use in precipitation.

### Claim 8 (depends on 1)

The precipitation method of claim 1, wherein the dilute mixed acid solution is concentrated by evaporation to produce a concentrated mixed acid solution.

### Claim 9 (depends on 1)

The precipitation method of claim 1, further including producing the crude rare earth sulphate solution by pre-leaching a rare earth rich calcium phosphate concentrate with phosphoric acid to form a pre-leach residue enriched in rare earths, mixing the pre-leach residue with sulphuric acid and subsequently heating the mixture to convert the rare earths in the pre-leach residue to water-soluble rare earth sulphates, and subjecting the heat treated mixture to a water leach to place in solution the rare earth sulphates to form the crude rare earth sulphate solution.

### Claim 10 (depends on 9)

The precipitation method of claim 9, further including removal of calcium phosphate from the rare earth rich calcium phosphate concentrate by pre-leaching with phosphoric acid to form the pre-leach residue enriched in rare earths and a pre-leach solution containing monocalcium phosphate, impurities and minor amounts of rare earths.

### Claim 11 (depends on 10)

The precipitation method of claim 10, wherein the leach is operated in a two-stage counter current configuration at a temperature between 30 and 45° C., with residence times between 30 and 90 minutes for each stage, and with a feed acid to feed concentrate mass ratio kept between 2 and 12 grams of P in the acid per gram of Ca in the concentrate.

### Claim 12 (depends on 10)

The precipitation method of claim 10, wherein heat is applied to the pre-leach solution to precipitate out of solution the minor amounts of rare earths as rare earth phosphates, leaving a recovery solution.

### Claim 13 (depends on 12)

The precipitation method of claim 12, wherein the heating occurs in several stages of increasing temperatures, the temperatures all being in the range of 60° C. to 110° C., with stage residence times of between 60 and 180 minutes.

### Claim 14 (depends on 9)

The precipitation method of claim 9, wherein sulphuric acid and the dilute and/or concentrate mixed acid solution are added to the recovery solution to convert the monocalcium phosphate to phosphoric acid and form a calcium sulphate precipitate.

### Claim 15 (depends on 14)

The precipitation method of claim 14, wherein the acid addition is conducted in stages at a temperature of 30 to 50° C. and a residence time of between 30 and 90 minutes per stage.

### Claim 16

(canceled)

### Claim 17 (depends on 9)

The precipitation method of claim 9, including mixing the pre-leach residue with sulphuric acid, heating the mixture up to a temperature within the range 210 to 270° C., then holding the material at this temperature for a period of time of up to about 60 minutes to convert the rare earths in the pre-leach residue and the rare earth phosphates to water-soluble rare earth sulphates.

### Claim 18 (depends on 17)

The precipitation method of claim 17, wherein the mixing occurs for a time of up to about 30 minutes, either where there is no temperature control in the mixing stage, with mixed material heated between the mix and hold periods of sulphation, or where the sulphuric acid is pre-heated prior to addition such that acid mixing operates up to the temperature range.

### Claim 19 (depends on 17)

The precipitation method of claim 17, wherein the water-soluble rare earth sulphates are cooled to a temperature less than about 50° C. over a time period of up to about 300 minutes.

### Claim 20 (depends on 17)

The precipitation method of claim 17, wherein the water-soluble rare earth sulphates are subjected to a water leach to place in solution the rare earth sulphate, phosphoric acid, and the remaining sulphuric acid, and thus to form the crude rare earth sulphate solution and a water leach residue containing insoluble gangue material for disposal.

### Claim 21 (depends on 20)

The precipitation method of claim 20, wherein the water leach is conducted so as to minimise the leach of impurities from the gangue material and to maximise the concentration of rare earths in the crude rare earth sulphate solution.

### Claim 22 (depends on 21)

The precipitation method of claim 21, wherein the water leach is conducted at a temperature of less than about 35° C. and for a period of time of less than about 20 minutes.

### Claim 23 (depends on 1)

A method of processing the rare earth sulphate precipitate produced by the method of claim 1, further including washing and drying the rare earth sulphate precipitate, leaching in water the washed and dried rare earth sulphate precipitate to dissolve soluble rare earth sulphate and form a leach solution rich in rare earth sulphate and a leach residue containing impurities in the form of insoluble phosphates, precipitation of impurities from the rare earth sulphate leach solution to form a purified rare earth sulphate solution and a purification residue, precipitation of the rare earths in the purified rare earth sulphate solution as rare earth hydroxide, and selectively leaching the rare earth hydroxide precipitate to form a rare earth chloride solution and a residue.

