# US 2021/0083276 A1 · Composition and method for lamination of silicon dominant anodes utilizing water based adhesives

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083276 A1
- Document ID: US20210083276A1
- Status: Published application
- Kind: A1
- Application number: 16/570,311
- Filed: 2019-09-13
- Published: 2021-03-18
- Earliest claimed: 2019-09-13
- Assignees: Enevate Corporation
- Applicants: Enevate Corporation
- Inventors: Ambica J. Nair; Younes Ansari; Frederic Bonhomme; Benjamin Park; Sung Won Choi; Giulia Canton
- Web page: https://patentgrep.com/patent/US20210083276A1

## CPC

- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/622: {being polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are anodes created using water based adhesive solutions, low temperature methods for laminating anodes comprising water based adhesives, and alkali ion batteries that comprise the anodes.

## Claims

### Claim 1

An anode comprising: a current collector; a solid film comprising electrochemically active material in electrical communication with the current collector, the film comprising a silicon carbon composite film; and a layer of adhesive material between the current collector and the film, wherein the adhesive layer comprises a mixture of polyacrylic acid (PAA) and polyvinyl alcohol (PVA) that adheres the film to the current collector.

### Claim 2 (depends on 1)

The anode of claim 1, wherein the silicon carbon composite film is in direct contact with the current collector and the adhesive material is between the current collector and the film at the locations where the film is not in direct contact with the current collector.

### Claim 3 (depends on 1)

The anode of claim 1, wherein at least one of PAA and PVA comprises 20-80% of the total adhesive layer.

### Claim 4 (depends on 3)

The anode of claim 3, wherein said adhesive layer comprises 50% PAA and 50% PVA.

### Claim 5 (depends on 3)

The anode of claim 3, wherein said adhesive layer comprises 60% PAA and 40% PVA

### Claim 6 (depends on 3)

The anode of claim 3, wherein said adhesive layer comprises 40% PAA and 60% PVA

### Claim 7 (depends on 1)

The anode of claim 1, wherein the adhesive layer has a final thickness of about 1 microns to about 4 microns.

### Claim 8 (depends on 1)

The anode of claim 1, wherein the anode is a silicon dominant anode.

### Claim 9 (depends on 1)

The anode of claim 1, wherein the current collector comprises copper.

### Claim 10

A method of forming an electrode comprising:
coating a current collector with a solution comprising a mixture of polyacrylic acid (PAA) and polyvinyl alcohol (PVA);
drying the coated current collector; and
applying pressure and heat to the coated current collector and a solid film comprising electrochemically active material under conditions to adhere the coated current collector to the solid film to form the electrode.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the coating step solution comprises 20%-80% of at least one of PAA and PVA

### Claim 12 (depends on 10)

The method according to claim 10, wherein the coating step solution comprises 40% PVA and 60% PAA.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the drying step provides a PAA/PVA layer having a final thickness of about 1 microns to about 4 microns.

### Claim 14 (depends on 10)

The method according to claim 10, wherein the drying step comprises a temperature of about 90° C. and a time of about 1 hour.

### Claim 15 (depends on 10)

The method according to claim 10, wherein the applying pressure and heat comprises up to about 10000 psi of pressure at temperatures less than about 200° C.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the applying pressure and heat comprises about 3000-4000 psi of pressure at about 90-200° C.

### Claim 17 (depends on 10)

The method according to claim 10, wherein the applying pressure is between about 20 pounds/inch to about 2000 pounds/inch.

### Claim 18 (depends on 10)

The method according to claim 10, wherein the electrode is an anode.

### Claim 19 (depends on 10)

The method according to claim 10, wherein the electrode is a silicon carbon composite anode

### Claim 20 (depends on 10)

The method according to claim 10, wherein the electrode is a silicon dominant anode.

### Claim 21 (depends on 10)

The method according to claim 10, wherein the current collector comprises copper.

### Claim 22 (depends on 10)

An electrode formed by the method of claim 10.

### Claim 23

A method of forming a battery, the method comprising:
providing an anode, a cathode, and a separator, the anode comprising a current collector coated with a mixture of polyacrylic acid (PAA) and polyvinyl alcohol (PVA) adhered to an anode substrate comprising a silicon carbon composite material; and
assembling the cathode, the separator, and the anode, with an electrolyte to form the battery.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the anode comprises a silicon dominant anode.

### Claim 25 (depends on 23)

The method according to claim 23, wherein the current collector comprises copper.

### Claim 26 (depends on 23)

The method according to claim 23, wherein the cathode comprises an active material comprising one or more of lithium, sodium, and potassium.

### Claim 27 (depends on 26)

The method according to claim 26, wherein the cathode active material comprises lithium.

### Claim 28 (depends on 26)

The method according to claim 26, wherein the cathode active material comprises lithium doped with a transition metal oxide or a non-transition metal oxide.

### Claim 29 (depends on 26)

The method according to claim 26, wherein the cathode active material comprises 5% to 30% excess of lithium.

### Claim 30

A battery comprising:
an anode, a cathode, an electrolyte, and a separator, wherein:
the anode comprises a current collector coated with a mixture of polyacrylic acid (PAA) and polyvinyl alcohol (PVA) adhered to an anode substrate comprising a silicon carbon composite material.

### Claim 31 (depends on 30)

The battery according to claim 30, wherein the electrolyte comprises a liquid, solid, or gel.

### Claim 32 (depends on 30)

The battery according to claim 30, wherein the anode comprises a silicon dominant anode.

### Claim 33 (depends on 30)

The battery according to claim 30, wherein the current collector comprises copper.

### Claim 34 (depends on 30)

The battery according to claim 30, wherein the cathode comprises an active material comprising one or more of lithium, sodium, and potassium.

### Claim 35 (depends on 34)

The battery according to claim 34, wherein the cathode active material comprises lithium.

### Claim 36 (depends on 34)

The battery according to claim 34, wherein the cathode active material comprises lithium doped with a transition metal oxide or a non-transition metal oxide.

### Claim 37 (depends on 34)

The battery according to claim 34, wherein the cathode active material comprises 5% to 30% excess of lithium.