# US 2021/0083272 A1 · ION CONDUCTOR CONTAINING Li2B12H12 AND LiBH4, METHOD FOR PRODUCING SAME, AND SOLID ELECTROLYTE FOR ALL-SOLID-STATE BATTERIES, WHICH CONTAINS SAID ION CONDUCTOR

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083272 A1
- Document ID: US20210083272A1
- Status: Published application
- Kind: A1
- Application number: 16/971,868
- Filed: 2019-02-22
- Published: 2021-03-18
- Earliest claimed: 2018-02-28
- Assignees: Mitsubishi Gas Chemical Company, Inc.; Tohoku Techno Arch Co., Ltd.
- Applicants: Mitsubishi Gas Chemical Company, Inc.; Tohoku Techno Arch Co., Ltd.
- Inventors: Genki NOGAMI; Masahiro SHIMADA; Naoki TOYAMA; Sangryun KIM; Shin-ichi ORIMO
- Web page: https://patentgrep.com/patent/US20210083272A1

## CPC

- H01B 1/06: mainly consisting of other non-metallic substances
- H01M 4/364: {as mixtures}
- C01B 6/21: Preparation of borohydrides of alkali metals, alkaline earth metals, magnesium or beryllium; Addition complexes thereof, e.g. LiBH4.2N2H4, NaB2H7
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- C01P 2002/74: by peak-intensities or a ratio thereof only
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application provides a method for producing an ion conductor containing Li2B12H12 and LiBH4, which includes obtaining a mixture by mixing LiBH4 and B10H14 at a molar ratio LiBH4/B10H14 of from 2.1 to 4.3; and subjecting the mixture to a heat treatment.

## Claims

### Claim 1

A method for producing an ion conductor comprising Li2B12H12 and LiBH4, which comprises:
obtaining a mixture by mixing LiBH4 and B10H14 at a molar ratio LiBH4/B10H14 of from 2.1 to 4.3; and
subjecting the mixture to a heat treatment.

### Claim 2 (depends on 1)

The method for producing an ion conductor according to claim 1, wherein the temperature of the heat treatment is 100 to 300° C.

### Claim 3 (depends on 1)

The method for producing an ion conductor according to claim 1, which comprises subjecting the mixture to a mechanical milling treatment prior to the heat treatment.

### Claim 4 (depends on 3)

The method for producing an ion conductor according to claim 3, wherein the time for carrying out the mechanical milling treatment is 0.5 to 7 hours.

### Claim 5 (depends on 3)

The method for producing an ion conductor according to claim 3, which comprises subjecting the mixture to a second mechanical milling treatment after the heat treatment.

### Claim 6 (depends on 5)

The method for producing an ion conductor according to claim 5, wherein the time for carrying out the second mechanical milling treatment is 10 to 30 hours.

### Claim 7 (depends on 1)

The method for producing an ion conductor according to claim 1, wherein the ion conductor obtained has peaks at at least −15.6 ppm (±1 ppm), −17.6 ppm (±1 ppm), −1.7 ppm and −29.4 ppm (±1.5 ppm), and −42.0 ppm (±2 ppm) in a B11MAS NMR measurement, and wherein when −15.6 ppm (±1 ppm) is regarded as Peak A and −42.0 ppm (±2 ppm) is regarded as Peak B, the intensity ratio of Peak B to Peak A (B/A) is 0.1 to 2.0.

### Claim 8 (depends on 1)

A method for producing an all-solid-state battery, which comprises carrying out molding using the ion conductor obtained by the method according to claim 1 under an atmosphere at a dew point of −30° C. to −80° C.

### Claim 9

An ion conductor comprising Li2B12H12 and LiBH4, which has peaks at at least −15.6 ppm (±1 ppm), −17.6 ppm (±1 ppm), −1.7 ppm and −29.4 ppm (±1.5 ppm), and −42.0 ppm (±2 ppm) in a B11MAS NMR measurement, wherein when −15.6 ppm (±1 ppm) is regarded as Peak A and −42.0 ppm (±2 ppm) is regarded as Peak B, the intensity ratio of Peak B to Peak A (B/A) is 0.1 to 2.0.

### Claim 10 (depends on 9)

The ion conductor according to claim 9, which has X-ray diffraction peaks at at least 2θ=16.1±0.5 deg, 18.6±0.5 deg, 24.0±0.5 deg, 24.9±0.8 deg, 27.0±0.8 deg, 31.0±0.8 deg and 32.5±0.8 deg.

### Claim 11 (depends on 9)

A solid electrolyte for all-solid-state batteries, which comprises the ion conductor according to claim 9.