### Claim 24 (depends on 23)

The processing method of claim 23, wherein the washing of the rare earth sulphate precipitate is conducted using a water-soluble, volatile, organic compound.

### Claim 25 (depends on 23)

The processing method of claim 23, wherein the dry rare earth sulphate precipitate is leached with water at about 40° C. for a period of 60 to 180 minutes, leaving a rare earth sulphate solution laced with impurities and a leach residue containing impurities in the form of insoluble phosphates.

### Claim 26 (depends on 23)

The processing method of claim 23, wherein magnesia is added to the rare earth sulphate leach solution to purify that solution by precipitation of impurities, leaving the purified rare earth sulphate solution and the purification residue.

### Claim 27 (depends on 26)

The processing method of claim 26, wherein the magnesia is added in multiple stages, each at a temperature of up to about 55° C. and for a time of about 30 to 120 minutes, with the pH of the purified rare earth sulphate solution being about 4.5 to 6.0.

### Claim 28 (depends on 23)

The processing method of claim 23, wherein the precipitation of the rare earths in the purified rare earth sulphate solution as rare earth hydroxide and the subsequent selective leaching occurs in:
a) contacting the rare earth sulphate solution with sodium hydroxide to precipitate rare earths as rare earth hydroxide, including the addition of an oxidant to oxidise cerium contained in the rare earth hydroxide precipitate; and
b) selectively leaching the rare earth hydroxide precipitate with hydrochloric acid to form a rare earth chloride solution and a residue.

### Claim 29 (depends on 28)

The processing method of claim 28, wherein the precipitation occurs in a two-stage counter-current process, including a precipitation stage and refining stage, wherein the rare earth sulphate solution feeds into the precipitation stage with spent solution from the refining stage, to precipitate rare earth hydroxide containing sulphate.

### Claim 30 (depends on 29)

The processing method of claim 29, wherein the sulphate containing rare earth hydroxide is subsequently converted to clean rare earth hydroxide in the refining stage with the addition of fresh sodium hydroxide.

### Claim 31 (depends on 29)

The processing method of claim 29, wherein the oxidant is hydrogen peroxide and/or sodium hypochlorite, which is added to the precipitation and/or refining stages following sodium hydroxide addition.

### Claim 32 (depends on 29)

The processing method of claim 29, wherein both the precipitation and the refining stage operate at a temperature of about 40 to 80° C., and for a time of about 30 to 60 minutes, with the stoichiometry of sodium hydroxide addition being in the range of 100 to 110%, and with 100 to 130% of stoichiometry dosing of oxidant.

### Claim 33 (depends on 28)

The processing method of claim 28, wherein the rare earth chloride solution contains negligible cerium, and the residue consists primarily of cerium (IV) hydroxide.

### Claim 34 (depends on 28)

The processing method of claim 28, wherein the selective leaching of rare earth hydroxide precipitate is conducted in two stages, each stage having multiple tanks and each stage using hydrochloric acid diluted to 5 to 15% w/w with leach solution from the first leach stage.

### Claim 35 (depends on 34)

The processing method of claim 34, wherein leach solution from the second leach stage is used to re-pulp, leach rare earth hydroxide precipitate, and precipitate cerium (IV) dissolved in the second leach stage, prior to the first leach stage.

### Claim 36 (depends on 34)

The processing method of claim 34, wherein the selective leaching occurs at a temperature of 60 to 80° C., the first leach stage is operated to maximise rare earth dissolution while minimising cerium (IV) dissolution, which is achieved with an endpoint pH of about pH 3 to 4, and the second leach stage is operated to minimise the concentration of non-cerium rare earth elements in the residue.

### Claim 37 (depends on 28)

The processing method of claim 28, wherein barium chloride is added to the rare earth chloride solution, with sulphuric acid when sulphate levels are low, to remove radium via co-precipitation with barium sulphate to form a purified rare earth chloride solution.

### Claim 38 (depends on 37)

The processing method of claim 37, wherein the purified rare earth chloride solution is concentrated by evaporation.