# US 2021/0083058 A1 · Method of producing epitaxial silicon wafer, epitaxial silicon wafer, and method of producing solid-state imaging device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083058 A1
- Document ID: US20210083058A1
- Status: Published application
- Kind: A1
- Application number: 16/956,232
- Filed: 2018-08-24
- Published: 2021-03-18
- Earliest claimed: 2017-12-26
- Assignees: Sumco Corporation
- Applicants: Sumco Corporation
- Inventors: Takeshi KADONO; Kazunari KURITA
- Web page: https://patentgrep.com/patent/US20210083058A1

## CPC

- H10D 62/60: Impurity distributions or concentrations
- H10F 39/811: {Interconnections}
- C23C 16/24: Deposition of silicon only
- C30B 25/02: Epitaxial-layer growth
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3254: {Graded layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 30/224: {of a cluster, e.g. using a gas cluster ion beam}
- H10P 36/03: {within silicon bodies}
- H10F 39/199: {Back-illuminated image sensors}
- H10P 14/3818: {using particle beams}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method of producing an epitaxial silicon wafer having high gettering capability resulting in even more reduced white spot defects in a back-illuminated solid-state imaging device. The method includes: a first step of irradiating a surface of a silicon wafer with cluster ions of CnHm (n=1 or 2, m=1, 2, 3, 4, or 5) generated using a Bernas ion source or an IHC ion source, thereby forming, in the silicon wafer, a modifying layer containing, as a solid solution, carbon and hydrogen that are constituent elements of the cluster ions; and a subsequent second step of forming a silicon epitaxial layer on the surface. In the first step, peaks of concentration profiles of carbon and hydrogen in the depth direction of the modifying layer are made to lie in a range of more than 150 nm and 2000 nm or less from the surface.

## Claims

### Claim 1

A method of producing an epitaxial silicon wafer, comprising:
a first step of irradiating a surface of a silicon wafer with cluster ions of CnHm (n=1 or 2, m=1, 2, 3, 4, or 5) generated using one of a Bernas ion source and an IHC ion source, thereby forming, in the silicon wafer, a modifying layer containing, as a solid solution, carbon and hydrogen that are constituent elements of the cluster ions; and
a second step of forming a silicon epitaxial layer on the surface after the first step,
wherein in the first step, peaks of concentration profiles of the carbon and the hydrogen in a depth direction of the modifying layer are made to lie in an area with a depth in a range of more than 150 nm and 2000 nm or less from the surface of the silicon wafer.

### Claim 2 (depends on 1)

The method of producing an epitaxial silicon wafer, according to claim 1, wherein in the first step, the irradiation with the cluster ions is performed at a beam current value of 170 μA or more.

### Claim 3 (depends on 1)

The method of producing an epitaxial silicon wafer, according to claim 1, wherein in the first step, the irradiation with the cluster ions is performed so that a tilt angle and a twist angle of the silicon wafer are both 0°.

### Claim 4 (depends on 1)

The method of producing an epitaxial silicon wafer, according to claim 1, further comprising a step of cleaning the surface of the silicon wafer between the first step and the second step.

### Claim 5

An epitaxial silicon wafer, comprising: a silicon wafer; a modifying layer containing carbon and hydrogen as a solid solution, the modifying layer being formed in the silicon wafer; and a silicon epitaxial layer formed on the modifying layer,
wherein peaks of concentration profiles of the carbon and the hydrogen in the depth direction of the modifying layer lie in an area with a depth in a range of more than 150 nm and 2000 nm or less from a surface of the silicon wafer.

### Claim 6 (depends on 5)

The epitaxial silicon wafer according to claim 5, wherein a distance between the peak position of the concentration profile of the carbon in the depth direction and the peak position of the concentration profile of the hydrogen in the depth direction is within 1000 nm.

### Claim 7 (depends on 5)

The epitaxial silicon wafer according to claim 5, wherein the peak concentration of the concentration profile of the carbon in the depth direction and the peak concentration of the concentration profile of the hydrogen in the depth direction are both 1×1016 atoms/cm3 or more.

### Claim 8 (depends on 1)

A method of producing a solid-state imaging device comprising forming a solid-state imaging device in the silicon epitaxial layer of the epitaxial silicon wafer produced according to the method of producing an epitaxial silicon wafer, according to claim 1.

### Claim 9 (depends on 5)