# US 2021/0083285 A1 · Process for making an electrode active material, and electrode active material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083285 A1
- Document ID: US20210083285A1
- Status: Published application
- Kind: A1
- Application number: 16/968,322
- Filed: 2019-01-31
- Published: 2021-03-18
- Earliest claimed: 2018-02-09
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Heino SOMMER; Maraike AHLF; Jacob HAAG; Regina VOGELSANG; Fatih CETINEL
- Web page: https://patentgrep.com/patent/US20210083285A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/70: defined by measured X-ray, neutron or electron diffraction data
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Process for making a partially coated electrode active material wherein said process comprises the following steps: (a) Providing an electrode active material according to general formula Li1+x, TM1+XO2, wherein TM is a combination of Ni, Co and, optionally, Mn, and, optionally, at least one metal selected from Al, Ti and Zr, and x is in the range of from zero to 0.2, wherein at least 60 mole-% of the transition metal of TM is Ni, and wherein said electrode active material has a residual moisture content in the range of from 50 to 1,000 ppm, (b) treating said electrode active material with a metal alkoxide or metal halide or metal amide or alkyl metal compound, (c) treating the material obtained in step (b) with moisture, (d) repeating the sequence of steps (b) and (c) twice to ten times, (e) performing a post-treatment by heating the material obtained after the last step (d) at a temperature from 200 to 400° C.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A process for making a partially coated electrode active material, the process comprising:
(a) providing an electrode active material according to the following formula
Li1+xTM1−xO2,
wherein TM is a combination of Ni Co, optionally Mn, and optionally at least one metal selected from the group consisting of Al, Ti, and Zr,
x is in a range of from 0 to 0.2,
at least 60 mole-% of the transition metal of TM is Ni, and
said electrode active material has a residual moisture content in a range of from 50 to 1,000 ppm,
(b) treating said electrode active material with a metal alkoxide, metal halide, metal amide, or alkyl metal compound,
(c) treating the material obtained in (b) with moisture,
(d) repeating the sequence of (b) and (c) two to ten times, and
(e) performing a post-treatment by heating the material obtained after the last repetition of (d) at a temperature in a range of from 200 to 400° C.

### Claim 15 (depends on 14)

The process of claim 14, wherein TM is a combination of metals according to the following formula (I)
(NiaCobMnc)1−dMd (I)
wherein
a is in a range of from 0.6 to 0.9,
b is in a range of from 0.05 to 0.2,
c is in a range of from 0.05 to 0.2,
d is in a range of from 0 to 0.1,
M is Al, and
a+b+c=1.

### Claim 16 (depends on 14)

The process of claim 14, wherein (b) is performed in a rotary kiln, a free fall mixer, a continuous vibrating bed, or a fluidized bed.

### Claim 17 (depends on 14)

The process of claim 14, wherein the alkyl metal compound of (c) is selected from the group consisting of trimethylaluminum, and triethylaluminum.

### Claim 18 (depends on 14)

The process of claim 14, wherein each flushing step between (b) and (c) has a duration in a range of from 1 second to 10 minutes.

### Claim 19 (depends on 14)

The process of claim 14, wherein (b) to (c) are performed in a free-fall mixer.

### Claim 20 (depends on 14)

The process of claim 14, wherein (b) to (c), and (e) are performed in a fluidized bed.

### Claim 21 (depends on 14)

The process of claim 14, wherein TM is selected from the group consisting of Ni0.6Co0.2Mn0.2, Ni0.7Co0.2Mn0.1, and Ni0.8Co0.1Mn0.1.

### Claim 22 (depends on 14)

The process of claim 14, wherein (e) is performed in an atmosphere of inert gas.

### Claim 23 (depends on 14)

The process of claim 14, wherein (e) has a duration in a range of from 10 minutes to 2 hours.

### Claim 24

A particulate electrode active material according to the following formula
Li1+xTM1−xO2,
wherein TM is a combination of Ni, Co, optionally Mn, and optionally at least one metal selected from Al, Ti, and Zr,
x is in a range of from 0 to 0.2,
at least 60 mole-% of the transition metal of TM is Ni, and
an outer surface of said particles is non-homogeneously coated with an acidic oxide selected from the group consisting of acidic aluminum oxyhydroxide, and acidic alumina.

### Claim 25 (depends on 24)

The particulate electrode active material of claim 24, wherein TM is selected from the group consisting of Ni0.6Co0.2Mn0.2, Ni0.7Co0.2Mn0.1, and Ni0.8Co0.1Mn0.1 and
said acidic oxide is selected from the group consisting of acidic aluminum oxyhydroxide, and acidic alumina.

### Claim 26 (depends on 24)

A process of manufacturing a lithium ion battery, the process comprising obtaining the particulate electrode active material of claim 24.