# US 2021/0083346 A1 · Metal-air fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083346 A1
- Document ID: US20210083346A1
- Status: Published application
- Kind: A1
- Application number: 17/036,642
- Filed: 2020-09-29
- Published: 2021-03-18
- Earliest claimed: 2015-09-17
- Assignees: Zinc8 Energy Solutions Inc.
- Applicants: Zinc8 Energy Solutions Inc.
- Inventors: Stuart Smedley; Wolf Tivy; Boguslaw Wozniczka; David Robert Bruce
- Web page: https://patentgrep.com/patent/US20210083346A1

## CPC

- H01M 12/06: with one metallic and one gaseous electrode
- H01M 4/06: Electrodes for primary cells
- H01M 4/42: Alloys based on zinc
- H01M 4/78: Shapes other than plane or cylindrical, e.g. helical
- H01M 8/225: {Fuel cells in which the fuel is based on materials comprising particulate active material in the form of a suspension, a dispersion, a fluidised bed or a paste}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0014: Alkaline electrolytes
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of charging a metal-air fuel cell. The method includes a step of orienting an anode chamber horizontally. The method further method includes a step of providing metal particles suspended in an electrolyte to flow through the anode chamber in a downstream direction oriented horizontally. The method further method includes a step of allowing a bed of the metal particles to form on the anode current collector. The plurality of particle collectors perturb the flow of electrolyte through the anode chamber and encourage settling of the particles one of on and between the particle collectors. The method further method includes a step of maintaining uniform formation of the bed.

## Claims

### Claim 1

A method of charging a metal-air fuel cell, the method comprising the steps of:
(a) orienting an anode chamber horizontally wherein a corresponding anode current collector is positioned below the anode chamber, the anode current collector comprising a plurality of particle collectors projecting into the anode chamber;
(b) providing metal particles suspended in an electrolyte to flow through the anode chamber in a downstream direction oriented horizontally;
(c) allowing a bed of the metal particles to form on the anode current collector, wherein the plurality of particle collectors perturb the flow of electrolyte through the anode chamber and encourage settling of the particles one of on and between the particle collectors; and
(d) maintaining uniform formation of the bed.

### Claim 2 (depends on 1)

The method according to claim 1, wherein step (c) comprises at least one of:
(i) maintaining the flow of the metal particles suspended in the electrolyte at a predetermined flow rate; and
(ii) periodically stopping the flow of the metal particles suspended in the electrolyte.

### Claim 3 (depends on 2)

The method according to claim 2, wherein step (d) comprises providing a uniform flow of the electrolyte through the anode chamber.

### Claim 4 (depends on 3)

The method according to claim 3, wherein providing the uniform flow comprises providing a continuous pressure drop in a downstream direction in the anode chamber and a minimal pressure drop in a direction normal to the downstream direction.

### Claim 5 (depends on 4)

The method according to claim 4, wherein providing the continuous pressure drop in the downstream direction and the minimal pressure drop in the direction normal to the downstream direction comprises providing one of a parallel flow and a serpentine flow path for the anode chamber.

### Claim 6 (depends on 3)

The method according to claim 3, wherein a flow velocity of the electrolyte in the anode chamber ranges from 1 cm3/s to 5000 cm3/s.

### Claim 7 (depends on 6)

The method according to claim 6, wherein a flow rate of the electrolyte in the anode chamber ranges from one of 1 L/min. to 7 L/min, 3 L/min. to 7 L/min, and 3 L/min. to 5 L/min.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the gauge pressure of the electrolyte in the anode chamber ranges from one of 0.69 kPa to 103.4 kPa and 13.8 kPa to 68.9 kPa.

### Claim 9 (depends on 8)

The method according to claim 8, wherein a pressure drop traversing the anode chamber is less than 103.4 kPa.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the metal particles are zinc particles and the electrolyte is aqueous potassium hydroxide.

### Claim 11 (depends on 10)

The method according to claim 10, further comprising a step of drawing a current density of at least 50 mA/cm2 from the fuel cell.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising a step of applying a load to the fuel cell.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising a step of discharging for a period of 1 to 20 hours.