# US 2021/0083070 A1 · Doped encapsulation material for diamond semiconductors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083070 A1
- Document ID: US20210083070A1
- Status: Published application
- Kind: A1
- Application number: 16/573,187
- Filed: 2019-09-17
- Published: 2021-03-18
- Earliest claimed: 2019-09-17
- Assignees: Massachusetts Institute of Technology; Arizona Board of Regents on behalf of Arizona State University
- Applicants: Massachusetts Institute of Technology; Arizona Board of Regents on behalf of Arizona State University
- Inventors: Michael Geis; Joseph Varghese; Robert Nemanich
- Web page: https://patentgrep.com/patent/US20210083070A1

## CPC

- H10D 48/031: {of three-or-more electrode devices}
- H10W 74/137: {the encapsulations being directly on the semiconductor body (H10W74/134 takes precedence)}
- H10D 30/01: Manufacture or treatment
- H10D 62/8303: {Diamond}
- H10P 14/6314: {of a metallic layer}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6929: {the material containing aluminium, e.g. AlSiOx}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 14/69395: {the material containing zirconium, e.g. ZrO2}
- H10P 14/69397: {the material containing two or more metal elements}
- H10P 95/94: {Hydrogenation or deuterisation, e.g. using atomic hydrogen from a plasma}
- H10W 74/01: Manufacture or treatment
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

According to some embodiments, a method for stabilizing electrical properties of a diamond semiconductor comprises terminating a surface of a diamond with hydrogen (H) or deuterium (D) atoms and over-coating the surface of the diamond with an encapsulating material comprising metal oxide salt doped with one or more elements capable of generating negative charge in the metal oxide salt.

## Claims

### Claim 1

A method for stabilizing electrical properties of a diamond semiconductor, the method comprising:
terminating a surface of a diamond with hydrogen (H) or deuterium (D) atoms; and
over-coating the surface of the diamond with an encapsulating material comprising metal oxide salt doped with one or more elements capable of generating negative charge in the metal oxide salt.

### Claim 2 (depends on 1)

The method of claim 1 wherein the metal oxide salt comprises aluminum oxide (Al2O3) and the one or more elements capable of generating negative charge comprise at least one of silicon dioxide (SiO2) and/or zirconium oxide (ZrO2).

### Claim 3 (depends on 1)

The method of claim 1 wherein the metal oxide salt comprises aluminum phosphate (AlPO4) and the one or more elements capable of generating negative charge comprise at least one of silicon dioxide (SiO2) and/or zirconium oxide (ZrO2).

### Claim 4 (depends on 1)

The method of claim 1 wherein the metal oxide salt comprises boron oxide (B2O3) and the one or more elements capable of generating negative charge comprise at least one of silicon dioxide (SiO2) and/or zirconium oxide (ZrO2).

### Claim 5 (depends on 1)

The method of claim 1 wherein the encapsulating material comprises at least one of aluminum (Al) or boron (B), wherein, in the encapsulating material, the concentration of Al or B is less than that of the or more elements capable of generating negative charge.

### Claim 6 (depends on 1)

The method of claim 1 wherein over-coating the surface of the diamond with the encapsulating material comprises using an evaporation process.

### Claim 7 (depends on 6)

The method of claim 6 wherein the encapsulating material has a thickness of less than 2 nm.

### Claim 8 (depends on 6)

The method of claim 6 wherein the evaporation process comprises:
mounting the diamond to a vacuum system;
heating the diamond to a temperature greater than 100° C.;
wherein over-coating the surface of the diamond with the encapsulating material comprises:
coating the surface of the diamond with at least one of Al or B using an evaporation technique;
adding, to the surface of the diamond, the one or more elements capable of generating negative charge; and
annealing the diamond in an oxidizing atmosphere to oxidize the Al or B and the one or more elements capable of generating negative charge.

### Claim 9 (depends on 8)

The method of claim 8 wherein adding the one or more elements capable of generating negative charge occurs before coating the surface of the diamond.

### Claim 10 (depends on 8)

The method of claim 8 wherein adding the one or more elements capable of generating negative charge occurs during coating of the surface of the diamond.

### Claim 11 (depends on 1)

The method of claim 1 wherein over-coating the surface of the diamond with the encapsulating material comprises using an atomic layer deposition (ALD) process.

### Claim 12 (depends on 11)

The method in claim 11 where, during the ALD process, the temperature of the diamond is increased from less than 300° C. to more than 350° C.

### Claim 13 (depends on 11)

The method of claim 11 wherein the ALD process comprises:
flowing argon (Ar) gas over the diamond;
heating the diamond to a temperature of between 100 to 500 degrees Celsius;
injecting alternating gas pulses into the argon gas;
cooling the diamond semiconductor under argon gas; and
annealing the diamond in an oxidizing atmosphere to oxidize the Al or B and the one or more elements capable of generating negative charge.

### Claim 14 (depends on 13)

The method of claim 13 wherein the alternating gas pulses comprise:
water (H2O);
an aluminium (Al) precursor; and
a silicon dioxide (SiO2) precursor.

### Claim 15 (depends on 13)

The method of claim 13 wherein the Al precursor comprises trimethyl aluminum (Al(CH3)3)).

### Claim 16 (depends on 13)

The method of claim 13 wherein the SiO2 precursor comprises tris(tert-butoxy)silanol ((OC(CH3)3)3SiOH).

### Claim 17 (depends on 13)

The method in claim 13 wherein the alternating gas pulses comprise a boron oxide (B2O3) precursor.

### Claim 18 (depends on 13)

The method of claim 13 wherein the alternating gas pulses comprise a zirconium dioxide (ZrO2) precursor.

### Claim 19 (depends on 13)

The method of claim 13 wherein the alternating gas pulses comprise silicon dioxide (SiO2) and a zirconium dioxide (ZrO2) precursor.

### Claim 20 (depends on 13)

The method of claim 13 wherein one or more steps of the ALD process occur within an ALD chamber, the method comprising:
before placing the diamond in the ALD chamber, precoating the chamber with SiO2 or ZrO2 using a SiO2 precursor or a ZrO2 precursors, and an oxygen (O2) plasma.

### Claim 21 (depends on 1)

The method of claim 1 wherein over-coating the surface of the diamond with the encapsulating material comprises using a sol-gel spin coating process.

### Claim 22 (depends on 21)

The method of claim 21 wherein the sol-gel spin coating process comprises:
mixing an aluminum (Al) solution with a silicon (SiO2) precursor solution;
spin-coating the mixed solution onto the surface of the diamond with a surfactant to ensure wetting of the diamond surface with the sol-gel;
heating the sol-gel to a temperature greater than 100° C.;
annealing the diamond in an oxidizing atmosphere to oxidize the Al or B and the one or more elements capable of generating negative charge.

### Claim 23 (depends on 1)

The method of claim 1 comprising over-coating the encapsulating material with a dielectric layer.

### Claim 24

A diamond semiconductor comprising:
a surface terminated with hydrogen (H) or deuterium (D) atoms; and
an encapsulating layer disposed over the surface of the diamond, the encapsulating layer comprising metal oxide salt doped with one or more elements capable of generating negative charge.