# US 2021/0083293 A1 · Lithium Secondary Battery and Method of Preparing Anode for Lithium Secondary Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083293 A1
- Document ID: US20210083293A1
- Status: Published application
- Kind: A1
- Application number: 17/021,145
- Filed: 2020-09-15
- Published: 2021-03-18
- Earliest claimed: 2019-09-16
- Assignees: SK Innovation Co., Ltd.
- Applicants: SK Innovation Co., Ltd.
- Inventors: Jong Hyuk Lee; Dock Young Yoon; Hee Gyoung Kang
- Web page: https://patentgrep.com/patent/US20210083293A1

## CPC

- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/622: {being polymers}
- H01M 50/105: Pouches or flexible bags
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium secondary battery according to exemplary embodiments includes a cathode, a separation layer, and an anode facing the cathode with the separation layer interposed therebetween. The anode includes an anode current collector, and an anode active material layer formed on the anode current collector. The anode active material layer includes an anode active material and a conductive additive. The conductive additive includes an expandable graphite having a particle diameter of 10 μm or less.

## Claims

### Claim 1

A lithium secondary battery, comprising:
a cathode;
a separation layer; and
an anode facing the cathode with the separation layer interposed therebetween, wherein the anode comprises:
an anode current collector; and
an anode active material layer formed on the anode current collector, the anode active material layer including an anode active material and a conductive additive,
wherein the conductive additive includes an expandable graphite having a particle diameter of 10 μm or less.

### Claim 2 (depends on 1)

The lithium secondary battery according to claim 1, wherein the particle diameter of the expandable graphite is in a range from 1 μm to 7 μm.

### Claim 3 (depends on 1)

The lithium secondary battery according to claim 1, wherein an expansion ratio of the expandable graphite is from 150% to 500%.

### Claim 4 (depends on 1)

The lithium secondary battery according to claim 1, wherein the anode active material includes natural graphite or artificial graphite.

### Claim 5 (depends on 1)

The lithium secondary battery according to claim 1, wherein the anode active material layer further includes at least one of a carbon-based conductive agent and a metal-based conductive agent.

### Claim 6 (depends on 1)

The lithium secondary battery according to claim 1, wherein an amount of the expandable graphite is in a range from 1 wt % to 8 wt % based on a total weight of the anode active material layer.

### Claim 7 (depends on 1)

The lithium secondary battery according to claim 1, wherein the anode active material layer includes pores formed by an elastic deformation of the expandable graphite.

### Claim 8 (depends on 1)

The lithium secondary battery according to claim 1, wherein a porosity of the anode active material layer is from 17% to 29%.

### Claim 9 (depends on 1)

The lithium secondary battery according to claim 1, wherein a density of the anode active material layer is from 1.4 g/cc to 1.9 g/cc.

### Claim 10

A method of fabricating an anode for a lithium secondary battery, comprising:
grinding a graphite particle including natural graphite or artificial graphite to have a particle diameter of 10 μm or less;
acid-treating the grinded graphite particle;
washing and drying the acid-treated graphite particle to prepare an expandable graphite;
mixing the expandable graphite with an anode active material to prepare an anode slurry; and
coating the anode slurry on a current collector to form an anode active material layer.

### Claim 11 (depends on 10)

The method according to claim 10, further comprising heating the acid-treated graphite particle before washing and drying.

### Claim 12 (depends on 10)

The method according to claim 10, wherein forming the anode active material layer comprises:
drying the anode slurry coated on the current collector; and
pressing the dried anode slurry.

### Claim 13 (depends on 12)

The method according to claim 12, wherein an expansion ratio of the expandable graphite before pressing is 500% or less, and an expansion ratio of the expandable graphite after pressing is from 110% to 300%.

### Claim 14 (depends on 10)

The method according to claim 10, wherein the expandable graphite is included by an amount of 1 wt % to 8 wt % based on a solid content of the anode slurry.