# US 2021/0123113 A1 · Method for treating and phosphatizing metal board without using acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0123113 A1
- Document ID: US20210123113A1
- Status: Published application
- Kind: A1
- Application number: 17/079,621
- Filed: 2020-10-26
- Published: 2021-04-29
- Earliest claimed: 2019-10-29
- Assignees: Kunshan Airbag Packing Corp
- Applicants: Kunshan Airbag Packing Corp.
- Inventors: TAI-AN LIAO; KAO-HSIUNG LIAO; PING-YUAN LIAO; TSAI-MING KUO
- Web page: https://patentgrep.com/patent/US20210123113A1

## CPC

- C21D 7/06: by shot-peening or the like
- B24C 11/00: Selection of abrasive materials {or additives} for abrasive blasts (polishing compositions C09G)
- C23C 22/10: containing oxidants
- C23C 22/12: containing zinc cations
- C23C 22/18: containing manganese cations
- C23C 22/73: characterised by the process
- C23C 22/77: Controlling or regulating of the coating process
- C23C 22/78: Pretreatment of the material to be coated
- C23G 5/06: using emulsions
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

A method for treating and phosphatizing a metal board without using acid includes the following steps: performing a degreasing step to remove grease and dirt from a surface of the metal board with a degreasing agent; performing a blast-peening step by blasting and peening polygon blast-peening granules on the metal board through a centrifugal impeller to remove an oxidized layer; performing a washing step to clean remaining powders from the metal board after the blast-peening step; performing a phosphatizing step to form a protective phosphate coating on the metal board; performing another washing step to wash off remaining phosphatizing agents from the metal board; performing a rustproofing step to apply a rustproofing agent on the metal board; and performing a drying step to dry the metal board.

## Claims

### Claim 1

A method for treating and phosphatizing a metal board without using acid, comprising:
performing a degreasing step, wherein a degreasing agent is provided to remove grease and dirt from a surface of the metal board;
performing a blast-peening step by blasting and peening polygon blast-peening granules on the surface of the metal board through centrifugal impellers to remove an oxidized layer;
performing a washing step to wash the surface of the metal board, so as to remove powders generated from the blast-peening step;
performing a phosphatizing step to form a phosphate coating on the surface of the metal board, so as to provide protection;
performing another washing step to wash off remaining phosphatizing agents from the metal board;
performing a rustproofing step to apply a rustproofing agent on the metal board; and
performing a drying step to dry the metal board.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the blast-peening step includes providing a plurality of centrifugal impellers, the plurality of centrifugal impellers being arranged symmetrically at an upper surface and a lower surface of the metal board, respectively, and symmetrically performing blast-peening on the upper surface and the lower surface of the metal board.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a speed of blast-peening the granules in the blast-peening step is from 50 to 200 meters per second, a material of the blast-peening granules is carborundum or silicon carbide, and a diameter of the blast-peening granules is from 320 to 1400 μm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the blast-peening step includes adjusting distances between nozzles of the centrifugal impellers and the metal board.

### Claim 5 (depends on 4)

The method according to claim 4, further including providing a distance detector to detect the distances between the nozzles of the centrifugal impellers and the metal board.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the blast-peening step includes adjusting angles of blast-peening between nozzles of the centrifugal impellers and the metal board.

### Claim 7 (depends on 1)

The method according to claim 1, wherein each of the centrifugal impellers includes a program-controllable motor, such that rotational speeds of the centrifugal impellers may be adjusted.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the phosphatizing step includes using manganese phosphate solution or zinc phosphate solution.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a thickness of the oxidized layer removed in the blast-peening step is greater than 10 μm.

### Claim 10 (depends on 1)

The method according to claim 1, further including a surface real-time observation step, wherein a detector is used to detect a status of removing the oxidized layer from the surface of the metal board in real-time, and wherein, when detecting that the powder generated from removing the oxidized layer has a characteristic in the air that undergoes a change, the blast-peening step is stopped.