# US 2021/0130922 A1 · Method for refining magnetic domains of grain-oriented electrical steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0130922 A1
- Document ID: US20210130922A1
- Status: Published application
- Kind: A1
- Application number: 16/472,484
- Filed: 2017-12-20
- Published: 2021-05-06
- Earliest claimed: 2016-12-22
- Assignees: Posco
- Applicants: Posco
- Inventors: Oh-Yeoul KWON; Ki-Young MIN; Se-Min PARK; Jong-Tae PARK; Seong-Cheol HONG
- Web page: https://patentgrep.com/patent/US20210130922A1

## CPC

- C21D 10/005: {by laser shock processing}
- B23K 26/0622: by shaping pulses
- B23K 26/073: Shaping the laser spot
- B23K 26/364: for making a groove or trench, e.g. for scribing a break initiation groove
- C21D 3/04: Decarburising
- C21D 3/08: Extraction of nitrogen
- C21D 6/008: {containing Si}
- C21D 8/1233: {Cold rolling}
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1283: {Application of a separating or insulating coating}
- C21D 8/1288: {Application of a tension-inducing coating}
- C21D 8/1294: involving a localised treatment
- C21D 9/46: for sheet metals
- C21D 10/00: Modifying the physical properties by methods other than heat treatment or deformation
- B23K 2103/04: Steel {or steel} alloys
- C21D 2201/05: Grain orientation
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for refining magnetic domains of a grain-oriented electrical steel sheet according to an exemplary embodiment of the present invention includes: a step of preparing a grain-oriented electrical steel sheet; and a step of forming a groove by irradiating a quasi-continuous laser beam of which a duty is from 98.0 to 99.9% on a surface of the grain-oriented electrical steel sheet.

## Claims

### Claim 1

A method for refining magnetic domains of a grain-oriented electrical steel sheet, comprising:
a step of preparing a grain-oriented electrical steel sheet; and
a step of forming a groove by irradiating a quasi-continuous laser beam of which a duty is from 98.0 to 99.9% on a surface of the grain-oriented electrical steel sheet,
wherein the duty is a ratio (Tb/Ta) of [a time of irradiation with an output of 10% or more of a maximum output (Pmax)] Tb to [an output modulation cycle time] Ta in a time diagram for an output of a laser beam.

### Claim 2 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
a frequency of the quasi-continuous laser beam is from 100 Hz to 8 kHz.

### Claim 3 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
a ratio P/W of an average output P of a laser beam for a quasi-continuous laser beam width W is from 30 W/mm to 300 W/mm.

### Claim 4 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
a ratio W/L of a beam width W in a steel sheet rolling direction to a beam length L in a steel sheet width direction of the quasi-continuous laser beam is from 0.1 to 0.86.

### Claim 5 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
the laser has a TEM00 mode, and M2 of a beam quality factor is 1.0 to 1.1.

### Claim 6 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
3 to 8 grooves are intermittently formed from in the width direction of the steel sheet.

### Claim 7 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
the grooves are linear and are formed at an angle from 82° to 98° with respect to a rolling direction of the electrical steel sheet.

### Claim 8 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, wherein
a depth D of the groove is formed from 3% to 8% of the thickness of the steel sheet.

### Claim 9 (depends on 1)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 1, further comprising,
after the step of forming the groove:
a step of forming an oxide layer on the surface of the steel sheet through decarburization annealing or nitride annealing; and
a step of coating an annealing separator on the surface of the steel sheet formed with the oxide layer and forming non-metal oxide layer on the surface of the steel sheet through high temperature annealing.

### Claim 10 (depends on 9)

The method for refining magnetic domains of the grain-oriented electrical steel sheet of claim 9, further comprising,
after the step of forming the non-metal oxide layer,
a step of forming an insulating coating layer on the non-metal oxide layer.