# US 2021/0083362 A1 · Packaging Structure and Packaging Method for Antenna

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083362 A1
- Document ID: US20210083362A1
- Status: Published application
- Kind: A1
- Application number: 17/108,953
- Filed: 2020-12-01
- Published: 2021-03-18
- Earliest claimed: 2018-03-16
- Assignees: SJ Semiconductor(Jiangyin) Corporation
- Applicants: SJ Semiconductor (Jiangyin) Corporation
- Inventors: Yenheng CHEN; Chengchung LIN; Chengtar WU; Jangshen LIN
- Web page: https://patentgrep.com/patent/US20210083362A1

## CPC

- H01Q 1/2283: {mounted in or on the surface of a semiconductor substrate as a chip-type antenna or integrated with other components into an IC package}
- H01Q 21/0093: {Monolithic arrays}
- H10W 44/20: at high-frequency [HF] or radio frequency [RF]
- H10W 70/05: of insulating or insulated package substrates, or of interposers, or of redistribution layers (manufacture or treatment of leadframes H10W70/04)
- H10W 70/095: {of vias therein}
- H10W 70/099: {Connecting interconnections to insulating or insulated package substrates, interposers or redistribution layers}
- H10W 70/685: comprising multiple insulating layers
- H10W 70/69: Insulating materials thereof
- H10W 72/072: {of bump connectors}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 90/701: {characterised by the relative positions of pads or connectors relative to package parts}
- H10P 72/74: {using temporarily an auxiliary support}
- H10P 72/7412: {the auxiliary support including means facilitating the separation of a device or wafer from the auxiliary support}
- H10P 72/7424: {used as a support during the manufacture of self-supporting substrates}
- H10P 72/743: {used as a support during manufacture of interconnect decals or build up layers}
- H10P 72/7436: {used to support a device or a wafer when forming electrical connections thereto}
- H10W 44/206: {Wires}
- H10W 44/248: {for antennas}
- H10W 70/656: Fan-in layouts
- H10W 70/695: Organic materials
- H10W 72/07207: {Temporary substrates, e.g. removable substrates}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07307: {the auxiliary member being a temporary substrate, e.g. a removable substrate}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H01Q: ANTENNAS, i.e. RADIO AERIALS (radiators or antennas for microwave heating H05B6/72)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present disclosure provides a packaging structure and a packaging method for an antenna. The packaging structure comprises a redistribution layer, having a first surface and an opposite second surface; a first metal joint pin, formed on the second surface of the redistribution layer; a first packaging layer, disposed on the redistribution layer covering the first metal joint pin; a first antenna metal layer, patterned on the first packaging layer, and a portion of the first antenna metal layer electrically connects with the first metal joint pin; a second metal joint pin, formed on the first antenna metal layer; a second packaging layer, disposed on the first antenna metal layer covering the second metal joint pin; a second antenna metal layer, formed on the second packaging layer; and a metal bump and an antenna circuit chip, bonded to the first surface of the redistribution layer.

## Claims

### Claim 1

An IC antenna structure, comprising:
a supporting substrate having a separation layer on a first surface of the supporting substrate
a first antenna metal layer disposed on the separation layer over the first surface of the supporting substrate;
a first metal joint pin disposed on the first antenna metal layer over the first surface of the supporting substrate,
a first packaging layer disposed over the first surface of the supporting substrate, and a top surface of the first metal joint pin is exposed from a top surface of the first packaging layer;
a second antenna metal layer disposed on the top surface of the first packaging layer, wherein a portion of the second antenna metal layer is electrically connected with the first metal joint pin;
a second metal joint pin disposed on said portion of the second antenna metal layer over the first surface of the supporting substrate, wherein the second antenna metal layer and the second metal joint pin are packaged with a second packaging layer, and wherein a top surface of the second metal joint pin is exposed from a top surface of the second packaging layer;
a redistribution layer formed on the top surface of the second packaging layer over the first surface of the supporting substrate, wherein the redistribution layer is above the first and the second metal joint pins and is electrically connected with the second metal joint pin;
a metal bump formed on the redistribution layer over the first surface of the supporting substrate; and
an antenna circuit chip bonded on the redistribution layer next to the metal bump over the first surface of the supporting substrate.

### Claim 2 (depends on 1)

The IC antenna structure according to claim 1, wherein the first packaging layer is selected from one of polyimide, silica gel and epoxy resin, and the second packaging layer is made from one of polyimide, silica gel and epoxy resin.

### Claim 3 (depends on 1)

The IC antenna structure according to claim 1, wherein the redistribution layer is formed of a stack comprising a patterned first dielectric layer, a patterned first metal wiring layer, a patterned second dielectric layer and a patterned second metal wiring layer, and wherein the patterned first metal wiring layer is electrically connected with the patterned second metal wiring layer.

### Claim 4 (depends on 3)

The IC antenna structure according to claim 3, wherein the first dielectric layer and the second dielectric layer are made from one or a combination of two or more of epoxy resin, silica gel, PI, PBO, BCB, silicon oxide, phosphorosilicate glass and fluorine-containing glass, and the patterned first metal wiring layer and the patterned second metal wiring layer are made from one or a combination of two or more of copper, aluminum, nickel, gold, silver and titanium.

### Claim 5 (depends on 1)

The IC antenna structure according to claim 1, wherein the first metal joint pin and the second metal joint pin are made from one of Au, Ag, Cu, and Al.

### Claim 6 (depends on 1)

The IC antenna structure according to claim 1, wherein the metal bump comprises one of tin solder, silver solder and gold-tin alloy solder.

### Claim 7 (depends on 1)

The IC antenna structure according to claim 1, further comprising a bottom filling layer formed between the antenna circuit chip and the redistribution layer to increase the bonding strength of the antenna circuit chip and the redistribution layer and protect the redistribution layer.

### Claim 8 (depends on 1)

The IC antenna structure according to claim 1, wherein the second antenna metal layer protrudes from a surface of the second packaging layer.

### Claim 9 (depends on 1)